- [21] The effect of quenching medium on the wear behaviour of a Ti–6Al–4V alloy Journal of Materials Science, 2008, 43 : 788 - 792
- [22] Effects of Laser Power on the Microstructure Evolution and Mechanical Properties of Ti–6Al–4V Alloy Manufactured by Direct Energy Deposition Metals and Materials International, 2022, 28 : 197 - 204
- [23] Dense layer, microstructure, and mechanical performances of Ti–6Al–4V alloy prepared by metal injection molding The International Journal of Advanced Manufacturing Technology, 2023, 126 : 3861 - 3871
- [25] Evolution of Mechanical Properties of Ti–6Al–4V Alloy in the Temperature Range of 20 to − 196 °C Metals and Materials International, 2021, 27 : 3214 - 3224
- [26] Microstructural characterization and mechanical properties of SLM-printed Ti–6Al–4V alloy: Effect of build orientation Journal of Materials Research, 2022, 37 : 2645 - 2660
- [27] The Effect of Lamellar and Globular α-Phase on Mechanical Behavior of Strongly Textured Ti–6Al–4V alloy Transactions of the Indian Institute of Metals, 2020, 73 : 1301 - 1309
- [29] Enhancement in Strain Hardening on Boron Addition in As-Cast Ti–6Al–4V Alloy Transactions of the Indian Institute of Metals, 2015, 68 : 195 - 205
- [30] Refining prior-β grains of Ti–6Al–4V alloy through yttrium addition Journal of Alloys and Compounds, 2021, 841