Surface crack analysis of 8Cr4Mo4V steel based on Crystal/Phase microstructure model by grinding

被引:5
|
作者
Zhang, Bohan [1 ]
Liu, Haitao [1 ]
Zhang, Mingliang [1 ]
Dai, Chuyan [1 ]
Xie, Zhenwei [1 ]
Ma, Xinxin [2 ]
Sun, Yazhou [1 ]
机构
[1] Harbin Inst Technol, Sch Mechatron Engn, Dept Mech Mfg & Automat, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Grinding; Crack; Microstructure; 8Cr4Mo4V; FEM; MECHANICAL-PROPERTIES; GROWTH; OVERLOAD; DAMAGE; SPEED; ALLOY; TIP;
D O I
10.1016/j.jmapro.2023.12.016
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Metal polycrystalline materials tend to be homogeneous and isotropic at the macroscopic level, which leads it difficult to visually characterize the sprouting and expansion of cracks by traditional grinding simulation. In this study, the Johnson-Cook constitutive model was used for the finite element method (FEM) based on grinding characteristics with a high strain rate and large plastic deformation. The models are focused on the actual microstructure distribution, one of them contains grains and grain boundaries, and another contains phase organization (martensite and acicular martensite) and carbides. The study pinpoints the changes in microstructure under different grinding parameters during the grinding process and the influences on the formation of microscopic cracks. Ultimately, it was found that the shedding of large primary carbide is a critical factor for inducing surface cracks. The uncoordinated deformation between brittle carbides with the other phases is the main cause of carbide shedding. Therefore, this article visualized shows the influence of grinding parameters on surface cracks from the perspective of microstructure modeling, which is of great significance in guiding practical processing.
引用
收藏
页码:151 / 161
页数:11
相关论文
共 50 条
  • [21] Investigation of the Corrosion-Wear Interaction Behavior of 8Cr4Mo4V Bearing Steel at Various Corrosion Intervals
    Zhao, Chao
    Ying, Lixia
    Nie, Chongyang
    Zhu, Tianlin
    Tang, Rongxiang
    Liu, Ruxin
    COATINGS, 2024, 14 (10)
  • [22] 8Cr4Mo4V材料钢球滚动接触疲劳试验研究
    杨晓峰
    于庆杰
    王文雪
    韩松
    李正辉
    沙磊
    宋阿开
    失效分析与预防, 2021, 16 (05) : 295 - 299
  • [23] 喷砂处理对8Cr4Mo4V钢表面状态的影响
    魏英华
    袁晓光
    安敏
    周驰滨
    于兴福
    航空制造技术, 2019, 62 (21) : 40 - 46
  • [24] Evolution of wetted and corroded areas on 8Cr4Mo4V bearing steel exposed to salt water contaminated lubricant oil
    He, Wanjun
    Zeng, Qunfeng
    Xiao, Qi
    Pang, Zeming
    Wu, Yang
    Yan, Chao
    Huang, Shan
    Zhuang, Jian
    Wang, Jiahe
    Li, Haolin
    Wei, Xunkai
    CORROSION SCIENCE, 2024, 241
  • [25] Simulation of Residual Stress Evolution of 8Cr4Mo4V Steel Induced by Laser Shock and Its Influence on Fatigue Performance
    Sun Y.
    Liu W.
    Zhang H.
    Su Y.
    Wei Y.
    Liu G.
    Yu X.
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2023, 37 (12): : 933 - 942
  • [26] Characterization of vein-like structures formed in nitrided layers during plasma nitriding of 8Cr4Mo4V steel
    Niu, J. B.
    Zhang, X. H.
    Ma, X. X.
    Liu, Y.
    Wang, L. Q.
    Wu, T. B.
    MATERIALIA, 2022, 22
  • [27] Research on Contact Fatigue and Tribological Performance of Si3N4 Ceramic Ball and 8Cr4Mo4V Bearing Steel
    Wang, Wenxue
    Sha, Lei
    Yang, Xiaofeng
    Yan, Jiasen
    Liu, Jinke
    Wang, Tingjian
    Zhang, Chuanwei
    Mocaxue Xuebao/Tribology, 2024, 44 (11): : 1516 - 1527
  • [28] 8Cr4Mo4V钢制轴承外圈仿形辗扩工艺改进
    王战冶
    王超
    陈辉
    哈尔滨轴承, 2018, 39 (02) : 51 - 52+55
  • [29] 8Cr4Mo4V异形滚子盐浴软氮化工艺试验
    刘汇河
    宋海涛
    姚颖才
    李付伟
    张艺
    轴承, 2020, (04) : 15 - 18
  • [30] 8Cr4Mo4V钢大尺寸轴承外圈锻造金属流线控制
    姜宏伟
    孙慧广
    王铄
    闫国斌
    轴承, 2024, (11) : 31 - 36