Influence of Si3N4 on the Dry Sliding Wear Characteristics of Stir-Cast Cu-10Sn/xSi3N4 Metal Matrix Composite for Bearing Applications

被引:3
|
作者
Satheesh, Sooraj [1 ]
Priya, Gokul Krishna Gopakumar [1 ]
Venugopal, Govind [1 ]
Anil, Anuranjan [1 ]
Jayasree, Jayakrishna Ajithkumar [1 ]
Vishnu, Anandhan Ajan [1 ]
Shankar, Karthik Venkitraman [1 ]
Kumar, Anil [2 ]
机构
[1] Amrita Vishwa Vidyapeetham, Dept Mech Engn, Amritapuri 690525, India
[2] Kamla Nehru Inst Technol, Dept Mech Engn, Sultanpur 228118, India
关键词
Cu-10Sn; Si3N4; specific wear rate; coefficient of friction; hardness; density; agglomeration; dispersion hardening; BEHAVIOR; PERFORMANCE; ALUMINA;
D O I
10.3390/lubricants10120351
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Bronze metal matrix composites (MMCs) are futuristic materials that may find applications in automobile, aviation, and marine industries, specifically for propellers in submarines, bearings, and bushings for defence purposes. The present investigation studied the effect of Si3N4 (5, 10, 15 wt%) ceramic particles on the physical, metallurgical, and tribological behaviour of Cu-10Sn/Si3N4 MMCs. Cast rods of three composites and a base alloy were fabricated using the liquid metallurgy route. The microstructural characterisation for the cast samples was conducted using FESEM (Field Emission Scanning Electron Microscope), EDS (Energy Dispersive Spectroscopy), XRD (X-ray diffraction), and TEM (Transmission Electron Microscope), which revealed that the Cu-10Sn alloy reinforced with 5 wt% of Si3N4 had homogeneous distribution and perfect bonding of the Si3N4 with the bronze MMC. The dry sliding wear test was performed by varying parameters such as the applied load (10, 20, 30 N) and sliding velocity (1, 2, 3 m/s). The specific wear rate (SWR) increased against an increased load. However, the SWR and coefficient of friction decreased and then increased against an increasing sliding velocity due to tribolayer formation. The primary wear mechanism observed at low and high loads was severe delamination. In contrast, the wear mechanism was adhesion wear at high and low velocities. Amongst the researched samples, Cu-10Sn/5 wt% Si3N4 composites revealed the least SWR at a load of 10 N and sliding velocity of 2 m/s and hence can be recommended for manufacturing bearings and bushings in the automobile and defence industry.
引用
收藏
页数:22
相关论文
共 50 条
  • [21] A TEM analysis of the Si3N4/Si3N4 joint with a Cu-Zn-Ti filler metal
    Zhang, J
    Liu, CF
    Naka, M
    Meng, QC
    Zhou, Y
    JOURNAL OF MATERIALS SCIENCE, 2004, 39 (14) : 4587 - 4591
  • [22] LEAKAGE CHARACTERISTICS OF SYSTEM METAL - SI3N4 - METAL
    RUZICKA, M
    SVEC, M
    CZECHOSLOVAK JOURNAL OF PHYSICS, 1973, B 23 (10) : 1143 - 1146
  • [23] Fretting Friction and Wear Characteristics and Damage Behaviors of Si3N4 Ceramic Balls Sliding against Bearing Steel
    Wei W.
    Su Y.
    Fan H.
    Liang H.
    Song J.
    Zhang Y.
    Hu L.
    Mocaxue Xuebao/Tribology, 2022, 42 (01): : 113 - 122
  • [24] Chemical influence on wear of Si3N4 and hBN in water
    Saito, T
    Imada, Y
    Honda, F
    WEAR, 1999, 236 (1-2) : 153 - 158
  • [25] Effect of active metal on bonding characteristics and interfacial structure of the Si3N4/Si3N4 joints brazed by Ag-Cu filler metal
    Morizono, Yasuhiro
    Nakata, Takashi
    Nishida, Minoru
    Chiba, Akira
    Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan, 1995, 103 (1200): : 810 - 815
  • [26] Dry Sliding Friction and Wear Behavior of AA7075-Si3N4 Composite
    Mir Irfan Ul Haq
    Ankush Anand
    Silicon, 2018, 10 : 1819 - 1829
  • [27] Dry Sliding Friction and Wear Behavior of AA7075-Si3N4 Composite
    Ul Haq, Mir Irfan
    Anand, Ankush
    SILICON, 2018, 10 (05) : 1819 - 1829
  • [28] EFFECT OF ACTIVE METAL ON BONDING CHARACTERISTICS AND INTERFACIAL STRUCTURE OF THE SI3N4/SI3N4 JOINTS BRAZED BY AG-CU FILLER METAL
    MORIZONO, Y
    NAKATA, T
    NISHIDA, M
    CHIBA, A
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1995, 103 (08) : 810 - 815
  • [29] Effect of reinforcement content on the adhesive wear behavior of Cu10Sn5Ni/Si3N4 composites produced by stir casting
    K. Sanesh
    S. Shiam Sunder
    N. Radhika
    International Journal of Minerals, Metallurgy, and Materials, 2017, 24 : 1052 - 1060
  • [30] Effect of reinforcement content on the adhesive wear behavior of Cu10Sn5Ni/Si3N4 composites produced by stir casting
    K.Sanesh
    S.Shiam Sunder
    N.Radhika
    International Journal of Minerals Metallurgy and Materials, 2017, 24 (09) : 1052 - 1060