MODELING CONDITIONS SUITABLE FOR INITIATION OF STRESS CORROSION CRACKING IN THE HEAT AFFECTED ZONE OF THE CROSS WELD OF AUSTENITIC STEEL PIPES

被引:0
|
作者
Mares, Vratislav [1 ]
Bystriansky, Jaroslav [2 ]
Kraus, Martin [1 ]
机构
[1] VSB Tech Univ Ostrava, Ctr Adv Innovat Technol, Ostrava, Czech Republic
[2] Univ Chem & Technol Prague, Dept Met & Corros Engn, Prague, Czech Republic
关键词
Stress corrosion cracking; austenitic steel; the corrosive environment; weld joint; heat-affected zone; STAINLESS-STEELS; WATER; ENVIRONMENTS;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Steels in the cooling water circuits are most vulnerable to localized corrosion, crevice corrosion or deposit corrosion, intergranular corrosion. Austenitic steels excel in their resistance to corrosive environments. In case of use of the tubes in the cooling circuits is necessary to connect them by welding. Welding of austenitic steel is not the easy process in the field of welding. Place of weld joint then becomes a critical place for mechanical properties, but also for corrosion resistance. For application of invoking of stress corrosion cracking have been selected tubular bodies of the most commonly used steels EN 1.4541 and 1.4571. On these transverse welded tubes were manufactured artificial defects by (EDM) method. For the tests were used modified welds with artificial defect and without it. These defects were intended to localize of future damage. The thus prepared samples were exposed in corrosive environments. To induce stress corrosion cracking for tubular bodies from austenitic steels was used method of exposure in the melt MgCl2.6H(2)O [1]. It is known that method for austenitic high alloy steels, is very sensitive to the presence of local areas and under the influence of tensile stress (and residual stress). Modeling of conditions for crack initiation corrosive damage help to determine how the weld joint behaves in aggressive environment exposure. These knowledges help to prevent accidents. Of course is possible take into account the resulting knowledge in the design and life prediction of cooling water circuits.
引用
收藏
页码:924 / 929
页数:6
相关论文
共 50 条
  • [41] Understanding the stress corrosion cracking resistance of laser shock surface patterned austenitic stainless-steel weld joints
    Merbin John
    Md Shariful Islam
    Manoranjan Misra
    Pradeep L. Menezes
    The International Journal of Advanced Manufacturing Technology, 2024, 131 : 4089 - 4105
  • [42] Effect of high energy shot peening pressure on the stress corrosion cracking of the weld joint of 304 austenitic stainless steel
    Lu Zhiming
    Shi Laimin
    Zhu Shenjin
    Tang Zhidong
    Jiang Yazhou
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 637 : 170 - 174
  • [43] Understanding the stress corrosion cracking resistance of laser shock surface patterned austenitic stainless-steel weld joints
    John, Merbin
    Islam, Md Shariful
    Misra, Manoranjan
    Menezes, Pradeep L.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2024, 131 (7-8): : 4089 - 4105
  • [44] THE STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEEL HEAT EXCHANGE TUBES-THREE CASES STUDY
    Xu, Shugen
    Wang, Weiqiang
    Liu, Huadong
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2010, VOL 5, 2010, : 335 - 343
  • [45] Stress corrosion cracking behavior of 16Mn steel and heat-affected zone in alkaline sulfide with different Ph value
    Hao, Wen-Kui
    Liu, Zhi-Yong
    Ma, Yan
    Du, Cui-Wei
    Li, Xiao-Gang
    Hu, Shan-Shan
    Cailiao Gongcheng/Journal of Materials Engineering, 2015, 43 (03): : 28 - 34
  • [46] Influence of Weld Preparation Procedure and Heat Tinting on Sulfide Stress Corrosion Cracking of Duplex Stainless Steel
    Wickstroem, Leyla
    Hinds, Gareth
    Turnbull, Alan
    CORROSION, 2015, 71 (08) : 1036 - 1047
  • [47] An overview of the heat-affected zone sensitization and stress corrosion cracking behaviour of 12 % chromium type 1.4003 ferritic stainless steel
    Du Toit M.
    Van Rooyen G.T.
    Smith D.
    Welding in the World, 2007, 51 (9-10) : 41 - 50
  • [48] STUDY ON SULFIDE STRESS-CORROSION CRACKING IN LINEPIPE .2. METALLOGRAPHIC FACTORS AFFECTING SSC SUSCEPTIBILITY OF HEAT-AFFECTED ZONE IN WELD
    HYODO, T
    UME, K
    KOBAYASHI, Y
    TAIRA, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 25 (12) : B365 - B365
  • [49] Improvement of Corrosion Resistance of Simulated Weld Heat Affected Zone in High Strength Pipeline Steel Using Electropulsing
    Ding, Shengli
    Xiang, Siqi
    Ba, Xin
    Zhang, Xinfang
    Fu, Yabo
    ISIJ INTERNATIONAL, 2020, 60 (09) : 2015 - 2023
  • [50] In situ corrosion characterization of simulated weld heat affected zone on API X80 pipeline steel
    Wang, L. W.
    Liu, Z. Y.
    Cui, Z. Y.
    Du, C. W.
    Wang, X. H.
    Li, X. G.
    CORROSION SCIENCE, 2014, 85 : 401 - 410