Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature

被引:0
|
作者
Takahashi, Koji [1 ]
Kim, Byung-Soo [1 ]
Chu, Min-Cheol [1 ]
Sato, Shigemi [1 ]
Ando, Kotoji [1 ]
机构
[1] Department of Energy and Safety Eng., Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama-shi, Kanagawa 240-8501, Japan
关键词
Bending (deformation) - Cracks - Silicon nitride - Sintering - Strength of materials - Stress analysis - X ray diffraction analysis;
D O I
10.1299/kikaia.68.1063
中图分类号
学科分类号
摘要
Si3N4/SiC composite ceramics were sintered and subjected to three-point bending. A semi-elliptical surface crack of 100 μm in surface length was made on each specimen. A crack was healed under static bending stress of 210 MPa at 800, 900 and 1000°C Applied stress of 210 MPa is ∼70% of the bending strength of as-cracked specimen. Bending strength and static fatigue strengths of crack healed specimens were systematically investigated at each crack-healed temperature. The bending strength of crack healed specimen showed almost the same value as the smooth specimen. Thus, Si3N4SiC composite ceramics could heal a crack even under static bending stress of 210 MPa at 800, 900 and 1000 °C. Moreover, crack-healed zone bad sufficient static fatigue strength at each crack-healed temperature. These conclusions indicate that Si3N4/SiC composite ceramics has the ability to heal a crack under service condition, i.e. high temperature and applied stress.
引用
收藏
页码:1063 / 1070
相关论文
共 50 条
  • [41] In situ crack-healing behavior of Al2O3/SiC composite ceramics under cyclic-fatigue strength
    Liu, Sung-Po
    Ando, Kotoji
    Kim, Byung-Soo
    Takahashi, Koji
    INTERNATIONAL COMMUNICATIONS IN HEAT AND MASS TRANSFER, 2009, 36 (06) : 558 - 562
  • [42] Strength recovery behavior of machined alumina/SiC whisker composite by crack-healing
    Osada, Toshio
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2007, 115 (1340) : 278 - 284
  • [43] Behavior of crack growth resistance in toughened silicon nitride ceramics
    Kawamoto, H
    Hiramatsu, K
    Takigawa, Y
    Okada, A
    Usami, H
    FRACTURE AND DUCTILE VS. BRITTLE BEHAVIOR-THEORY, MODELLING AND EXPERIMENT, 1999, 539 : 113 - 118
  • [44] Behavior of crack growth resistance in toughened silicon nitride ceramics
    Kawamoto, H.
    Hiramatsu, K.
    Takigawa, Y.
    Okada, A.
    Usami, H.
    Materials Research Society Symposium - Proceedings, 1999, 539 : 113 - 118
  • [45] High temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers
    Ando, K
    Lee, SK
    Takahashi, K
    Yokouchi, M
    SMART MATERIALS III, 2005, 5648 : 29 - 36
  • [46] Critical crack-healing condition for SiC whisker reinforced alumina under stress
    Nakao, W
    Ono, M
    Lee, SK
    Takahashi, K
    Ando, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (16) : 3649 - 3655
  • [47] ACTION OF SALTS ON THE STRENGTH AND CRACK RESISTANCE OF SILICON-NITRIDE CERAMICS
    GOGOTSI, GA
    GOGOTSI, YG
    ZAVADA, VP
    SOPENKO, SI
    STRENGTH OF MATERIALS, 1984, 16 (11) : 1515 - 1519
  • [48] Effect of Salts on Strength and Crack Resistance of Silicon Nitride Ceramics.
    Gogotsi, G.A.
    Gogotsi, Yu.G.
    Zavada, V.P.
    Sopenko, S.I.
    Problemy Prochnosti, 1984, : 17 - 21
  • [49] Threshold stress for crack healing of mullite reinforced by SiC whiskers and SiC particles and resultant fatigue strength at the healing temperature
    Takahashi, Koji
    Uchiide, Kenichi
    Kimura, Yoshitaka
    Nakao, Wataru
    Ando, Kotoji
    Yokouchi, Masahiro
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (07) : 2159 - 2164
  • [50] CRACK-HEALING BEHAVIOR AND BENDING STRENGTH PROPERTIES OF SiC CERAMICS BASED ON THE TYPE OF ADDITIVE SiO2 EMPLOYED
    Nam, Ki Woo
    Kim, Jong Soon
    Park, Seung Won
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2010, 24 (15-16): : 2869 - 2874