HYDROGEN BLISTERING AND BUBBLE FORMATION IN METALLIC GLASSES FE40NI40P14B6 AND FE40NI38MO4B18

被引:4
|
作者
TYAGI, AK
NANDEDKAR, RV
机构
[1] Indira Gandhi Cent for Atomic, Research, Kalpakkam, India, Indira Gandhi Cent for Atomic Research, Kalpakkam, India
关键词
GLASS; METALLIC - Radiation Effects - IRON NICKEL MOLYBDENUM BORON ALLOYS - Radiation Effects - IRON NICKEL PHOSPHORUS BORON ALLOYS - Radiation Effects;
D O I
10.1016/0022-3115(87)90520-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The critical dose for blister formation is 1. 5 multiplied by 10**1**9 ions/cm**2. A comparative study of Fe//4//0Ni//4//0P//1//4B//6 in amorphous and thermally crystallized states showed that the critical dose for blistering in the amorphous state is nearly three times higher than that in the crystallized state. TEM investigations revealed the precipitation of implanted hydrogen into gas bubbles in metallic glasses as well as the crystallized alloy.
引用
收藏
页码:72 / 75
页数:4
相关论文
共 50 条
  • [21] MAGNETOMECHANICAL COUPLING IN FE40NI40B6P14 METALLIC GLASSES
    KACZKOWSKI, Z
    CHIRIAC, H
    CIOBOTARU, I
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1990, 83 (1-3) : 363 - 364
  • [22] RESPONSE OF METALLIC GLASSES FE40NI40P14B6 AND FE80B20 TO IRRADIATION WITH 800 MEV PROTONS
    COST, JR
    SOMMER, WF
    JOURNAL OF NUCLEAR MATERIALS, 1982, 103 (1-3) : 773 - 777
  • [23] GMI Effect in Annealed Fe40Ni38Mo4B18 Microwires
    Komova, E.
    Sidik, F.
    Klein, P.
    Varga, R.
    Vazquez, M.
    ACTA PHYSICA POLONICA A, 2014, 126 (01) : 74 - 75
  • [24] Influence of primary crystallization on hydrogen permeation in an Fe40Ni38Mo4B18 amorphous metallic alloy
    dos Santos, DS
    de Biasi, RS
    de Miranda, PEV
    MECHANICALLY ALLOYED, METASTABLE AND NANOCRYSTALLINE MATERIALS, PART 2, 1998, 269-2 : 819 - 824
  • [25] HYDROGEN IN FE80B20 AND FE40NI40P14B6 AMORPHOUS-ALLOYS
    MOSER, P
    MO, CM
    MOUMENE, M
    JOURNAL DE PHYSIQUE, 1983, 44 (NC-9): : 91 - 97
  • [26] Modeling of Reversible Structural Relaxation in the Fe40Ni40P14B6 Metallic Glass
    Naberezhnykh, V. P.
    Physics of Metals and Metallography, 79 (03):
  • [27] CRACKING OF AMORPHOUS FE40NI38MO4B18 INDUCED BY STATIC CHARGING WITH HYDROGEN
    LIN, JJ
    PERNG, TP
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (01): : 191 - 196
  • [28] GASEOUS-HYDROGEN EMBRITTLEMENT OF AMORPHOUS FE40NI38MO4B18 ALLOY
    LIN, JJ
    PERNG, TP
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1991, 10 (24) : 1443 - 1445
  • [29] LOW-TEMPERATURE HEAT-CAPACITY OF METALLIC GLASSES FE80P14B6,FE40NI40P14B6 AND NI80P14B6
    ONN, DG
    JOHNSON, WD
    GLEESON, PF
    DONNELLY, TA
    EGAMI, T
    LIEBERMANN, HH
    JOURNAL OF PHYSICS C-SOLID STATE PHYSICS, 1977, 10 (22): : L639 - L642
  • [30] THE OXIDATION BEHAVIOR OF AMORPHOUS ALLOY FE40NI40P14B6
    GAO, W
    CANTOR, B
    ACTA METALLURGICA, 1988, 36 (01): : 167 - 180