Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature

被引:0
|
作者
Takahashi, Koji [1 ]
Kim, Byung-Soo [1 ]
Chu, Min-Cheol [1 ]
Sato, Shigemi [1 ]
Ando, Kotoji [1 ]
机构
[1] Department of Energy and Safety Eng., Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama-shi, Kanagawa 240-8501, Japan
关键词
Bending (deformation) - Cracks - Silicon nitride - Sintering - Strength of materials - Stress analysis - X ray diffraction analysis;
D O I
10.1299/kikaia.68.1063
中图分类号
学科分类号
摘要
Si3N4/SiC composite ceramics were sintered and subjected to three-point bending. A semi-elliptical surface crack of 100 μm in surface length was made on each specimen. A crack was healed under static bending stress of 210 MPa at 800, 900 and 1000°C Applied stress of 210 MPa is ∼70% of the bending strength of as-cracked specimen. Bending strength and static fatigue strengths of crack healed specimens were systematically investigated at each crack-healed temperature. The bending strength of crack healed specimen showed almost the same value as the smooth specimen. Thus, Si3N4SiC composite ceramics could heal a crack even under static bending stress of 210 MPa at 800, 900 and 1000 °C. Moreover, crack-healed zone bad sufficient static fatigue strength at each crack-healed temperature. These conclusions indicate that Si3N4/SiC composite ceramics has the ability to heal a crack under service condition, i.e. high temperature and applied stress.
引用
收藏
页码:1063 / 1070
相关论文
共 50 条
  • [21] Crack healing in silicon nitride and alumina ceramics
    Natl Inst for Research in Inorganic, Materials, Ibaraki, Japan
    J Mater Sci Lett, 22 (1976-1978):
  • [22] Crack healing in silicon nitride and alumina ceramics
    Mitomo, M
    Nishimura, T
    Tsutsumi, M
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1996, 15 (22) : 1976 - 1978
  • [23] Critical conditions for crack-healing of structural ceramics under constant or cyclic stress
    Ono, Masato
    Nakao, Wataru
    Takahashi, Koji
    Ando, Kotoji
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 461 - 464
  • [24] Crack-healing behavior of CVD grown silicon carbide
    Lee, Pete Sihyun
    Lee, Hee-Jun
    Kim, Hyun Mi
    Kim, Seong Hoon
    Park, Jae Hwa
    Shim, Kwang Bo
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2016, 17 (07): : 782 - 788
  • [25] Influence of the crack area on the crack-healing performance of silicon carbide whisker reinforced silicon nitride composite
    Hu, Jun Feng
    Qiu, Ming Yue
    Deng, Xi
    Xu, Teng Zhou
    Chen, Zhou
    MATERIALS EXPRESS, 2019, 9 (05) : 429 - 436
  • [26] Crack-healing under cyclic stress and improvement of the resultant fatigue strength of Si3N4/SiC
    Takahashi, Koji
    Ando, Kotoji
    Saito, Shinji
    SCIENCE OF ENGINEERING CERAMICS III, 2006, 317-318 : 453 - 456
  • [27] Strength of crack-healed Si3N4/SiC composite ceramics
    Chu, MC
    Ando, K
    Yao, F
    Sato, S
    FRACTURE AND STRENGTH OF SOLIDS, PTS 1 AND 2, 2000, 183-1 : 833 - 838
  • [28] Strength of crack-healed Si3N4/SiC composite ceramics
    Chu, M.C.
    Ando, K.
    Yao, F.
    Sato, S.
    Key Engineering Materials, 2000, 183 (II : 833 - 838
  • [30] Fatigue strength of crack-healed Si3N4/SiC composite ceramics
    Ando, K
    Chu, MC
    Yao, F
    Sato, S
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1999, 22 (10) : 897 - 903