Surface crack analysis of 8Cr4Mo4V steel based on Crystal/Phase microstructure model by grinding

被引:5
|
作者
Zhang, Bohan [1 ]
Liu, Haitao [1 ]
Zhang, Mingliang [1 ]
Dai, Chuyan [1 ]
Xie, Zhenwei [1 ]
Ma, Xinxin [2 ]
Sun, Yazhou [1 ]
机构
[1] Harbin Inst Technol, Sch Mechatron Engn, Dept Mech Mfg & Automat, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Grinding; Crack; Microstructure; 8Cr4Mo4V; FEM; MECHANICAL-PROPERTIES; GROWTH; OVERLOAD; DAMAGE; SPEED; ALLOY; TIP;
D O I
10.1016/j.jmapro.2023.12.016
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Metal polycrystalline materials tend to be homogeneous and isotropic at the macroscopic level, which leads it difficult to visually characterize the sprouting and expansion of cracks by traditional grinding simulation. In this study, the Johnson-Cook constitutive model was used for the finite element method (FEM) based on grinding characteristics with a high strain rate and large plastic deformation. The models are focused on the actual microstructure distribution, one of them contains grains and grain boundaries, and another contains phase organization (martensite and acicular martensite) and carbides. The study pinpoints the changes in microstructure under different grinding parameters during the grinding process and the influences on the formation of microscopic cracks. Ultimately, it was found that the shedding of large primary carbide is a critical factor for inducing surface cracks. The uncoordinated deformation between brittle carbides with the other phases is the main cause of carbide shedding. Therefore, this article visualized shows the influence of grinding parameters on surface cracks from the perspective of microstructure modeling, which is of great significance in guiding practical processing.
引用
收藏
页码:151 / 161
页数:11
相关论文
共 50 条
  • [41] 回火工艺对8Cr4Mo4V钢微观组织和力学性能的影响
    苏勇
    缪龙静
    于兴福
    夏云志
    热加工工艺, 2023, 52 (06) : 120 - 123
  • [42] 热处理工艺对8Cr4Mo4V钢疲劳裂纹扩展速率的影响
    于芸
    朱光辉
    高建杰
    理化检验(物理分册), 2012, 48 (10) : 635 - 639
  • [43] Solidification microstructure of Cr4Mo4V steel forged in the semi-solid state
    Weifeng Liu
    Yanfei Cao
    Yifeng Guo
    Mingyue Sun
    Bin Xu
    Dianzhong Li
    JournalofMaterialsScience&Technology, 2020, 38 (03) : 170 - 182
  • [44] Solidification microstructure of Cr4Mo4V steel forged in the semi-solid state
    Liu, Weifeng
    Cao, Yanfei
    Guo, Yifeng
    Sun, Mingyue
    Xu, Bin
    Li, Dianzhong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 38 : 170 - 182
  • [45] 冷处理对8Cr4Mo4V轴承钢尺寸稳定性的影响
    王松
    夏云志
    于兴福
    赵开礼
    马欣新
    金属热处理, 2018, 43 (05) : 163 - 167
  • [46] 8Cr4Mo4V轴承钢晶粒尺寸与残余应力的电冲击处理调控
    赵鸿杰
    王丰
    孙洪鑫
    谢乐春
    轴承, 2024, (11) : 37 - 42
  • [47] Optimization of Heat Treatment Process Parameters for 8Cr4Mo4V Bearing Ring Using FEA-NN- PSO Method
    Xia, Tao
    Chen, Yixin
    Song, Tianpeng
    Cui, Puchang
    Liu, Yong
    Zhu, Jingchuan
    METALS AND MATERIALS INTERNATIONAL, 2025,
  • [48] 分级固溶处理对8Cr4Mo4V钢的微观组织和硬度的影响
    于兴福
    王士杰
    郑冬月
    王全振
    苏勇
    赵文增
    邢飞
    材料研究学报, 2022, 36 (04) : 287 - 297
  • [49] 8Cr4Mo4V钢圆柱滚子外径面点状缺陷产生的原因及解决措施
    杨树新
    王晔
    李颖
    孙丽杰
    轴承, 2019, (02) : 35 - 39
  • [50] Effect of deep tempering on microstructure and mechanical properties of G13Cr4Mo4Ni4V steel
    Yu, Xingfu
    Gao, Yue
    Wang, Shijie
    Wang, Huimin
    Xia, Yunzhi
    Yang, Shuxin
    Su, Yong
    MATERIALS EXPRESS, 2021, 11 (07) : 1200 - 1206