摘要
A glass wall assembly was exposed to an intense real-scale compartment fire. The wall assembly consisted of four glass sections, two of which were fitted with tempered double-pane glass and the other two sections were fitted with tempered single-pane glass. At each glass section, temperatures were measured at the exposed face and the unexposed face. Total heat flux gauges were used to measure both the temporal variation of the energy incident on the glass wall and the transmitted energy rate detected through two of the glass sections. Visual and infrared cameras were used to image the unexposed face of each wall assembly during the fire exposure. Results of glass breakage and subsequent glass fall out were compared to studies in the literature for glass sections exposed to compartment fires. The behavior of the glass wall assembly under a fire load is presented.
引用
收藏
页码:77 / 89
页数:12
相关论文
共 50 条
  • [31] Performance of glass brick wall exposed to fire
    Sokol, Z.
    Eliasova, M.
    STRUCTURES AND ARCHITECTURE: BRIDGING THE GAP AND CROSSING BORDERS, 2019, 1 : 638 - 645
  • [32] Fabrication of Non-load Bearing Cotton Stalks Bales and Pressure-resistant Property Test
    Qiang, Jin
    Yong, Feng
    Chun, He Jin
    Quan, Luo Li
    MATERIALS SCIENCE AND PROCESSING, ENVIRONMENTAL ENGINEERING AND INFORMATION TECHNOLOGIES, 2014, 665 : 383 - 387
  • [33] Experimental study of load bearing cold-formed steel wall systems under fire conditions
    Gunalan, Shanmuganathan
    Kolarkar, Prakash
    Mahendran, Mahen
    THIN-WALLED STRUCTURES, 2013, 65 : 72 - 92
  • [34] Simplified theoretical model on fire performance of load bearing cold-formed steel wall systems
    Key Laboratory of Concrete and Prestressed Concrete Structures of China Ministry of Education, Southeast University, Nanjing
    210096, China
    不详
    201803, China
    Jianzhu Jiegou Xuebao, 8 (123-132):
  • [35] Experimental assessment of thermal break strips performance in load-bearing and non-load-bearing LSF walls
    Santos, Paulo
    Mateus, Diogo
    JOURNAL OF BUILDING ENGINEERING, 2020, 32
  • [36] Determination of notch factors for transverse non-load carrying stiffeners based on numerical analysis and metamodeling
    Josef Neuhäusler
    Klemens Rother
    Welding in the World, 2022, 66 : 753 - 766
  • [37] Improved fire resistant performance of load bearing cold-formed steel interior and exterior wall systems
    Chen, Wei
    Ye, Jihong
    Bai, Yu
    Zhao, Xiao-Ling
    THIN-WALLED STRUCTURES, 2013, 73 : 145 - 157
  • [38] Load bearing tests of earthquake resisting wall using toughened glass
    Nippon Sheet Glass Co., Ltd., Japan
    不详
    不详
    不详
    AIJ J. Technol. Des., 2007, 26 (523-528):
  • [39] Realize the Non-load Bearing Walls Material Products Development of Building Envelope of Energy Conservation and Durable Fire Integration and Realize the Complete Sets of Technology Researching
    Cao, Wanzhi
    Wang, Hongzhen
    Sun, Qingxia
    FRONTIERS OF GREEN BUILDING, MATERIALS AND CIVIL ENGINEERING, PTS 1-8, 2011, 71-78 : 1136 - +
  • [40] Development of macroporous eggshell derived apatite bone cement for non-load bearing defect repair in orthopedics
    Dewangan, Vimal Kumar
    Kumar, T. S. Sampath
    Doble, Mukesh
    Varghese, Viju Daniel
    CERAMICS INTERNATIONAL, 2022, 48 (24) : 37000 - 37012