Evaluation of the chemical index model for predicting supplementary cementitious material dosage to prevent the alkali-silica reaction in concrete

被引:12
|
作者
Cassiani, Juan [1 ]
Dugarte, Margareth [2 ]
Martinez-Arguelles, Gilberto [2 ]
机构
[1] Univ Fed Armed Forces Hamburg, Helmut Schmidt Univ, Construct Mat & Bldg Preservat, D-22043 Hamburg, Germany
[2] Univ Norte, Dept Civil & Environm Engn, Km 5 Via Puerto Colombia, Barranquilla, Colombia
关键词
Alkali-silica reaction; Natural aggregate; Recycled concrete aggregate; Supplementary cementitious materials; Modeling; Chemical constituents; Fly ash; Silica fume; Slag; FLY-ASH DOSAGE; REACTION MITIGATION; ACCELERATED TEST; TERNARY BLENDS; DURABILITY; SLAG; RELIABILITY; EFFICIENCY; CALCIUM; IMPACT;
D O I
10.1016/j.conbuildmat.2020.122158
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This study investigates the chemical index model effectiveness in predicting the minimum replacement of several types of Supplementary Cementitious Materials (SCMs) to mitigate the potential Alkali-Silica Reaction (ASR) in concrete. The experimental program results evaluating four natural aggregates (AF1, AF2, AF3, and AF4) and two Recycled Concrete Aggregates (RCA1 and RCA2), as presented here, were used in the model predictions. The SCMs used in this study consisted of fly ash class C (FA1), fly ash class F (FA2), ground granulated blast-furnace slag (SL), and silica fume (SF). For each SCMs, three levels of Portland cement replacements were used in the production of mortar bars: 15%-20%-25% for FA1-FA2; 20%-40%-60% for SL; and 5%-8%-10% for SF. The natural aggregates were tested according to the ASTM C1260 accelerated mortar bar test. For the RCA, an alternative preparation procedure was applied in the experimental phase to eliminate variability in the results given the RCA's high absorption. Further testing was then implemented for the aggregates classified as potentially reactive by evaluating different SCMs replacement levels to mitigate ASR using the accelerated mortar bar method, following the ASTM C1567. A Monte Carlo simulation was conducted to evaluate the chemical index prediction uncertainty, based on the model inputs statistical variation. The SCMs evaluated in this investigation were effective in mitigating ASR while used in sufficient proportion. The most effective SCMs in reducing ASR was silica fume, with a 10% replacement of Portland cement's weight, fly ash class F was next (15-25%), and finally ground granulated blast-furnace slag (40-60%). The chemical index has proven to give good results when predicting the minimum replacement of supplementary cementitious materials required to suppress ASR based on its chemical composition. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Using electrical resistivity to determine the efficiency of supplementary cementitious materials to prevent alkali-silica reaction in concrete
    Chopperla, Krishna Siva Teja
    Ideker, Jason H.
    CEMENT & CONCRETE COMPOSITES, 2022, 125
  • [2] Correlation Between the Reactivity of Supplementary Cementitious Materials and Their Efficacy to Prevent Alkali-Silica Reaction
    Chopperla, Krishna Siva Teja
    Parashar, Anuj
    Ideker, Jason H.
    PROCEEDINGS OF THE 75TH RILEM ANNUAL WEEK 2021, 2023, 40 : 74 - 82
  • [3] A material model for alkali-silica reaction in reinforced concrete
    Winnicki, A.
    Pietruszczak, S.
    Computational Modelling of Concrete Structures, 2006, : 657 - 664
  • [4] An extended chemical index model to predict the fly ash dosage necessary for mitigating alkali-silica reaction in concrete
    Vayghan, Asghar Gholizadeh
    Wright, Jared Robert
    Rajabipour, Farshad
    CEMENT AND CONCRETE RESEARCH, 2016, 82 : 1 - 10
  • [5] A review of ground waste glass as a supplementary cementitious material: A focus on alkali-silica reaction
    Bueno, Eduard Tora
    Paris, Jerry M.
    Clavier, Kyle A.
    Spreadbury, Chad
    Ferraro, Christopher C.
    Townsend, Timothy G.
    JOURNAL OF CLEANER PRODUCTION, 2020, 257
  • [6] Using Supplementary Cementitious Materials to Mitigate Alkali-Silica Reaction in Concrete with Recycled-Concrete Aggregate
    Adams, Matthew P.
    Ideker, Jason H.
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2020, 32 (08)
  • [7] Role of temperature on Alkali-Silica reaction and the efficacy of supplementary cementitious materials
    Sinno, Noura
    Shehata, Medhat H.
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 313
  • [8] A Modified Chemical Index to Predict Fly Ash Dosage for Mitigating Alkali-Silica Reaction
    Deschenes, Richard
    Jones, Casey
    Giannini, Eric R.
    Hale, Micah
    ADVANCES IN CIVIL ENGINEERING MATERIALS, 2019, 8 (01): : 699 - 722
  • [9] Performance Evaluation of Novel Alkali-Silica Reaction Inhibiting Chemical Admixtures in Cementitious Systems
    Kaladharan, Gopakumar
    Rajabipour, Farshad
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2023, 35 (09)
  • [10] Rapid Test Method for Evaluating Inhibiting Effectiveness of Supplementary Cementitious Materials on Alkali-Silica Reaction Expansion of Concrete
    Yi, Lei
    Mao, Zhongyang
    Deng, Min
    Liu, Xiang
    Fan, Zhiyuan
    Huang, Xiaojun
    Zhang, Tao
    Tang, Mingshu
    MATERIALS, 2022, 15 (09)