Densification kinetics, phase assemblage and hardness of spark plasma sintered Cu–10 wt% TiB2 and Cu–10 wt% TiB2–10 wt% Pb composites

被引:0
|
作者
Amit S. Sharma
Nisha Mishra
Krishanu Biswas
Bikramjit Basu
机构
[1] Indian Institute of Technology Kanpur,Department of Materials Science and Engineering
[2] Materials Research Center,undefined
[3] Indian Institute of Science,undefined
来源
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The present work demonstrates the synthesis of Cu–10 wt% TiB2 composites with a theoretical density of more than 90% by tailoring the spark plasma sintering (SPS) conditions in the temperature range of 400–700 °C. Interestingly, 10 wt% Pb addition to Cu–10 wt% TiB2 lowers the sinter density and the difference in the densification behavior of the investigated compositions was discussed in reference to the current profile recorded during a SPS cycle. The sintering kinetics and phase assemblage were also discussed in reference to surface melting of the constituents prior to bulk melting temperature, temperature dependent wettability of Pb on Cu, diffusion kinetics of Cu as well as the formation of various oxides. An important result is that a high hardness of around 2 GPa and relative density close to 92% ρtheoretical was achieved for the Cu–10 wt% TiB2–10 wt% Pb composite, and such a combination has never been achieved before using any conventional processing route.
引用
收藏
页码:1517 / 1528
页数:11
相关论文
共 50 条
  • [21] Enhanced densification of spark plasma sintered TiB2 ceramics with low content AlN additive
    Thang Phan Nguyen
    Germi, Mohammad Dashti
    Mahaseni, Zahra Hamidzadeh
    Delbari, Seyed Ali
    Quyet Van Le
    Ahmadi, Zohre
    Shokouhimehr, Mohammadreza
    Namini, Abbas Sabahi
    Asl, Mehdi Shahedi
    CERAMICS INTERNATIONAL, 2020, 46 (14) : 22127 - 22133
  • [22] Effect of Mushy State Rolling on the Microstructure, Microhardness, and Microtexture in Al-4.5wt.%Cu-5wt.%TiB2 In Situ Composite
    Mandal, Monalisa
    Mitra, Rahul
    JOM, 2016, 68 (07) : 1902 - 1908
  • [23] Effect of Mushy State Rolling on the Microstructure, Microhardness, and Microtexture in Al-4.5wt.%Cu-5wt.%TiB2 In Situ Composite
    Monalisa Mandal
    Rahul Mitra
    JOM, 2016, 68 : 1902 - 1908
  • [24] Arc erosion behavior of TiB2/Cu composites
    Li G.
    Liu Y.
    Guo X.
    Feng J.
    Song K.
    Tian B.
    Liu, Yong (liuyong@haust.edu.cn.), 2018, Beijing University of Aeronautics and Astronautics (BUAA) (35): : 616 - 622
  • [26] Investigation of indentation and dry sliding wear behaviour of Al-12.6 wt.% Si-10 wt.% TiB2 composites produced by sequential milling and pressureless sintering
    Tekoglu, Emre
    Yurekturk, Yakup
    Agaogullari, Duygu
    Dilawary, Shaikh Asad Ali
    Baydogan, Murat
    Ovecoglu, M. Lutfi
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2019, 110 (11) : 1047 - 1057
  • [27] Fabrication of TiB2/TiC Composites by Spark Plasma Sintering
    Ma Zhi-Qiang
    Ji Ying-Hu
    Wang Lian-Jun
    JOURNAL OF INORGANIC MATERIALS, 2012, 27 (09) : 961 - 964
  • [28] Effect of TiB2 on the Microstructure and Mechanical Properties of TiB2/Al-5Cu Matrix Composites
    Tang, Jingchuan
    Omar, Mohd Zaidi
    Jiang, Ripeng
    Mohamed, Intan Fadhlina
    JOM, 2025, 77 (03) : 1064 - 1078
  • [29] Effect of TiN addition on the properties of spark plasma sintered TiB2
    Koide, Manabu
    Jabri, Khaled
    Saito, Atsuhiro
    Imori, Masakazu
    Sato, Tomohiro
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2017, 125 (05) : 413 - 415
  • [30] Influence of TiB2 contents on microstructure and wear performance of TiB2/Cu composites fabricated by microwave sintering
    Zhang, Jian-Ping
    Zhang, Meng
    Ai, Yun-Long
    Zuo, Hong-Yan
    He, Wen
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (05): : 25 - 29