Fatigue limit and microstructure in lamellar graphite iron

被引:1
|
作者
Fourlakidis, Vasilios [1 ]
Schmidt, Pal [2 ]
Jarfors, Anders E. W. [1 ]
Svidro, Peter [1 ]
Dioszegi, Attila [1 ]
机构
[1] Jonkoping Univ, Dept Mat & Mfg, Box 1026, SE-55111 Jonkoping, Sweden
[2] Volvo Technol AB, S-40508 Gothenburg, Sweden
关键词
Lamellar graphite iron; Fatigue limit; Ultimate tensile strength; Graphite ferret; Inter-dendritic hydraulic diameter; CAST-IRON; STRENGTH; MORPHOLOGY;
D O I
10.1016/j.msea.2020.140617
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Demanding environmental legislation and improve performance specifications requires increasing fatigue strength for the engine components that are made of lamellar graphite iron (LGI). Components design, metallurgy and casting conditions define the microstructure formation and mechanical properties. The graphite inclusions embedded in the metallic matrix acting as defects and have a detrimental effect on the fatigue strength of LGI. The cooling conditions determine the coarseness of the microstructure and also have, a great impact on the fatigue resistance. The experimental material was an LGI alloy produced with three different solidification times. A fully reversed fatigue test was performed, and various microstructure features were quantitatively estimated by utilizing the Gumbel's statistics of extremes. The stereological parameter of Hydraulic Diameter of the Inter-dendritic Phase and the graphite Feret size found to be the most suitable microstructure parameters to be correlated with the fatigue limit. The results also indicate the sizeable effect of the solidification time on the fatigue limit. Several other microstructure features that have been reported to influence the tensile strength were also found to be related to the fatigue limit. The obtained endurance ratio ranges from 0.25 to 0.30, a value that is in line with previous investigations.
引用
收藏
页数:7
相关论文
共 50 条
  • [21] Relationship between Fatigue Limit and Defect Size in Spheroidal Graphite Cast Iron with Different Graphite Spheroidization Ratios and Microstructures
    Shiraki, Naoto
    Watanabe, Takuya
    Kanno, Toshitake
    MATERIALS TRANSACTIONS, 2015, 56 (12) : 2010 - 2016
  • [22] Estimation of Fatigue Limit of Spheroidal Graphite Cast Iron Using X-ray CT
    Shiraki, Naoto
    Tanaka, Kaho
    Sugawara, Akira
    Fujimoto, Ryosuke
    Tomizawa, Masami
    Hara, Takumi
    MATERIALS TRANSACTIONS, 2021, 62 (12) : 1745 - 1749
  • [23] MODELING THE KINETICS OF SOLIDIFICATION OF CAST IRON WITH LAMELLAR GRAPHITE
    Kapturkiewicz, W.
    Fras, E.
    Burbelko, A. A.
    ARCHIVES OF METALLURGY AND MATERIALS, 2009, 54 (02) : 369 - 380
  • [24] STRUCTURAL FRATURES OF ALUMINIUM IRON WITH LAMELLAR OR SPHEROIDAL GRAPHITE
    ZHUKOV, AA
    EPSHTEYN, LZ
    OGAREV, AP
    TOMAS, VK
    ULYANOVA, BY
    RUSSIAN METALLURGY-METALLY-USSR, 1968, (05): : 84 - &
  • [26] Fatigue behaviour and endurance limit of graphite and of aluminium-infiltrated graphite
    Papakyriacou, M
    Mayer, H
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2006, 37 (03) : 264 - 271
  • [27] The Microstructure of Graphite Spherulites in Cast Iron
    苗柏和
    方克明
    北京科技大学学报, 1989, (06) : 581 - 584
  • [28] MICROSTRUCTURE OF VERMICULAR GRAPHITE IN CAST IRON
    WANG Yanan Anshan Institute of Iron and Steel Technology
    Acta Metallurgica Sinica(English Edition), 1990, (11) : 357 - 359
  • [29] Investigation on the Thermal Fatigue and Microstructure Evolution Mechanism of Compacted Graphite Iron under Elevated Temperature
    Shi, Guo Qing
    Yang, Zhong
    Guo, Min
    Tao, Dong
    Sun, S.
    Li, J. P.
    Yan, F. H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (04) : 2593 - 2605
  • [30] Investigation on the Thermal Fatigue and Microstructure Evolution Mechanism of Compacted Graphite Iron under Elevated Temperature
    Guo Qing Shi
    Zhong Yang
    Min Guo
    Dong Tao
    S. Sun
    J. P. Li
    F. H. Yan
    Journal of Materials Engineering and Performance, 2022, 31 : 2593 - 2605