Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing

被引:185
|
作者
Sundh, A
Molin, M
Sjögren, G
机构
[1] Umea Univ, Fac Med, Dept Odontol, SE-90187 Umea, Sweden
[2] Cty Council Vasterbotten, Natl Dent Hlth Serv, Norsjo, Sweden
[3] Cad Esthet AB, Res & Dev, Skelleftea, Sweden
关键词
all-ceramic bridges; dental ceramics; FPDs; fracture load; Y-TZP;
D O I
10.1016/j.dental.2004.07.013
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Yttria-stabilized zirconia (Y-TZP) ceramic is a high-performance material with excellent mechanical properties suitable for fixed partial dentures. The purpose of this study was to evaluate after fatigue testing, the effect of heat-treatment and veneering on the fracture resistance of frameworks manufactured using sintered and subsequently hot isostatic pressed yttrium oxide partially-stabilized zirconia (Denzir). Methods. The specimens were subjected to dynamic loading in water. Thereafter, using a universal testing machine, the fracture resistance of three-unit fixed partial dentures was determined; (i) of the frameworks as delivered after machining, (ii) after the frameworks had been subjected to heat-treatment similar to veneering with a glass-ceramic (Eris) or a feldspar-based ceramic (Vita D) and (iii) after the frameworks had been veneered with these ceramics. In addition, the fracture resistance of frameworks as delivered after machining not subjected to dynamic loading in water was determined. Results. Cyclic loading in water did not significantly (p > 0.05) affect the fracture resistance. The load necessary to fracture the frameworks as delivered after machining was significantly (p < 0.001) higher than for the heat-treated and veneered specimens. No significant difference was seen between the specimens veneered with Eris and those veneered with Vita D (p > 0.05). For all but three specimens the fractures were Located in the loading point and through one of the connectors. Significance. Heat-treatment and veneering reduce fracture resistance of hot isostatic pressed zirconia. Nevertheless, the results obtained indicate that it is an interesting material for potential in all-ceramic restorations. (c) 2004 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:476 / 482
页数:7
相关论文
共 34 条
  • [1] Fracture resistance of all-ceramic zirconia bridges with differing phase stabilizers and quality of sintering
    Sundh, Anders
    Sjogren, Goran
    DENTAL MATERIALS, 2006, 22 (08) : 778 - 784
  • [2] Effect of Incisal Porcelain Veneering Thickness on the Fracture Resistance of CAD/CAM Zirconia All-Ceramic Anterior Crowns
    Badran, Noha
    Kader, Sanaa Abdel
    Alabbassy, Fayza
    INTERNATIONAL JOURNAL OF DENTISTRY, 2019, 2019
  • [3] Fracture resistance of zirconia-based all-ceramic crowns after bur adjustment
    Rues, Stefan
    Schwindling, Franz S.
    Meyer, Andre
    Rammelsberg, Peter
    Schmitter, Marc
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2017, 125 (04) : 310 - 313
  • [5] CYCLIC FATIGUE LIFETIME PREDICTIONS OF PARTIALLY-STABILIZED ZIRCONIA WITH CRACK RESISTANCE CURVE CHARACTERISTICS
    HOFFMAN, MJ
    LENTZ, W
    SWAIN, MV
    MAI, YW
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1993, 11 (05) : 445 - 453
  • [6] Topological design of all-ceramic dental bridges for enhancing fracture resistance
    Zhang, Zhongpu
    Chen, Junning
    Li, Eric
    Li, Wei
    Swain, Michael
    Li, Qing
    INTERNATIONAL JOURNAL FOR NUMERICAL METHODS IN BIOMEDICAL ENGINEERING, 2016, 32 (06) : 1 - 13
  • [7] Fatigue testing of two porcelain-zirconia all-ceramic crown systems
    Coelho, P. G.
    Silva, N. R.
    Bonfante, E. A.
    Guess, P. C.
    Rekow, E. D.
    Thompson, V. P.
    DENTAL MATERIALS, 2009, 25 (09) : 1122 - 1127
  • [8] A thick frame decreases the fracture toughness of veneering ceramics used for zirconia-based all-ceramic restorations
    Yamauchi, Shinobu
    Miura, Shoko
    Kasahara, Shin
    Sun, Jirun
    Egusa, Hiroshi
    JOURNAL OF PROSTHODONTIC RESEARCH, 2019, 63 (02) : 184 - 192
  • [9] Effect of Incisal Porcelain Veneering Thickness on the Fracture Resistance of CAD/CAM Zirconia All-Ceramic Anterior Crowns (vol 2019, 6548519, 2019)
    Badran, Noha
    Abdel Kader, Sanaa
    Alabbassy, Fayza
    Azer, Amir
    INTERNATIONAL JOURNAL OF DENTISTRY, 2020, 2020
  • [10] THE INFLUENCE OF VENEERING PORCELAIN THICKNESS OF ALL-CERAMIC AND METAL CERAMIC CROWNS ON FAILURE RESISTANCE AFTER CYCLIC LOADING
    Shirakura, Akihiko
    Lee, Heeje
    Geminiani, Alessandro
    Ercoli, Carlo
    Feng, Changyong
    JOURNAL OF PROSTHETIC DENTISTRY, 2009, 101 (02): : 119 - 127