Initial Stages in the Metal-dusting Process on Alloy 800

被引:0
|
作者
Daniel Röhnert
Fritz Phillipp
Helfried Reuther
Till Weber
Egbert Wessel
Michael Schütze
机构
[1] Karl-Winnacker-Institut der DECHEMA e.V.,
[2] Max-Planck-Institut für Metallforschung,undefined
[3] Forschungszentrum Rossendorf,undefined
[4] Forschungszentrum Jülich,undefined
来源
Oxidation of Metals | 2007年 / 68卷
关键词
Initial stages; Incubation; Metal-dusting; Mechanisms;
D O I
暂无
中图分类号
学科分类号
摘要
The initial stages of the metal-dusting process on Alloy 800 at 620 °C were investigated by light optical microscopy, RAMAN spectroscopy, atomic-force microscopy, Auger electron spectroscopy, transmission-electron microscopy and electron back-scatter diffraction. As it turned out the incubation period for metal-dusting is characterized by simultaneous formation of a heterogeneously growing oxide scale and deposition of carbon. The material surface shows different tarnish colors depending on the substrate-grain orientation with different susceptibility to the beginning of metal-dusting attack. “Low-index” grains were not attacked within the times investigated while the other grain orientations showed pitting. Carbon is evidently incorporated into the oxide scale from the very beginning of exposure with different intensities depending on the underlying substrate-grain orientation leading to differences in the tarnish colors. As a consequence carbides are formed even underneath “dense” oxide layers. Evidently metal-dusting attack starts at positions of the oxide scale where “higher carbon concentrations” are present.
引用
收藏
页码:271 / 293
页数:22
相关论文
共 50 条
  • [21] Effect of Pressure on Metal Dusting Initiation on Alloy 800H and Alloy 600 in CO-rich Syngas
    S. Madloch
    A. S. Dorcheh
    M. C. Galetz
    Oxidation of Metals, 2018, 89 : 483 - 498
  • [22] Metal dusting of low alloy steels
    Grabke, H.J.
    Bracho-Troconis, C.B.
    Mueller-Lorenz, E.M.
    Werkstoffe und Korrosion, 1994, 45 (04): : 215 - 221
  • [23] Metal dusting behaviour of Alloy800H in laboratory carbonaceous environments under high pressure
    Nishiyama, Yoshitaka
    Kitamura, Kazuyuki
    Otsuka, Nobuo
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 7, PTS 1 AND 2, 2008, 595-598 : 649 - 660
  • [24] Effect of syngas composition on metal dusting of alloy 800H in simulated reforming gas atmospheres
    Nishiyama, Y
    Kudo, T
    Otsuka, N
    CORROSION, 2006, 62 (01) : 54 - 63
  • [25] Behavior of copper-containing high-entropy alloys in harsh metal-dusting environments
    Galetz, Mathias C.
    Schlereth, Clara
    White, Emma M. H.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2021, 72 (07): : 1232 - 1242
  • [26] METAL DUSTING OF LOW-ALLOY STEELS
    GRABKE, HJ
    BRACHOTROCONIS, CB
    MULLERLORENZ, EM
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1994, 45 (04): : 215 - 221
  • [27] METAL DUSTING OF LOW-ALLOY AND HIGH-ALLOY STEELS
    GRABKE, HJ
    CORROSION, 1995, 51 (09) : 711 - 720
  • [28] MATHEMATICAL MODEL FOR METAL DUSTING ON LOW ALLOY STEELS
    Chen, Cheng
    Zhou, Changyu
    Hu, Guiming
    Lei, Na
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, VOL 6, PTS A AND B, 2010, : 977 - 982
  • [29] AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL
    Rupp, Ryann E.
    Sham, Ting-Leung
    PROCEEDINGS OF ASME 2022 PRESSURE VESSELS AND PIPING CONFERENCE, PVP2022, VOL 1, 2022,
  • [30] Metal Dusting of Process Gas Heater Convection Tubes
    Al-Meshari A.
    van Zyl G.
    Al-Musharraf M.
    Journal of Failure Analysis and Prevention, 2017, 17 (3) : 363 - 369