Characteristic of cavity growth of superplastic al 7475 alloy containing a small amount of liquid

被引:0
|
作者
Iwasaki, H [1 ]
Mori, T [1 ]
Mabuchi, M [1 ]
Higashi, K [1 ]
机构
[1] Himeji Inst Technol, Dept Mat Sci & Engn, Himeji, Hyogo 6712201, Japan
关键词
cavity growth; superplasticity; 7475 alminum alloy; liquidp hase;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The change in an artificial hole during superplastic flow was measured at 773 and 806 K in AA 7475 Al alloy to investigate the effect of a small amount of liquid on plastic cavity growth during grain boundary sliding, where 773 K was lower than the incipient partial melting temperature and 806 K was slightly above the incipient partial melting temperature. The cavity growth rate at 806 K was lower than that at 773 K, indicating that cavity growth is suppressed by the presence of a small amount of liquid. The low cavity growth rate due to a small amount of liquid is suggested to be attributed to the change in the. stress state at the liquid boundaries.
引用
收藏
页码:1995 / 1997
页数:3
相关论文
共 50 条
  • [11] Microstructural evolution during superplastic deformation of a 7475 Al alloy
    Dong H Shin
    Yeon J Joo
    Woo J Kim
    Chong S Lee
    Journal of Materials Science, 1998, 33 : 3073 - 3078
  • [12] Effect of deformation schedule on cavitation in superplastic 7475 Al alloy
    Iwasaki, H
    Mori, T
    Higashi, K
    TOWARDS INNOVATION IN SUPERPLASTICITY II, 1999, 304-3 : 675 - 680
  • [13] Microstructure and texture evolution during superplastic deformation of 7475 Al alloy
    Kim, BK
    Szpunar, JA
    Alexandre, B
    Takayama, Y
    TEXTURES OF MATERIALS, PTS 1 AND 2, 2002, 408-4 : 1513 - 1518
  • [14] Cavity formation and early growth in a superplastic Al-Mg alloy
    Bae, DH
    Ghosh, AK
    ACTA MATERIALIA, 2002, 50 (03) : 511 - 523
  • [15] Superplastic forming of 7475 Al alloy by variable-pressure blowing
    Yang, CF
    Chiu, LH
    Lee, SC
    SCRIPTA MATERIALIA, 1996, 34 (10) : 1555 - 1560
  • [16] Superplastic forming of 7475 Al alloy by variable-pressure blowing
    Tatung Inst of Technology, Taipei, Taiwan
    Scripta Mater, 10 (1555-1560):
  • [17] Effect of prestrain on the superplastic behaviour of a fine grained 7475 Al alloy
    Mahidhara, RK
    Mukherjee, AK
    JOURNAL OF MATERIALS SCIENCE, 1996, 31 (02) : 381 - 385
  • [18] SUPERPLASTIC FLOW AND FAILURE IN A FINE-GRAINED 7475-AL-ALLOY
    MAHIDHARA, RK
    MATERIALS LETTERS, 1995, 25 (3-4) : 111 - 116
  • [19] Study of cavity nucleation during superplastic deformation of high strength aluminium alloy 7475
    Xinggang, Jiang
    Jianzhong, Cui
    Longxiang, Ma
    Materials Science and Engineering A, 1992, A157 (01) : 37 - 41
  • [20] THE FRACTURE PROCESS IN A FINE-GRAINED SUPERPLASTIC 7475-AL-ALLOY
    MAHIDHARA, RK
    MATERIALS & DESIGN, 1994, 15 (06): : 357 - 370