Effect of Nickel Addition on Microstructure and Mechanical Properties of the Spark Plasma Sintered Ti–6Al–4V Alloy

被引:0
|
作者
A. Muthuchamy
M. Rajadurai
A. Raja Annamalai
Dinesh K. Agrawal
机构
[1] VIT,School of Mechanical Engineering
[2] VIT,Centre for Innovative Manufacturing Research
[3] Pennsylvania State University,Material Research Institute
关键词
Ti–6Al–4V; Nickel; Spark plasma sintering; Microstructure; Mechanical properties;
D O I
暂无
中图分类号
学科分类号
摘要
The effect of nickel addition (2–6 wt%) to Ti–6Al–4V has been investigated using spark plasma sintering. The sintered samples were studied and characterized by using field emission scanning electron microscopy equipped with energy-dispersive X-ray spectroscopy and X-ray diffraction techniques. Mechanical properties of the sintered samples were determined. Results show that an increase in nickel addition significantly reduces the relative densities from 97.9 to 95.9% and the microhardness of the alloys increases from 330 to 502 HV500. The microstructural studies reveal a transformation; as Ni content increases, the equiaxed alpha phase and Widmanstatten alpha platelets in the Ti–6Al–4V alloy get refined and develop the clear grain boundaries with Widmanstatten lamellar microstructure. Sintered samples held for 30 min has the highest hardness value, while fracture morphology of the sintered compacts shows a transgranular fracture with fine dimple’s features, confirming good strength and cohesion of the grains. The percentage of elongation is greatly affected by the addition of nickel so that the sample exhibits a brittle nature with high ultimate tensile strength.
引用
收藏
页码:2127 / 2134
页数:7
相关论文
共 50 条
  • [41] Electrochemical Polishing of Additively Manufactured Ti–6Al–4V Alloy
    Yifei Zhang
    Jianzhong Li
    Shuanghang Che
    Yanwen Tian
    Metals and Materials International, 2020, 26 : 783 - 792
  • [42] Effect of severe plastic deformation on creep behaviour of a Ti–6Al–4V alloy
    Petr Kral
    Jiri Dvorak
    Sergey Zherebtsov
    Gennady Salishchev
    Marie Kvapilova
    Vaclav Sklenicka
    Journal of Materials Science, 2013, 48 : 4789 - 4795
  • [43] Enhanced wear and fatigue properties of Ti–6Al–4V alloy modified by plasma carburizing/CrN coating
    Y. G. Park
    M. Y. Wey
    S. I. Hong
    Journal of Materials Science: Materials in Medicine, 2007, 18 : 925 - 931
  • [44] Effect of particle size and sintering time on the mechanical properties of porous Ti–6Al–4V implant
    Akeem A. Azeez
    Yiporo Danyuo
    John. D. Obayemi
    SN Applied Sciences, 2020, 2
  • [45] Enhanced adhesive performance of Ti–6Al–4V/PEEK interface by loading SPEEK on Ti–6Al–4V plates
    Pan, Lei
    Wang, Menglin
    Hu, Jingling
    Xue, Pengbo
    Guo, Huaxin
    Zhong, Lang
    Yuan, Xiaosa
    Shi, Hanqiao
    International Journal of Adhesion and Adhesives, 2022, 114
  • [46] Effects of Cr and Fe Addition on Microstructure and Tensile Properties of Ti–6Al–4V Prepared by Direct Energy Deposition
    Yool Byun
    Sangwon Lee
    Seong-Moon Seo
    Jong-taek Yeom
    Seung Eon Kim
    Namhyun Kang
    Jaekeun Hong
    Metals and Materials International, 2018, 24 : 1213 - 1220
  • [47] Evaluation of the effects of plasma nitriding temperature and time on the characterisation of Ti 6Al 4V alloy
    Hosseini, S. R.
    Ahmadi, A.
    VACUUM, 2013, 87 : 30 - 39
  • [48] Effect of Multi-pass Deformation on Microstructure Evolution of Spark Plasma Sintered Ti-6Al-4V Alloy
    Dai, Xueyan
    Zhang, Zhimin
    Xue, Yong
    JOM, 2024, 76 (04) : 1844 - 1855
  • [49] Effect of Multi-pass Deformation on Microstructure Evolution of Spark Plasma Sintered Ti-6Al-4V Alloy
    Xueyan Dai
    Zhimin Zhang
    Yong Xue
    JOM, 2024, 76 : 1844 - 1855
  • [50] Characterization of Vacuum Plasma Sprayed Reinforced Hydroxyapatite Coatings on Ti–6Al–4V alloy
    Amardeep Singh
    Gurbhinder Singh
    Vikas Chawla
    Transactions of the Indian Institute of Metals, 2017, 70 : 2609 - 2628