Translucency and mechanical behavior of  partially stabilized monolithic zirconia after staining, finishing procedures and artificial aging

被引:0
|
作者
Allan Oliveira da Silva
Lívia Fiorin
Adriana Claudia Lapria Faria
Ricardo Faria Ribeiro
Renata Cristina Silveira Rodrigues
机构
[1] University of São Paulo (USP),Department of Dental Materials and Prosthesis, School of Dentistry of Ribeirão Preto
[2] University of São Paulo (USP),Department of Dental Materials and Prosthesis, School of Dentistry of Ribeirão Preto
[3] University of São Paulo (USP),Department of Dental Materials and Prosthesis, School of Dentistry of Ribeirão Preto
[4] University of São Paulo (USP),Department of Dental Materials and Prosthesis, School of Dentistry of Ribeirão Preto
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Partially stabilized zirconia (5Y-PSZ) has been widely used to manufacture indirect monolithic restorations, and the effect of finishing procedures on the optical and mechanical properties of these materials are still unclear. The purpose of this study was to evaluate the effect of staining, polishing and glazing on surface roughness, crystalline phase content, microhardness, fracture toughness, dynamic elastic modulus, three-point flexural strength, strain distribution, color (∆E00/∆L/∆a/∆b), and translucency before and after artificial accelerated aging (water spray and ultraviolet) of 5Y-PSZ. Bar-shaped and rectangle-shaped specimens of the 5Y-PSZ were prepared and divided into six groups, according to finishing procedure: GC (control), GS (staining), GG (glazing), GSG (staining and glazing), GP (polishing), GSP (staining and polishing). There was a significant difference between groups for surface roughness (p < 0.05), dynamic elastic modulus (p = 0.007), microhardness (p =  < 0.05), ∆E00 (p = 0.010), and ∆a (p = 0.008). GC presented higher cubic phase content, and the stained groups (GS, GSG and GSP) presented higher monoclinic content. The different finishing procedures affected roughness, dynamic elastic modulus, microhardness, and color of 5Y-PSZ; polishing being the finish that provides minors changes to the 5Y- PSZ. Accelerated artificial aging caused color change, regardless of finishing procedure used.
引用
收藏
相关论文
共 32 条
  • [21] Mechanical and electrochemical behavior of novel electrolytes based on partially stabilized zirconia for solid oxide fuel cells
    Celik, Selahattin
    Timurkutluk, Bora
    Toros, Serkan
    Timurkutluk, Cigdem
    CERAMICS INTERNATIONAL, 2015, 41 (07) : 8785 - 8790
  • [22] MARTENSITE-TRANSFORMATION BEHAVIOR DURING ISOTHERMAL AGING IN PARTIALLY-STABILIZED ZIRCONIA WITH AND WITHOUT ALUMINA ADDITION
    TSUBAKINO, H
    SONODA, K
    NOZATO, R
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1993, 12 (03) : 196 - 198
  • [23] Wear Behavior of Monolithic Zirconia after Staining, Glazing, and Polishing Opposing Dental Restorative Materials: An In Vitro Study
    Fiorin, Livia
    Oliveira, Paulo Eduardo Barros Souza
    Silva, Allan Oliveira da
    Faria, Adriana Claudia Lapria
    Macedo, Ana Paula
    Ribeiro, Ricardo Faria
    Rodrigues, Renata Cristina Silveira
    COATINGS, 2023, 13 (02)
  • [24] Mechanical behavior of yttria-stabilized tetragonal zirconia polycrystalline ceramic after different zirconia surface treatments
    Pozzobon, Joao Luiz
    Rocha Pereira, Gabriel Kalil
    Wandscher, Vinicius Felipe
    Dorneles, Lucio Strazzabosco
    Valandro, Luiz Felipe
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2017, 77 : 828 - 835
  • [25] Physical and mechanical behavior of zirconia-hydroxyapatite ceramics after aging in simulated body fluid
    Delgado, JA
    Martínez, S
    Morejón, L
    Ginebra, MP
    Fernández, E
    Clavaguera-Mora, MT
    Rodríguez-Viejo, J
    Gil, FJ
    Planell, JA
    BIOCERAMICS 14, 2002, 218-2 : 161 - 164
  • [26] Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing
    Sundh, A
    Molin, M
    Sjögren, G
    DENTAL MATERIALS, 2005, 21 (05) : 476 - 482
  • [27] Alumina-toughened zirconia for dental applications: Physicochemical, mechanical, optical, and residual stress characterization after artificial aging
    Bergamo, Edmara T. P.
    Cardoso, Karina B.
    Lino, Lucas F. O.
    Campos, Tiago M. B.
    Monteiro, Kelli N.
    Cesar, Paulo F.
    Genova, Luis A.
    Thim, Gilmar P.
    Coelho, Paulo G.
    Bonfante, Estevam A.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2021, 109 (08) : 1135 - 1144
  • [28] Effect of sintering procedures on optical properties, chemical composition, and grain size of monolithic zirconia ceramic at different thicknesses after hydrothermal aging: An in vitro study
    Albayrak, Haydar
    Eraslan, Ravza
    Aydinlioglu, Omer
    JOURNAL OF INDIAN PROSTHODONTIC SOCIETY, 2023, 23 (01): : 57 - 64
  • [29] Mechanical properties and phase structure of yttria-stabilized tetragonal zirconia polycrystals after low-temperature aging for long term
    Oishi, M
    Kitano, Y
    Iwanaga, H
    Masaki, T
    MATERIALS SCIENCE RESEARCH INTERNATIONAL, 1996, 2 (03): : 181 - 186
  • [30] INFLUENCE OF LONG-TERM AGING UPON THE MECHANICAL-PROPERTIES OF PARTIALLY-STABILIZED ZIRCONIA (MG-PSZ) FOR HEAT-ENGINE APPLICATIONS
    LAMON, J
    THOREL, A
    BROUSSAUD, D
    JOURNAL OF MATERIALS SCIENCE, 1986, 21 (07) : 2277 - 2282