The tensile and fatigue fracture behavior of Zr59Cu20Al10Ni8Ti3 bulk metallic glass was investigated. It was found that under tensile load the metallic glass always displays brittle shear fracture and the shear fracture plane makes an angle of θT (=54°) with respect to the stress axis, which obviously deviates from the maximum shear stress plane (45°). Under cyclic tension-tension loading, fatigue cracks first initiate along the localized shear bands on the specimen surface, then propagate along a plane basically perpendicular to the stress axis. Tensile fracture surface observations reveal that fracture first originates from some cores, then propagates in a radiate mode, leading to the formation of a veinlike structure and final failure. The fatigue fracture processes of the specimens undergo a propagation stage of fatigue cracks followed by catastrophic failure. Based on these results, a tensile fracture criterion for bulk metallic glasses is proposed by taking the effect of normal stress into account. It is suggested that both normal and shear stresses affect the fracture process of metallic glasses and cause the deviation of the fracture angle away from 45°
引用
收藏
页码:456 / 465
页数:9
相关论文
共 50 条
  • [31] Experimental and Statistical Analysis of Fatigue Behavior in Zr-based Bulk Metallic Glass
    Yao, Zhifeng
    Qiao, Jichao
    Jean-Marc, Pelletier
    Yao, Yao
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (11) : 3010 - 3016
  • [32] Fatigue of Zr-based Bulk Metallic Glass under Cyclic-torsion
    Nakai, Y.
    Nakagawa, K.
    Mikami, K.
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10
  • [33] Fractography of fatigue crack propagation in a nanocrystalline Zr-based bulk metallic glass
    Fujita, K
    Inoue, A
    Zhang, A
    SCRIPTA MATERIALIA, 2001, 44 (8-9) : 1629 - 1633
  • [34] Stress-life fatigue behavior of a Zr-based bulk metallic glass
    Menzel, BC
    Dauskardt, RH
    ACTA MATERIALIA, 2006, 54 (04) : 935 - 943
  • [35] Comments on "The fatigue-endurance limit of a Zr-based bulk metallic glass"
    Wang, G. Y.
    Landes, J. D.
    Peker, A.
    Liaw, P. K.
    SCRIPTA MATERIALIA, 2007, 57 (01) : 65 - 68
  • [36] Fatigue strength of sharp notched plate of Zr-based bulk metallic glass
    Nakai, Y.
    Fujihara, K.
    Sei, N.
    Ando, K.
    Kim, B. K.
    FATIGUE 2010, 2010, 2 (01): : 147 - 154
  • [37] Response to comments on "The fatigue endurance limit of a Zr-based bulk metallic glass"
    Menzel, B. C.
    Dauskardt, R. H.
    SCRIPTA MATERIALIA, 2007, 57 (01) : 69 - 71
  • [38] Effect of shot peening on the fatigue life of a Zr-based bulk metallic glass
    Raghavan, R.
    Ayer, R.
    Jin, H. W.
    Marzinsky, C. N.
    Ramamurty, U.
    SCRIPTA MATERIALIA, 2008, 59 (02) : 167 - 170
  • [39] Cold rolling improves the fracture toughness of a Zr-based bulk metallic glass
    Xie, Shenghui
    Kruzic, Jamie J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 694 : 1109 - 1120
  • [40] Fracture behavior of Zr-based bulk metallic glass under impact loading
    Shin, Hyung-Seop
    Kim, Ki-Hyun
    Oh, Sang-Yeob
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2006, 20 (25-27): : 4359 - 4364