Dendritic Morphologies of Hot-Dip Galvanized Zn-0.2 Wt Pct Al Coatings on Steel Sheets

被引:0
|
作者
Seong Gyoon Kim
Joo-Youl Huh
Gu-Jin Chung
Hyeon-Seok Hwang
Sang-Heon Kim
机构
[1] Kunsan National University,Department of Materials Science and Engineering
[2] Korea University,Department of Materials Science and Engineering
[3] POSCO,Technical Research Laboratories
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The dendritic morphologies of hot-dip galvanized Zn-0.2 wt pct Al coatings on steel sheets with two different surface roughness conditions were systematically examined as functions of the inclination angle and axis of the Zn basal plane with respect to the sheet surface by using electron backscattered diffraction. When the inclination axis of the basal plane was ⟨12¯10⟩\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \langle 1\bar{2}10 \rangle $$\end{document}, the dendrite changed its morphology by following the sequence of six-fold → eight-fold → elongated X → elongated X + C patterns with increasing inclination angle. When the inclination axis was ⟨101¯0⟩\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \langle 10\bar{1}0 \rangle $$\end{document}, the sequence of morphological patterns on the mirror-polished steel substrate was six-fold → eight-fold → two-fold → four-fold, whereas, for the steel substrate with a rough surface, the eight-fold pattern was missing in the sequence. These sequences of morphological changes indicated the presence of a third family of preferred dendritic growth directions, in addition to the two previously known families of ⟨101¯0⟩\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \langle 10\bar{1}0 \rangle $$\end{document} and ⟨0001⟩\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \langle 0001 \rangle $$\end{document}. The third growth direction family is proposed to be those normal to the 12¯11\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \left\{ {1\bar{2}11} \right\} $$\end{document} planes. The absence of the eight-fold pattern on the rough steel surface was attributed to the surface undulation that perturbed the growth in the six weakly preferred directions toward the two strongly preferred ⟨101¯0⟩\documentclass[12pt]{minimal} \usepackage{amsmath} \usepackage{wasysym} \usepackage{amsfonts} \usepackage{amssymb} \usepackage{amsbsy} \usepackage{mathrsfs} \usepackage{upgreek} \setlength{\oddsidemargin}{-69pt} \begin{document}$$ \langle 10\bar{1}0 \rangle $$\end{document} directions.
引用
收藏
页码:3186 / 3200
页数:14
相关论文
共 50 条
  • [41] Investigation and improvement of tiny spot defects on hot-dip galvanized automotive steel sheets
    GE Zhiyong
    YANG Bo
    YANG Jiwu
    Baosteel Technical Research, 2024, 18 (02) : 32 - 38
  • [42] Cause and Remedies of Bulge Particle Defect on Surface of Hot-Dip Galvanized Steel Sheets
    Guo, Taixiong
    Dong, Xueqiang
    Zhou, Yilin
    Jin, Yongqing
    RESEARCH IN MATERIALS AND MANUFACTURING TECHNOLOGIES, PTS 1-3, 2014, 835-836 : 330 - +
  • [43] Corrosion protection of steel cut-edges by hot-dip galvanized Al(Zn,Mg) coatings in 1wt% NaCl: Part II. Numerical simulations
    Dolgikh, Olga
    Simillion, Hans
    Lamaka, Sviatlana V.
    Bastos, Alexandre C.
    Xue, Huibin B.
    Taryba, Maryna G.
    Oliveira, Andre R.
    Allely, Christian
    Van den Bossche, Bart
    Van den Bergh, Krista
    De Strycker, Joost
    Deconinck, Johan
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (05): : 780 - 792
  • [44] Deformation and damage mechanisms of zinc coatings on hot-dip galvanized steel sheets: Part II. Damage modes
    Parisot, R
    Forest, S
    Pineau, A
    Nguyen, F
    Demonet, X
    Mataigne, JM
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (03): : 813 - 823
  • [45] Corrosion protection of steel cut-edges by hot-dip galvanized Al(Zn,Mg) coatings in 1wt% NaCl: Part I. Experimental study
    Dolgikh, Olga
    Simillion, Hans
    Lamaka, Sviatlana V.
    Bastos, Alexandre C.
    Xue, Huibin B.
    Taryba, Maryna G.
    Oliveira, Andre R.
    Allely, Christian
    Van den Bossche, Bart
    Van den Bergh, Krista
    De Strycker, Joost
    Deconinck, Johan
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (05): : 768 - 779
  • [46] Deformation and damage mechanisms of zinc coatings on hot-dip galvanized steel sheets: Part 1. Deformation modes
    Parisot, R
    Forest, S
    Pineau, A
    Grillon, F
    Demonet, X
    Mataigne, JM
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (03): : 797 - 811
  • [47] Deformation and damage mechanisms of zinc coatings on hot-dip galvanized steel sheets: Part I. Deformation modes
    Rodolphe Parisot
    Samuel Forest
    André Pineau
    François Grillon
    Xavier Demonet
    Jean-Michel Mataigne
    Metallurgical and Materials Transactions A, 2004, 35 : 797 - 811
  • [48] Deformation and damage mechanisms of zinc coatings on hot-dip galvanized steel sheets: Part II. Damage modes
    Rodolphe Parisot
    Samuel Forest
    André Pineau
    François Grillon
    Xavier Demonet
    Jean-Michel Mataigne
    Metallurgical and Materials Transactions A, 2004, 35 : 813 - 823
  • [49] Microstructure and Thickness of 55 pct Al-Zn-1.6 pct Si-0.2 pct RE Hot-Dip Coatings: Experiment, Thermodynamic, and First-Principles Study
    Wu, Guangxin
    Zhang, Jieyu
    Li, Qian
    Chou, Kuochih
    Wu, Xiaochun
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2012, 43 (01): : 198 - 205
  • [50] Microstructure and Thickness of 55 pct Al-Zn-1.6 pct Si-0.2 pct RE Hot-Dip Coatings: Experiment, Thermodynamic, and First-Principles Study
    Guangxin Wu
    Jieyu Zhang
    Qian Li
    Kuochih Chou
    Xiaochun Wu
    Metallurgical and Materials Transactions B, 2012, 43 : 198 - 205