Fatigue limit and microstructure in lamellar graphite iron

被引:1
|
作者
Fourlakidis, Vasilios [1 ]
Schmidt, Pal [2 ]
Jarfors, Anders E. W. [1 ]
Svidro, Peter [1 ]
Dioszegi, Attila [1 ]
机构
[1] Jonkoping Univ, Dept Mat & Mfg, Box 1026, SE-55111 Jonkoping, Sweden
[2] Volvo Technol AB, S-40508 Gothenburg, Sweden
关键词
Lamellar graphite iron; Fatigue limit; Ultimate tensile strength; Graphite ferret; Inter-dendritic hydraulic diameter; CAST-IRON; STRENGTH; MORPHOLOGY;
D O I
10.1016/j.msea.2020.140617
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Demanding environmental legislation and improve performance specifications requires increasing fatigue strength for the engine components that are made of lamellar graphite iron (LGI). Components design, metallurgy and casting conditions define the microstructure formation and mechanical properties. The graphite inclusions embedded in the metallic matrix acting as defects and have a detrimental effect on the fatigue strength of LGI. The cooling conditions determine the coarseness of the microstructure and also have, a great impact on the fatigue resistance. The experimental material was an LGI alloy produced with three different solidification times. A fully reversed fatigue test was performed, and various microstructure features were quantitatively estimated by utilizing the Gumbel's statistics of extremes. The stereological parameter of Hydraulic Diameter of the Inter-dendritic Phase and the graphite Feret size found to be the most suitable microstructure parameters to be correlated with the fatigue limit. The results also indicate the sizeable effect of the solidification time on the fatigue limit. Several other microstructure features that have been reported to influence the tensile strength were also found to be related to the fatigue limit. The obtained endurance ratio ranges from 0.25 to 0.30, a value that is in line with previous investigations.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] ON FATIGUE LIMIT IN ALPHA-IRON
    BERGSTROM, Y
    VINGSBO, O
    LAGERBERG, G
    MATERIALS SCIENCE AND ENGINEERING, 1970, 5 (03): : 153 - +
  • [32] Investigation of kinetics of borided ductile and lamellar graphite cast iron
    Yusuf Kayali
    Yelda Akcin
    Ersan Mertgenc
    Barış Gokce
    Protection of Metals and Physical Chemistry of Surfaces, 2017, 53 : 127 - 132
  • [33] Investigation of Kinetics of Borided Ductile and Lamellar Graphite Cast Iron
    Kayali, Yusuf
    Akcin, Yelda
    Mertgenc, Ersan
    Gokce, Baris
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2017, 53 (01) : 127 - 132
  • [34] Influence of microstructure and micro notches on the fatigue limit
    Kerscher, Eberhard
    XVII INTERNATIONAL COLLOQUIUM ON MECHANICAL FATIGUE OF METALS (ICMFM17), 2014, 74 : 210 - 217
  • [35] The Effect of Nb Supplement on Material Characteristics of Iron with Lamellar Graphite
    Devecili, Ahmet Oktay
    Yakut, Rifat
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2014, 2014
  • [36] VISUALIZING DISLOCATION STRUCTURE OF HYPEREUTECTIC LAMELLAR GRAPHITE OF CAST IRON
    SIDORENK.RA
    PHYSICS OF METALS AND METALLOGRAPHY-USSR, 1969, 28 (04): : 204 - &
  • [37] Quantification of the solidification morphology of lamellar and spheroidal graphite cast iron
    Mampaey, F
    INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 1999, 11 (05) : 307 - 312
  • [38] The Influence of Lamellar Graphite Cast Iron Annealing on Hardness and Structure
    Roucka, J.
    Prochazka, J.
    Kana, V
    Krutis, V
    Nedelova, K.
    ARCHIVES OF FOUNDRY ENGINEERING, 2019, 19 (04) : 105 - 112
  • [39] Strength Prediction for Pearlitic Lamellar Graphite Iron: Model Validation
    Fourlakidis, Vasilios
    Belov, Ilia
    Dioszegi, Attila
    METALS, 2018, 8 (09):
  • [40] DISLOCATION GROWTH OF HYPEREUTECTIC LAMELLAR GRAPHITE CRYSTALS IN CAST IRON
    SIDORENKO, RA
    PHYSICS OF METALS AND METALLOGRAPHY-USSR, 1967, 23 (04): : 159 - +