MODELING CONDITIONS SUITABLE FOR INITIATION OF STRESS CORROSION CRACKING IN THE HEAT AFFECTED ZONE OF THE CROSS WELD OF AUSTENITIC STEEL PIPES

被引:0
|
作者
Mares, Vratislav [1 ]
Bystriansky, Jaroslav [2 ]
Kraus, Martin [1 ]
机构
[1] VSB Tech Univ Ostrava, Ctr Adv Innovat Technol, Ostrava, Czech Republic
[2] Univ Chem & Technol Prague, Dept Met & Corros Engn, Prague, Czech Republic
关键词
Stress corrosion cracking; austenitic steel; the corrosive environment; weld joint; heat-affected zone; STAINLESS-STEELS; WATER; ENVIRONMENTS;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Steels in the cooling water circuits are most vulnerable to localized corrosion, crevice corrosion or deposit corrosion, intergranular corrosion. Austenitic steels excel in their resistance to corrosive environments. In case of use of the tubes in the cooling circuits is necessary to connect them by welding. Welding of austenitic steel is not the easy process in the field of welding. Place of weld joint then becomes a critical place for mechanical properties, but also for corrosion resistance. For application of invoking of stress corrosion cracking have been selected tubular bodies of the most commonly used steels EN 1.4541 and 1.4571. On these transverse welded tubes were manufactured artificial defects by (EDM) method. For the tests were used modified welds with artificial defect and without it. These defects were intended to localize of future damage. The thus prepared samples were exposed in corrosive environments. To induce stress corrosion cracking for tubular bodies from austenitic steels was used method of exposure in the melt MgCl2.6H(2)O [1]. It is known that method for austenitic high alloy steels, is very sensitive to the presence of local areas and under the influence of tensile stress (and residual stress). Modeling of conditions for crack initiation corrosive damage help to determine how the weld joint behaves in aggressive environment exposure. These knowledges help to prevent accidents. Of course is possible take into account the resulting knowledge in the design and life prediction of cooling water circuits.
引用
收藏
页码:924 / 929
页数:6
相关论文
共 50 条
  • [21] INTERGRANULAR STRESS-CORROSION CRACKING OF LOW-TEMPERATURE SENSITIZED TYPE-304 STAINLESS-STEEL PIPE WELD HEAT-AFFECTED ZONE
    SCHMIDT, CG
    CALIGIURI, RD
    EISELSTEIN, LE
    JOURNAL OF METALS, 1983, 35 (12): : 12 - 12
  • [22] Stress-corrosion cracking of steels for gas-main pipelines: III. Failure of pipes in the heat-affected zone
    Matvienko, AF
    Filippov, YI
    Sagaradze, VV
    Pecherkina, NL
    Baldin, AV
    Grigor'ev, PA
    PHYSICS OF METALS AND METALLOGRAPHY, 2000, 90 (03): : 309 - 317
  • [23] Effects of phosphorus segregation on stress corrosion cracking in the heat-affected zone of a dissimilar weld joint between a Ni-base alloy and a low alloy steel
    Zhai, Ziqing
    Abe, Hiroshi
    Miyahara, Yuichi
    Watanabe, Yutaka
    CORROSION SCIENCE, 2015, 92 : 32 - 42
  • [24] Heat-affected zone cracking susceptibility in high nitrogen-containing austenitic stainless steel
    Woo, I
    Horinouchi, T
    Kikuchi, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (07): : 486 - 493
  • [25] Comprehensive Impact of Machined Surface Integrity on Stress Corrosion Cracking Initiation in 316 Austenitic Stainless Steel
    Liu, Zongyi
    Zhang, Wenqian
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025, 34 (05) : 4230 - 4239
  • [26] Investigation of Stress Corrosion Cracking Initiation in Machined 304 Austenitic Stainless Steel in Magnesium Chloride Environment
    Zhang, Wenqian
    Wu, Huanchun
    Wang, Siyang
    Hu, Yujin
    Fang, Kewei
    Wang, Xuelin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (01) : 191 - 204
  • [27] Investigation of Stress Corrosion Cracking Initiation in Machined 304 Austenitic Stainless Steel in Magnesium Chloride Environment
    Wenqian Zhang
    Huanchun Wu
    Siyang Wang
    Yujin Hu
    Kewei Fang
    Xuelin Wang
    Journal of Materials Engineering and Performance, 2020, 29 : 191 - 204
  • [28] Pitting Corrosion and Stress Corrosion Cracking around Heat Affected Zone in Welded Joint of CrNiMoV Rotor Steel in Chloridized High Temperature Water
    Luo, L. H.
    Huang, Y. H.
    Xuan, F. Z.
    PRESSURE VESSEL TECHNOLOGY: PREPARING FOR THE FUTURE, 2015, 130 : 1190 - 1198
  • [29] Effect of machining-induced surface residual stress on initiation of stress corrosion cracking in 316 austenitic stainless steel
    Zhang, Wenqian
    Fang, Kewei
    Hu, Yujin
    Wang, Siyang
    Wang, Xuelin
    CORROSION SCIENCE, 2016, 108 : 173 - 184
  • [30] STRESS CORROSION CRACKING AND ITS MECHANISM OF 16Mn STEEL AND HEAT-AFFECTED ZONE IN ALKALINE SULFIDE SOLUTIONS
    Hao Wenkui
    Liu Zhiyong
    Li Xiaogang
    Du Cuiwei
    ACTA METALLURGICA SINICA, 2013, 49 (07) : 881 - 889