Fatigue limit and microstructure in lamellar graphite iron

被引:1
|
作者
Fourlakidis, Vasilios [1 ]
Schmidt, Pal [2 ]
Jarfors, Anders E. W. [1 ]
Svidro, Peter [1 ]
Dioszegi, Attila [1 ]
机构
[1] Jonkoping Univ, Dept Mat & Mfg, Box 1026, SE-55111 Jonkoping, Sweden
[2] Volvo Technol AB, S-40508 Gothenburg, Sweden
关键词
Lamellar graphite iron; Fatigue limit; Ultimate tensile strength; Graphite ferret; Inter-dendritic hydraulic diameter; CAST-IRON; STRENGTH; MORPHOLOGY;
D O I
10.1016/j.msea.2020.140617
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Demanding environmental legislation and improve performance specifications requires increasing fatigue strength for the engine components that are made of lamellar graphite iron (LGI). Components design, metallurgy and casting conditions define the microstructure formation and mechanical properties. The graphite inclusions embedded in the metallic matrix acting as defects and have a detrimental effect on the fatigue strength of LGI. The cooling conditions determine the coarseness of the microstructure and also have, a great impact on the fatigue resistance. The experimental material was an LGI alloy produced with three different solidification times. A fully reversed fatigue test was performed, and various microstructure features were quantitatively estimated by utilizing the Gumbel's statistics of extremes. The stereological parameter of Hydraulic Diameter of the Inter-dendritic Phase and the graphite Feret size found to be the most suitable microstructure parameters to be correlated with the fatigue limit. The results also indicate the sizeable effect of the solidification time on the fatigue limit. Several other microstructure features that have been reported to influence the tensile strength were also found to be related to the fatigue limit. The obtained endurance ratio ranges from 0.25 to 0.30, a value that is in line with previous investigations.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] The Effect of the Substitution of Silicon by Aluminum on the Properties of Lamellar Graphite Iron
    E. Aguado
    M. Ferrer
    P. Larrañaga
    D. M. Stefanescu
    R. Suárez
    International Journal of Metalcasting, 2019, 13 : 536 - 545
  • [42] The Effect of the Substitution of Silicon by Aluminum on the Properties of Lamellar Graphite Iron
    Aguado, E.
    Ferrer, M.
    Larranaga, P.
    Stefanescu, D. M.
    Suarez, R.
    INTERNATIONAL JOURNAL OF METALCASTING, 2019, 13 (03) : 536 - 545
  • [43] Fatigue properties of spherical graphite iron crankshafts
    Ma, Mingtu
    Ll, Zhigang
    Yl, Hongliang
    Zhang, Hao
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 2744 - +
  • [44] Fatigue behaviour of cast iron with globular graphite
    Hübner, P
    Pusch, G
    Krodel, L
    ADVANCED ENGINEERING MATERIALS, 2004, 6 (07) : 541 - 544
  • [45] Fatigue limit evaluation considering crack initiation for lamellar pearlitic steel
    Hamada, S.
    Sasaki, D.
    Ueda, M.
    Noguchi, H.
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10 : 1467 - 1472
  • [46] Characterization of Graphite Flakes in Grey Iron Microstructure
    Adedayo, A. V.
    ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2012, 37 (06): : 1645 - 1652
  • [47] Characteristics and Microstructure of Graphite Encapsulated Iron Nanoparticles
    曹宏
    Journal of Wuhan University of Technology(Materials Science Edition), 2007, (02) : 214 - 217
  • [48] Characteristics and microstructure of graphite encapsulated iron nanoparticles
    Cao, Hong
    Li, Ru
    Gui, Qiji
    Wang, Xuehua
    Bin, Xiaobei
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2007, 22 (02): : 214 - 217
  • [49] Characteristics and microstructure of graphite encapsulated iron nanoparticles
    Hong Cao
    Ru Li
    Qiji Gui
    Xuehua Wang
    Xiaobei Bin
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2007, 22 : 214 - 217
  • [50] Characterization of Graphite Flakes in Grey Iron Microstructure
    A. V. Adedayo
    Arabian Journal for Science and Engineering, 2012, 37 : 1645 - 1652