Room and high temperature flexural failure of spark plasma sintered boron carbide

被引:25
|
作者
Vasylkiv, O. [1 ,2 ]
Demirskyi, D. [1 ,2 ]
Badica, P. [2 ,3 ]
Nishimura, T. [1 ]
Tok, A. I. Y. [2 ]
Sakka, Y. [1 ]
Borodianska, H. [2 ]
机构
[1] Natl Inst Mat Sci, 1-2-1 Sengen, Tsukuba, Ibaraki 3050047, Japan
[2] Nanyang Technol Univ, 50 Nanyang Ave, Singapore 639798, Singapore
[3] Natl Inst Mat Phys, St Atomistilor 105 Bis, Magurele 077125, Romania
关键词
Boron carbide; Spark plasma sintering; Flexural mechanical properties; MECHANICAL-PROPERTIES; VIBRATIONAL PROPERTIES; PRESSURE-DEPENDENCE; RAMAN-SPECTROSCOPY; COMPOSITES; STRENGTH; SILICON; MICROSTRUCTURE; HARDNESS; CARBON;
D O I
10.1016/j.ceramint.2016.01.088
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Dense (95-98.6%) bulk boron carbide prepared by Spark Plasma Sintering (SPS) in Ar or N-2 atmospheres were subject to three-point flexural tests at room and at 1600 degrees C. Eight different consolidation conditions were used via SPS of commercially available B4C powder. Resulting specimens had similar grain size not exceeding 4 mu m and room-temperature bending strength (sigma(25) (degrees C)) of 300-600 MPa, suggesting that difference in sigma(25) (degrees C) m is due to development of secondary phases in monolithic boron carbide ceramics during SPS processing. To explain such difference the composition of boron carbide and secondary phases observed by XRD and Raman spectroscopy. The variation in intensity of the Raman peak at 490 cm(-1) of boron carbide suggests modification of the boron carbide composition and a higher intensity correlates with a higher room temperature bending strength (sigma(25) (degrees C)) and Vickers hardness (HV). Secondary phases can modify the level of mechanical characteristics within some general trends that are not dependent on additives (with some exceptions) or technologies. Namely, HV increases, sigma(25) (degrees C) decreases, and the ratio sigma(1600 degrees C)/sigma(25 degrees C) (sigma(1600 degrees C) - bending strength at 1600 degrees C) is lower when fracture toughness (K-IC) is higher. The ratio sigma(1600 degrees C)/sigma(25 degrees C) shows two regions of low and high K-IC delimited by K-IC=4.1 MPa m(0.5): in the low K-IC region, boron carbide specimens are produced in nitrogen. (c) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:7001 / 7013
页数:13
相关论文
共 50 条
  • [41] Microstructural designs of spark-plasma sintered silicon carbide ceramic scaffolds
    Roman-Manso, B.
    De Pablos, A.
    Belmonte, M.
    Osendi, M. I.
    Miranzo, P.
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2014, 53 (02): : 93 - 100
  • [42] Spark plasma sintering of silicon nitride-boron carbide composites
    Ayas, E.
    Kalemtas, A.
    Arslan, G.
    Kara, A.
    Kara, F.
    Key Engineering Materials, 2009, 403 : 225 - 226
  • [43] Spark plasma sintering of silicon carbide powders with carbon and boron as additives
    Yang J.
    Jiao J.
    Wang L.
    Li B.
    2018, Wiley Blackwell (263): : 137 - 143
  • [44] Bulk boron carbide nanostructured ceramics by reactive spark plasma sintering
    Moskovskikh, D. O.
    Paramonov, K. A.
    Nepapushev, A. A.
    Shkodich, N. F.
    Mukasyan, A. S.
    CERAMICS INTERNATIONAL, 2017, 43 (11) : 8190 - 8194
  • [45] DENSIFICATION AND MICROSTRUCTURAL PROPERTIES OF BORON-CARBIDE IN SPARK PLASMA SINTERING
    Toksoy, M. F.
    Haber, R. A.
    ADVANCES IN CERAMIC ARMOR VII, 2011, 32 : 81 - 89
  • [46] Laser Melting of Spark Plasma-Sintered Zirconium Carbide: Thermophysical Properties of a Generation IV Very High-Temperature Reactor Material
    Jackson, Heather F.
    Jayaseelan, Daniel D.
    Lee, William E.
    Reece, Michael J.
    Inam, Fawad
    Manara, Dario
    Casoni, Carlo Perinetti
    De Bruycker, Franck
    Boboridis, Konstantinos
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2010, 7 (03) : 316 - 326
  • [47] Spark Plasma Sintering of Silicon Nitride-Boron Carbide Composites
    Ayas, E.
    Kalemtas, A.
    Arslan, G.
    Kara, A.
    Kara, F.
    SIAIONS AND NON-OXIDES, 2009, 403 : 225 - 226
  • [48] BORON CARBIDE-BASED NANOSTRUCTURED COMPOSITE BY SPARK PLASMA SINTERING
    Xie, Sky Shumao
    Solodkyi, Ievgen
    Vasylkiv, Oleg
    Silberschmidt, Vadim
    Tok, Alfred I. Y.
    PROCEEDINGS OF THE 1ST INTERNATIONAL CONFERENCE ON PROGRESS IN ADDITIVE MANUFACTURING, 2014, : 109 - 114
  • [49] High-temperature strength of boron carbide with Pt grain-boundary framework in situ synthesized during spark plasma sintering
    Vasylkiv, O.
    Demirskyi, D.
    Borodianska, H.
    Kuncser, A.
    Badica, P.
    CERAMICS INTERNATIONAL, 2020, 46 (07) : 9136 - 9144
  • [50] Hydrogen spillover drives room temperature sensing on spark plasma sintered BaTiO3 with Pt electrodes
    Bell, Jon G.
    Huangfu, Shangxiong
    Artiglia, Luca
    Graule, Thomas
    Stuer, Michael
    JOURNAL OF MATERIALS CHEMISTRY A, 2024, 12 (46) : 31993 - 32013