The tensile and fatigue fracture behavior of Zr59Cu20Al10Ni8Ti3 bulk metallic glass was investigated. It was found that under tensile load the metallic glass always displays brittle shear fracture and the shear fracture plane makes an angle of θT (=54°) with respect to the stress axis, which obviously deviates from the maximum shear stress plane (45°). Under cyclic tension-tension loading, fatigue cracks first initiate along the localized shear bands on the specimen surface, then propagate along a plane basically perpendicular to the stress axis. Tensile fracture surface observations reveal that fracture first originates from some cores, then propagates in a radiate mode, leading to the formation of a veinlike structure and final failure. The fatigue fracture processes of the specimens undergo a propagation stage of fatigue cracks followed by catastrophic failure. Based on these results, a tensile fracture criterion for bulk metallic glasses is proposed by taking the effect of normal stress into account. It is suggested that both normal and shear stresses affect the fracture process of metallic glasses and cause the deviation of the fracture angle away from 45°
引用
收藏
页码:456 / 465
页数:9
相关论文
共 50 条
  • [21] Effect of nanocrystalline dispersion on fatigue in a Zr-based bulk metallic glass
    Fujita, K
    Takayama, T
    Inoue, A
    Zhang, T
    Kimura, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (02) : 79 - 84
  • [22] Fatigue strength of notched components of Zr-Based bulk metallic glass
    Nakai Y.
    Fujihara K.
    Sei N.
    Ando K.
    Kim B.K.
    Zairyo/Journal of the Society of Materials Science, Japan, 2010, 59 (02) : 104 - 109
  • [23] Fatigue coaxing experiments on a Zr-based bulk-metallic glass
    El-Shabasy, Adel B.
    Lewandowski, John J.
    SCRIPTA MATERIALIA, 2010, 62 (07) : 481 - 484
  • [24] Fatigue crack propagation in a nanocrystalline Zr-based bulk metallic glass
    Fujita, K
    Inoue, A
    Zhang, T
    MATERIALS TRANSACTIONS JIM, 2000, 41 (11): : 1448 - 1453
  • [25] Fatigue crack propagation in a nanocrystalline Zr-based bulk metallic glass
    Fujita, K
    Inoue, A
    Zhang, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (09) : 787 - 792
  • [26] A Highly Fatigue-Resistant Zr-Based Bulk Metallic Glass
    Steven E. Naleway
    Rawley B. Greene
    Bernd Gludovatz
    Neil K. N. Dave
    Robert O. Ritchie
    Jamie J. Kruzic
    Metallurgical and Materials Transactions A, 2013, 44 : 5688 - 5693
  • [27] A Highly Fatigue-Resistant Zr-Based Bulk Metallic Glass
    Naleway, Steven E.
    Greene, Rawley B.
    Gludovatz, Bernd
    Dave, Neil K. N.
    Ritchie, Robert O.
    Kruzic, Jamie J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2013, 44A (13): : 5688 - 5693
  • [28] Localized shear deformation and fracture in a Zr-based bulk metallic glass
    Morikawa, Tatsuya
    Kawada, Tetsuro
    Higashida, Kenji
    THERMEC 2006, PTS 1-5, 2007, 539-543 : 2094 - +
  • [29] Mode II fracture behavior of a Zr-based bulk metallic glass
    Flores, Katharine M.
    Dauskardt, Reinhold H.
    JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2006, 54 (11) : 2418 - 2435
  • [30] TENSILE BEHAVIOR OF Zr-BASED BULK METALLIC GLASS IN HIGH-SPEED TENSILE TESTS
    Sakino, Yoshihiro
    Kuroda, Toshio
    Kim, You-Chul
    CHARACTERIZATION AND CONTROL OF INTERFACES FOR HIGH QUALITY ADVANCED MATERIALS III, 2010, 219 : 43 - 47