Nonequilibrium carrier recombination in highly excited epitaxial layers of 4H-SiC and free standing 3C-SiC was analyzed numerically and studied experimentally by the time-resolved free carrier absorption (FCA) technique. The measurement setup combined interband carrier excitation by a picosecond laser pulse and probing of carrier dynamics at excess carrier densities in the Delta N = 10(17)-10(20) cm(-3) range by optically or electronically delayed probe pulses, thus providing temporal resolution of 10 ps and 10 ns, respectively. FCA decay kinetics at different excitation levels and subsequent numerical modeling were used to determine the bulk lifetime, surface recombination velocity, and bimolecular (B) and Auger recombination (C) coefficients at 300 K. Bulk lifetimes of similar to 800 ns and similar to 65 ns were determined in 4H and 3C epitaxial layers, respectively. The numerical fitting of FCA kinetics in the 4H layer provided values of B = (1.2 +/- 0.4) x 10(-12) cm(3)/s and C = (7 +/- 4) x 10(-31) cm(6)/s at lower excitations while the Auger coefficient decreased to C = (0.8 +/- 0.2) x 10(-31) cm(6)/s at Delta N similar to 10(20) cm(-3) due to screening of the Coulomb-enhanced Auger recombination. In 3C crystals, these values were measured to be B = (2.0 +/- 0.5) x 10(-12) cm(3)/s and C = (2.0 +/- 0.5) x 10(-32) cm(6)/s. The tendency for a strongly increased surface recombination rate in 3C at high excitation conditions was observed experimentally and associated with the screening of the surface potential by the high density carrier plasma. (C) 2010 American Institute of Physics. [doi:10.1063/1.3459894]
引用
收藏
页数:9
相关论文
共 50 条
  • [41] Cathodoluminescence Study of 3C-SiC Epilayers Grown on 4H-SiC Substrates
    Chen, Jun
    Sazawa, Hiroyuki
    Yi, Wei
    Sekiguchi, Takashi
    JOURNAL OF ELECTRONIC MATERIALS, 2023, 52 (08) : 5075 - 5083
  • [42] Resonance Properties of 3C-SiC Nanoelectromechanical Resonator in Room-Temperature Magnetomotive Transduction
    Jun, Seong Chan
    Cho, Joon Hyong
    Kim, Whan Kyun
    Jung, Young Mo
    Hwang, Sukju
    Shin, Sangchul
    Kang, Ji Yoong
    Shin, Jeashik
    Song, Insang
    Choi, Jae-Young
    Lee, SangYoon
    Kim, Jong Min
    IEEE ELECTRON DEVICE LETTERS, 2009, 30 (10) : 1042 - 1044
  • [43] A diffraction-based technique for determination of interband absorption coefficients in bulk 3C-, 4H-and 6H-SiC crystals
    Scajev, Patrik
    Kato, Masashi
    Jarasiunas, Kestutis
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2011, 44 (36)
  • [44] 4H-to 3C-SiC polytypic transformation during oxidation
    Okojie, RS
    Xhang, M
    Pirouz, P
    Tumakha, S
    Jessen, G
    Brillson, LJ
    SILICON CARBIDE AND RELATED MATERIALS 2001, PTS 1 AND 2, PROCEEDINGS, 2002, 389-3 : 451 - 454
  • [45] Comparison of Vibration-Assisted Scratch Characteristics of SiC Polytypes (3C-, 4H-and 6H-SiC)
    Lin, Wuqing
    Hu, Zhongwei
    Chen, Yue
    Zhang, Yuqiang
    Yu, Yiqing
    Xu, Xipeng
    Zhang, Jie
    MICROMACHINES, 2022, 13 (04)
  • [46] Thermal stability of deep levels between room temperature and 1500 °C in as-grown 3C-SiC
    Alfieri, G.
    Nagasawa, H.
    Kimoto, T.
    JOURNAL OF APPLIED PHYSICS, 2009, 106 (07)
  • [47] Thermal stability of deep levels between room temperature and 1500 °c in as-grown 3C-SiC
    Alfieri, G.
    Nagasawa, H.
    Kimoto, T.
    Journal of Applied Physics, 2009, 106 (07):
  • [48] Deuterium introduction into 6H-and 3C-SiC crystals and thermal stability with annealing
    Zavada, JM
    Zavada, JM
    Wilson, RG
    Pearton, SJ
    Lee, BK
    Steckl, AJ
    STATE-OF-THE-ART PROGRAM ON COMPOUND SEMICONDUCTORS (SOTAPOCS XXXI), 1999, 99 (17): : 100 - 107
  • [49] High temperature hot electron transport in 6H- and 3C-SiC
    Weng, XM
    Cui, HL
    PHYSICA STATUS SOLIDI B-BASIC RESEARCH, 1997, 201 (01): : 161 - 166
  • [50] CVD growth of 3C-SiC on 4H/6H mesas
    Neudeck, Philip G.
    Trunek, Andrew J.
    Spry, David J.
    Powell, J. Anthony
    Du, Hui
    Skowronski, Marek
    Huang, Xian Rong
    Dudley, Michael
    CHEMICAL VAPOR DEPOSITION, 2006, 12 (8-9) : 531 - 540