Characteristic of cavity growth of superplastic al 7475 alloy containing a small amount of liquid

被引:0
|
作者
Iwasaki, H [1 ]
Mori, T [1 ]
Mabuchi, M [1 ]
Higashi, K [1 ]
机构
[1] Himeji Inst Technol, Dept Mat Sci & Engn, Himeji, Hyogo 6712201, Japan
关键词
cavity growth; superplasticity; 7475 alminum alloy; liquidp hase;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The change in an artificial hole during superplastic flow was measured at 773 and 806 K in AA 7475 Al alloy to investigate the effect of a small amount of liquid on plastic cavity growth during grain boundary sliding, where 773 K was lower than the incipient partial melting temperature and 806 K was slightly above the incipient partial melting temperature. The cavity growth rate at 806 K was lower than that at 773 K, indicating that cavity growth is suppressed by the presence of a small amount of liquid. The low cavity growth rate due to a small amount of liquid is suggested to be attributed to the change in the. stress state at the liquid boundaries.
引用
收藏
页码:1995 / 1997
页数:3
相关论文
共 50 条
  • [1] Plastic cavity growth during superplastic flow in AA 7475 Al alloy containing a small amount of liquid
    Iwasaki, H
    Mabuchi, M
    Higashi, K
    ACTA MATERIALIA, 2001, 49 (12) : 2269 - 2275
  • [2] CAVITY GROWTH DURING SUPERPLASTIC DEFORMATION OF A 7475 AL-ALLOY
    RAO, MK
    MUKHERJEE, AK
    JOURNAL OF METALS, 1983, 35 (12): : 119 - 119
  • [3] Mechanisms of cavity growth in a fine-grained 7475 Al superplastic alloy
    Mahidhara, RK
    Mukherjee, AK
    MATERIALS & DESIGN, 1995, 16 (06): : 343 - 348
  • [4] GRAIN-GROWTH OF A SUPERPLASTIC 7475AL ALLOY
    SHERWOOD, DJ
    HAMILTON, CH
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (02): : 493 - 495
  • [5] GRAIN-GROWTH OF A SUPERPLASTIC 7475AL-ALLOY - DISCUSSION
    RIOS, PR
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (01): : 221 - 223
  • [6] STRAIN DISTRIBUTION IN THE SUPERPLASTIC 7475-AL-ALLOY
    MAHIDHARA, RK
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (09): : 1483 - 1488
  • [7] Cavity growth and filament formation of superplastically deformed Al 7475 Alloy
    Chen, CL
    Tan, MJ
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 298 (1-2): : 235 - 244
  • [8] Cavity growth and filament formation of superplastically deformed Al 7475 Alloy
    Chen, C.L.
    Tan, M.J.
    Materials Science and Engineering: A, 2001, 298 (1-2) : 235 - 244
  • [9] Microstructural evolution during superplastic deformation of a 7475 Al alloy
    Shin, DH
    Joo, YJ
    Kim, WJ
    Lee, CS
    JOURNAL OF MATERIALS SCIENCE, 1998, 33 (12) : 3073 - 3078
  • [10] CAVITY NUCLEATION IN 7475 AL-ALLOY
    RAO, MK
    MUKHERJEE, AK
    SCRIPTA METALLURGICA, 1986, 20 (03): : 411 - 414