Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature

被引:0
|
作者
Takahashi, Koji [1 ]
Kim, Byung-Soo [1 ]
Chu, Min-Cheol [1 ]
Sato, Shigemi [1 ]
Ando, Kotoji [1 ]
机构
[1] Department of Energy and Safety Eng., Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama-shi, Kanagawa 240-8501, Japan
关键词
Bending (deformation) - Cracks - Silicon nitride - Sintering - Strength of materials - Stress analysis - X ray diffraction analysis;
D O I
10.1299/kikaia.68.1063
中图分类号
学科分类号
摘要
Si3N4/SiC composite ceramics were sintered and subjected to three-point bending. A semi-elliptical surface crack of 100 μm in surface length was made on each specimen. A crack was healed under static bending stress of 210 MPa at 800, 900 and 1000°C Applied stress of 210 MPa is ∼70% of the bending strength of as-cracked specimen. Bending strength and static fatigue strengths of crack healed specimens were systematically investigated at each crack-healed temperature. The bending strength of crack healed specimen showed almost the same value as the smooth specimen. Thus, Si3N4SiC composite ceramics could heal a crack even under static bending stress of 210 MPa at 800, 900 and 1000 °C. Moreover, crack-healed zone bad sufficient static fatigue strength at each crack-healed temperature. These conclusions indicate that Si3N4/SiC composite ceramics has the ability to heal a crack under service condition, i.e. high temperature and applied stress.
引用
收藏
页码:1063 / 1070
相关论文
共 50 条
  • [31] HIGH TEMPERATURE FATIGUE BEHAVIOR OF MULLITE/SiC MULTI-COMPOSITE CRACK-HEALED
    Nakao, Wataru
    Nakamura, Jun
    Takahashi, Koji
    Ando, Kotoji
    Yokouchi, Masahiro
    MECHANICAL PROPERTIES AND PERFORMANCE OF ENGINEERING CERAMICS AND COMPOSITES II, 2007, 27 (02): : 11 - +
  • [32] Crack healing behavior of silicon carbide ceramics
    Korous, J
    Chu, MC
    Nakatani, M
    Ando, K
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (11) : 2788 - 2792
  • [33] Crack healing behavior of silicon carbide ceramics
    Korous, Jan, 1600, American Ceramic Soc, Westerville (83):
  • [34] Preparation and characterization of a silicon oxycarbide coating with crack-healing capability for silicon carbide ceramics
    Kang, Kyunghoon
    Yun, Jondo
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2011, 12 (05): : 583 - 587
  • [35] Crack-healing behavior and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900, 1000 °C)
    Takahashi, K
    Kim, BS
    Chu, MC
    Sato, S
    Ando, K
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (11) : 1971 - 1978
  • [36] Improvement of static fatigue strength Of Si3N4/SiC crack-healed under cyclic stress
    Takahashi, K
    Murase, H
    Yoshida, S
    Houjou, K
    Ando, K
    Saito, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2005, 25 (11) : 1953 - 1959
  • [37] Bending strength and crack-healing behavior of Al2O3/SiC composites ceramics
    Kim, Hae Sook
    Kim, Mi Kyung
    Kang, Sun Bae
    Ahn, Seok Hwan
    Nam, Ki Woo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 483-84 : 672 - 675
  • [38] In situ crack-healing behavior of Al2O3/SiC composite ceramics under static fatigue strength
    Liu, Sung-Po
    Ando, Kotoji
    Kim, Byung-Soo
    Takahashi, Koji
    INTERNATIONAL COMMUNICATIONS IN HEAT AND MASS TRANSFER, 2009, 36 (06) : 563 - 568
  • [39] Self-crack-healing behavior of mullite/SiC particles/SiC whiskers multi-composite and mechanical properties of the multi-composite crack-healed
    Nakao, W
    Lee, SK
    Takahashi, K
    Ando, K
    Yokouchi, M
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES 5, 2005, : 371 - 376
  • [40] Crack-healing behavior of zirconium diboride composite reinforced with silicon carbide whiskers
    Zhang, Xinghong
    Xu, Lin
    Du, Shanyi
    Han, Wenbo
    Han, Jiecai
    SCRIPTA MATERIALIA, 2008, 59 (11) : 1222 - 1225