Room and high temperature flexural failure of spark plasma sintered boron carbide

被引:25
|
作者
Vasylkiv, O. [1 ,2 ]
Demirskyi, D. [1 ,2 ]
Badica, P. [2 ,3 ]
Nishimura, T. [1 ]
Tok, A. I. Y. [2 ]
Sakka, Y. [1 ]
Borodianska, H. [2 ]
机构
[1] Natl Inst Mat Sci, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
[2] Nanyang Technol Univ, 50 Nanyang Ave, Singapore 639798, Singapore
[3] Natl Inst Mat Phys, St Atomistilor 105 Bis, Magurele 077125, Romania
关键词
Boron carbide; Spark plasma sintering; Flexural mechanical properties; MECHANICAL-PROPERTIES; VIBRATIONAL PROPERTIES; PRESSURE-DEPENDENCE; RAMAN-SPECTROSCOPY; COMPOSITES; STRENGTH; SILICON; MICROSTRUCTURE; HARDNESS; CARBON;
D O I
10.1016/j.ceramint.2016.01.088
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Dense (95-98.6%) bulk boron carbide prepared by Spark Plasma Sintering (SPS) in Ar or N-2 atmospheres were subject to three-point flexural tests at room and at 1600 degrees C. Eight different consolidation conditions were used via SPS of commercially available B4C powder. Resulting specimens had similar grain size not exceeding 4 mu m and room-temperature bending strength (sigma(25) (degrees C)) of 300-600 MPa, suggesting that difference in sigma(25) (degrees C) m is due to development of secondary phases in monolithic boron carbide ceramics during SPS processing. To explain such difference the composition of boron carbide and secondary phases observed by XRD and Raman spectroscopy. The variation in intensity of the Raman peak at 490 cm(-1) of boron carbide suggests modification of the boron carbide composition and a higher intensity correlates with a higher room temperature bending strength (sigma(25) (degrees C)) and Vickers hardness (HV). Secondary phases can modify the level of mechanical characteristics within some general trends that are not dependent on additives (with some exceptions) or technologies. Namely, HV increases, sigma(25) (degrees C) decreases, and the ratio sigma(1600 degrees C)/sigma(25 degrees C) (sigma(1600 degrees C) - bending strength at 1600 degrees C) is lower when fracture toughness (K-IC) is higher. The ratio sigma(1600 degrees C)/sigma(25 degrees C) shows two regions of low and high K-IC delimited by K-IC=4.1 MPa m(0.5): in the low K-IC region, boron carbide specimens are produced in nitrogen. (c) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:7001 / 7013
页数:13
相关论文
共 50 条
  • [21] High thermal conductivity of spark plasma sintered silicon carbide ceramics with yttria and scandia
    Seo, Yu-Kwang
    Kim, Young-Wook
    Nishimura, Toshiyuki
    Seo, Won-Seon
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2017, 100 (04) : 1290 - 1294
  • [22] Effect of boron on the microstructure of spark plasma sintered Ultrafine WC
    Kumar, A. K. Nanda
    Watabe, Masaki
    Kurokawa, Kazuya
    VACUUM, 2013, 88 : 88 - 92
  • [23] Observation of room-temperature ferroelectricity in spark-plasma sintered GdCrO3
    Mishra, Suryakanta
    Keerthana
    Rudrapal, Krishna
    Rahaman, Aminur
    Pal, Pratap
    Sagdeo, Archna
    Mishra, Ranjit
    Topwal, Dinesh
    Chaudhuri, Ayan Roy
    Adyam, Venimadhav
    Choudhury, Debraj
    PHYSICAL REVIEW B, 2021, 104 (18)
  • [24] LASER MELTING OF SPARK PLASMA SINTERED ZIRCONIUM CARBIDE: THERMOPHYSICAL PROPERTIES OF A GENERATION IV VERY HIGH TEMPERATURE REACTOR MATERIAL
    Jackson, Heather F.
    Daniel, Doni J.
    Clegg, William J.
    Reece, Mike J.
    Inam, Fawad
    Manara, Dario
    Casoni, Carlo Perinetti
    De Bruycker, Franck
    Boboridis, Konstantinos
    Lee, William E.
    CERAMICS IN NUCLEAR APPLICATIONS, 2010, 30 (10): : 161 - +
  • [25] Deuterium retention in sintered boron carbide exposed to a deuterium plasma
    Alimov, VK
    Komarov, DA
    Roth, J
    Mayer, M
    Lindig, S
    JOURNAL OF NUCLEAR MATERIALS, 2006, 349 (03) : 282 - 290
  • [26] Low temperature synthesis and spark plasma sintering of a boron carbide with a low residual carbon content
    Kenny, Jonathan
    McDonald, Nikkia
    Binner, Jon
    Chang, Isaac Tsz Hong
    Marinel, Sylvain
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (02) : 383 - 391
  • [27] Reflectance spectral studies of spark plasma sintered tungsten carbide pellet
    Chono, Toshiharu
    Tokutomi, Hisashi
    Nakamura, Kazuma
    Miyazaki, Koji
    Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 1
  • [28] Comparative analysis for the prediction of WEDM responses for machining spark plasma sintered boron carbide ceramic sample by RSM and ANFIS
    Pramanick, Ayan
    Mandal, Saikat
    Dey, Partha Pratim
    Das, Probal Kr
    MATERIALS TODAY-PROCEEDINGS, 2021, 41 : 1030 - 1095
  • [29] Reflectance spectral studies of spark plasma sintered tungsten carbide pellet
    Chono, Toshiharu
    Tokutomi, Hisashi
    Nakamura, Kazuma
    Miyazaki, Koji
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2025, 64 (01)
  • [30] Spark plasma sintering and mechanical properties of boron carbide ceramics
    Chen, Gang
    Zhang, Song
    Wang, Chuan-Bin
    Shen, Qiang
    Zhang, Lian-Meng
    Rengong Jingti Xuebao/Journal of Synthetic Crystals, 2009, 38 (01): : 165 - 169