Initial Stages in the Metal-dusting Process on Alloy 800

被引:0
|
作者
Daniel Röhnert
Fritz Phillipp
Helfried Reuther
Till Weber
Egbert Wessel
Michael Schütze
机构
[1] Karl-Winnacker-Institut der DECHEMA e.V.,
[2] Max-Planck-Institut für Metallforschung,undefined
[3] Forschungszentrum Rossendorf,undefined
[4] Forschungszentrum Jülich,undefined
来源
Oxidation of Metals | 2007年 / 68卷
关键词
Initial stages; Incubation; Metal-dusting; Mechanisms;
D O I
暂无
中图分类号
学科分类号
摘要
The initial stages of the metal-dusting process on Alloy 800 at 620 °C were investigated by light optical microscopy, RAMAN spectroscopy, atomic-force microscopy, Auger electron spectroscopy, transmission-electron microscopy and electron back-scatter diffraction. As it turned out the incubation period for metal-dusting is characterized by simultaneous formation of a heterogeneously growing oxide scale and deposition of carbon. The material surface shows different tarnish colors depending on the substrate-grain orientation with different susceptibility to the beginning of metal-dusting attack. “Low-index” grains were not attacked within the times investigated while the other grain orientations showed pitting. Carbon is evidently incorporated into the oxide scale from the very beginning of exposure with different intensities depending on the underlying substrate-grain orientation leading to differences in the tarnish colors. As a consequence carbides are formed even underneath “dense” oxide layers. Evidently metal-dusting attack starts at positions of the oxide scale where “higher carbon concentrations” are present.
引用
收藏
页码:271 / 293
页数:22
相关论文
共 50 条
  • [1] Initial stages in the metal-dusting process on alloy 800
    Roehnert, Daniel
    Phillipp, Fritz
    Reuther, Helfried
    Weber, Till
    Wessel, Egbert
    Schuetze, Michael
    OXIDATION OF METALS, 2007, 68 (5-6): : 271 - 293
  • [2] Initiation of Metal-Dusting Pits and a Method to Mitigate Metal-Dusting Corrosion
    Z. Zeng
    K. Natesan
    Oxidation of Metals, 2006, 66 : 1 - 20
  • [3] Initiation of metal-dusting pits and a method to mitigate metal-dusting corrosion
    Zeng, Z.
    Natesan, K.
    OXIDATION OF METALS, 2006, 66 (1-2): : 1 - 20
  • [4] CASE OF METAL-DUSTING
    CENTO, L
    METALLURGIA ITALIANA, 1973, 65 (06): : 343 - 348
  • [5] Corrosion resistance of a high-silicon alloy in metal-dusting environments
    Chun, C. M.
    Ramanarayanan, T. A.
    OXIDATION OF METALS, 2007, 67 (3-4): : 215 - 234
  • [6] Corrosion Resistance of a High-Silicon Alloy in Metal-Dusting Environments
    C. M. Chun
    T. A. Ramanarayanan
    Oxidation of Metals, 2007, 67 : 215 - 234
  • [7] Metal dusting of inlet tube made of alloy 800
    Hrivñák, I
    Caplovic, L
    Bakay, G
    Bitter, A
    KOVOVE MATERIALY-METALLIC MATERIALS, 2005, 43 (04): : 290 - 299
  • [8] Metal-dusting corrosion of low-chromium steels
    Chun, CM
    Ramanarayanan, TA
    OXIDATION OF METALS, 2004, 62 (1-2): : 71 - 92
  • [9] METAL-DUSTING CORROSION IN COAL-GASIFICATION ENVIRONMENTS
    PERKINS, RA
    COONS, WC
    RADD, FJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (08) : C253 - C253
  • [10] Relationship of carbon crystallization to the metal-dusting mechanism of nickel
    Zeng, Z
    Natesan, K
    CHEMISTRY OF MATERIALS, 2003, 15 (04) : 872 - 878