Microstructural Evaluation and Tensile Properties of Al-Mg-Sc-Zr Alloys Prepared by LPBF

被引:5
|
作者
Lu, Yuxian [1 ,2 ]
Zhang, Hao [1 ]
Xue, Peng [1 ]
Wu, Lihui [1 ]
Liu, Fengchao [1 ]
Jia, Luanluan [3 ]
Ni, Dingrui [1 ]
Xiao, Bolv [1 ]
Ma, Zongyi [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shi Changxu Innovat Ctr Adv Mat, Shenyang 110016, Peoples R China
[2] Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Peoples R China
[3] Binzhou Inst Technol, Shandong Key Lab Adv Aluminum Mat & Technol, Weiqiao UCAS Sci & Technol Pk, Binzhou 256606, Peoples R China
基金
中国国家自然科学基金;
关键词
additive manufacturing; laser powder bed fusion; Al-Mg-Sc-Zr alloy; fine grain strengthening; solution strengthening; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; ENERGY DENSITY; AL-12SI ALLOY; LASER; STRENGTH; PRECIPITATION; EVOLUTION; PARAMETER; BEHAVIOR;
D O I
10.3390/cryst13060913
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Laser powder bed fusion (LPBF) is a typical additive manufacturing technology that offers significant advantages in the production of complex components. With the rapid heating and cooling characteristics of LPBF, a large amount of solid solution of alloying elements in the matrix can be achieved to form supersaturated solid solutions, thus enhancing the properties of LPBF alloys. For the unique microstructure, the heat treatment process needs to be adjusted accordingly. In this work, a Zr/Sc-modified Al-Mg alloy processed by laser powder bed fusion (LPBF) with relatively low cost and good mechanical properties was investigated. The fine microstructure was obtained under rapid solidification conditions. The nanoscale Al-3(Sc,Zr) particles precipitated at the molten pool boundary during solidification. These particles, as effective heterogeneous nucleators, further refined the & alpha;-Al grains and improved the mechanical properties of the alloy. As a result, the alloy exhibited a heterogeneous microstructure consisting of columnar grains in the center of the molten pool and equiaxed grains at the boundaries. The rapid solidification resulted in the supersaturation of solute atoms in the & alpha;-Al matrix, which significantly enhanced the solid solution strengthening effect. With the LPBF processing parameters of a combination of a laser power of 250 W, a laser scanning speed of 833 mm/s, and stripe scanning mode, the tensile strength of the alloy reached 401.4 & PLUSMN; 5.7 MPa, which was significantly higher than that of the cast alloys with aging treatment (281.1 & PLUSMN; 1.3 MPa). The heat treatment promoted the formation of secondary Al-3(Sc,Zr), Mn/Mg-rich phases. The ultimate tensile strength and elongation at fracture after aging at 325 & DEG;C for 2 h were 536.0 & PLUSMN; 1.7 MPa and 14.8 & PLUSMN; 0.8%, respectively. The results provide insight into the preparation of aluminum alloys with relatively low cost and excellent mechanical properties.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Microstructural evolution in Al-Mg-Sc-Zr alloy during severe plastic deformation and annealing
    Avtokratova, Elena
    Sitdikov, Oleg
    Mukhametdinova, Oksana
    Markushev, Michael
    Murty, S. V. S. Narayana
    Prasad, M. J. N. V.
    Kashyap, Bhagwati P.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 673 : 182 - 194
  • [32] Cryogenic properties of Al-Mg-Sc-Zr friction-stir welds
    Zhemchuzhnikova, D.
    Malopheyev, S.
    Mironov, S.
    Kaibyshev, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 598 : 387 - 395
  • [33] Effect of annealing on microstructure and mechanical properties of an Al-Mg-Sc-Zr alloy
    Shen, Jiaojiao
    Chen, Biao
    Wan, Jie
    Shen, Jianghua
    Li, Jinshan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 838
  • [34] Influence of annealing process on the structure and properties of a Al-Mg-Sc-Zr alloy
    Li, HZ
    Zhang, YH
    Yin, ZM
    Pan, QL
    Peng, ZH
    RARE METAL MATERIALS AND ENGINEERING, 1999, 28 (02) : 110 - 112
  • [35] Effect of External Field on Microstructure and Properties of Al-Mg-Sc-Zr Alloy Prepared by Laser Melting Deposition
    Zhao Yuhui
    He Chen
    Zou Jian
    Wang Zhiguo
    He Zhenfeng
    Zhao Jibin
    ACTA OPTICA SINICA, 2023, 43 (02)
  • [36] Manipulating the microstructure and tensile properties of selective laser melted Al-Mg-Sc-Zr alloy through heat treatment
    Ma, Rulong
    Peng, Chaoqun
    Cai, Zhiyong
    Wang, Richu
    Zhou, Zhaohui
    Li, Xiaogeng
    Cao, Xuanyang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 831
  • [37] Fracture toughness and high-cycle fatigue behaviour of Al-Mg and Al-Mg-Sc-Zr alloys
    Li, Zhiliang
    Jiang, Feng
    Liu, Lele
    Wang, Ying
    MATERIALS SCIENCE AND TECHNOLOGY, 2023, 39 (15) : 1961 - 1972
  • [38] Effect of Rolling on Mechanical Properties and Fatigue Behavior of an Al-Mg-Sc-Zr Alloy
    Zhemchuzhnikova, Daria
    Kaibyshev, Rustam
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 331 - 336
  • [39] Sc/Zr ratio-dependent mechanisms of strength evolution and microstructural thermal stability of multi-scale hetero-structured Al-Mg-Sc-Zr alloys
    Zha, Min
    Tian, Teng
    Jia, Hai-Long
    Zhang, Hong-Min
    Wang, Hui-Yuan
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 140 : 67 - 78
  • [40] Tensile and fatigue properties of Al-Mg-Sc-Zr alloy fine-grained by equal-channel angular pressing
    Washikita, A
    Kitagawa, K
    Kopylov, VI
    Vinogradov, A
    ULTRAFINE GRAINED MATERIALS II, 2002, : 341 - 350