LASER SURFACE MELTING OF TI-6AL-4V ALLOY

被引:9
|
作者
AKGUN, OV
INAL, OT
机构
[1] Department of Materials and Metallurgical Engineering, New Mexico Institute of Mining and Technology, Socorro, 87801, NM
关键词
D O I
10.1007/BF01142062
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Surface hardening of Ti-6Al-4V alloy with laser surface melting (LSM) in a nitrogen atmosphere has been studied. In LSM, hardness increased almost three-fold in comparison to that of the substrate, the latter having a Vickers hardness of 350, by the formation of TiN in the range of 100-mu-m of melt depth. Hardness, then, decreased slowly and reached a minimum of 580 VHN at a maximum melt depth of 750-mu-m. Alpha'-Ti was formed in the heat-affected zone (HAZ) with a VHN of 450. Ageing treatments were performed for all specimens at 450-degrees-C and different ageing times (1-20 h). Short ageing treatments increased the hardness in the melted zone as well as in the HAZ (1-3 h). Long ageing treatments (7-20 h) resulted in uniform hardness distribution in the melted zone.
引用
收藏
页码:1404 / 1408
页数:5
相关论文
共 50 条
  • [41] SURFACE HARDENING OF TI-6AL-4V ALLOY BY HYDROGENATION
    WU, TI
    WU, JK
    SCRIPTA METALLURGICA ET MATERIALIA, 1991, 25 (10): : 2335 - 2338
  • [42] Use of a Laser/TIG Combination for Surface Modification of Ti-6Al-4V Alloy
    M.Labudovic and R.Kovacevic Southern Methodist University
    Journal of Materials Science & Technology, 2001, (02) : 237 - 239
  • [43] Laser Ablative Surface Treatment for Enhanced Bonding of Ti-6Al-4V Alloy
    Palmieri, Frank L.
    Watson, Kent A.
    Morales, Guillermo
    Williams, Thomas
    Hicks, Robert
    Wohl, Christopher J.
    Hopkins, John W.
    Connell, John W.
    ACS APPLIED MATERIALS & INTERFACES, 2013, 5 (04) : 1254 - 1261
  • [44] Formation of surface layers on Ti-6Al-4V titanium alloy by laser alloying
    Filip, R
    Sieniawski, J
    Pleszakov, E
    SURFACE ENGINEERING, 2006, 22 (01) : 53 - 57
  • [45] Surface deformation of Ti-6Al-4V titanium alloy under laser loading
    Yin, Fei
    Ye, Xia
    Yao, Hongbing
    FIRST OPTICS FRONTIER CONFERENCE, 2021, 11850
  • [46] Surface roughness of Selective Laser Melted Ti-6Al-4V alloy components
    Chen, Zhuoer
    Wu, Xinhua
    Tomus, Dacian
    Davies, Chris H. J.
    ADDITIVE MANUFACTURING, 2018, 21 : 91 - 103
  • [47] Use of a laser/TIG combination for surface modification of Ti-6Al-4V alloy
    Kvacevic, R. (kovacevi@seas.smu.edu), 2001, Chinese Society of Metals (17):
  • [48] Use of a Laser/TIG combination for surface modification of Ti-6Al-4V alloy
    Labudovic, M
    Kovacevic, R
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2001, 17 (02) : 237 - 239
  • [49] Optimum laser surface treatment of fatigue damaged Ti-6Al-4V alloy
    Altus, E
    Konstantino, E
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 302 (01): : 100 - 105
  • [50] Surface morphology of Ti-6Al-4V plate fabricated by vacuum selective laser melting
    Sato, Y.
    Tsukamoto, M.
    Yamashita, Y.
    APPLIED PHYSICS B-LASERS AND OPTICS, 2015, 119 (03): : 545 - 549