摘要
GaAs wafers are often sold by the manufacturers as 'epiready', meaning the substrates can be used with no further treatment. However, there is no clear agreement what epiready means, although one manufacturer recommends that they be used within 3 months of purchase. However, many growers find they are unable to obtain good growth results from their processes with untreated wafers and have to resort to long-established etching procedures. With the increase in multi-wafer molecular beam epitaxy (MBE) and metal organic vapour phase epitaxy (MOVPE) reactors, this approach is no longer viable. This work investigates the ageing of GaAs wafers stored, both under a variety of conditions [e.g. temperatures of 200 degreesC, room temperature and -20 degreesC] and assessed by atomic force microscopy (AFM) after various procedures had been performed, including annealing in molecular hydrogen using a MOVPE reactor. The primary source of ageing on an epiready GaAs wafer has been found to be the transfer oxidation from the native As2O3 (present at time = 0) to Ga2O3 (present after 24 h, 3 months and 2 years, respectively, at the storage temperatures mentioned above). This transfer oxidation does not occur across the whole surface but in discrete areas that may be associated with the step edges on the substrate surface. This is the cause of deterioration of an epiready substrate, but it can be slowed by storing the GaAs wafers at -20 degreesC. Storage in a domestic freezer has allowed even 2-year-old GaAs wafers to be used without any further preparation. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:76 / 83
页数:8
相关论文
共 50 条
  • [21] RADIAL YIELD VARIATIONS IN SEMICONDUCTOR WAFERS
    FERRISPRABHU, AV
    SMITH, LD
    BONGES, HA
    PAULSEN, JK
    IEEE CIRCUITS AND DEVICES MAGAZINE, 1987, 3 (02): : 42 - 47
  • [22] A comprehensive model for cleaning semiconductor wafers
    Burdick, G
    Eichenlaub, S
    Berman, N
    Beaudoin, S
    ULTRA CLEAN PROCESSING OF SILICON SURFACES V, 2003, 92 : 135 - 138
  • [23] NEW DEVICE FOR CHECKING SEMICONDUCTOR WAFERS
    不详
    BELL LABORATORIES RECORD, 1968, 46 (11): : 384 - &
  • [24] RELEASE OF ARSENIC FROM SEMICONDUCTOR WAFERS
    UNGERS, LJ
    JONES, JH
    MCINTYRE, AJ
    MCHENRY, CR
    AMERICAN INDUSTRIAL HYGIENE ASSOCIATION JOURNAL, 1985, 46 (08): : 416 - 420
  • [25] In situ monitoring of product wafers
    Tepermeister, I
    Conner, WT
    Alzaben, T
    Barnard, H
    Gehlert, K
    Scipione, D
    SOLID STATE TECHNOLOGY, 1996, 39 (03) : 63 - &
  • [26] Precision grinding and slicing of semiconductor substrate wafers
    Tonshoff, HK
    Hartmann, M
    2ND INTERNATIONAL CONFERENCE ON MACHINING OF ADVANCED MATERIALS (MAM), 1996, : 383 - 396
  • [27] ELLIPSOMETRIC CHARACTERIZATION OF LAYERS ON TRANSPARENT SEMICONDUCTOR WAFERS
    ZETTLER, JT
    SCHROTTKE, L
    PHYSICA STATUS SOLIDI B-BASIC RESEARCH, 1991, 163 (01): : K69 - K74
  • [28] SCRIBING AND SUBSEQUENT FRACTURING OF SILICON SEMICONDUCTOR WAFERS
    MISRA, A
    FINNIE, I
    JOURNAL OF MATERIALS SCIENCE, 1979, 14 (11) : 2567 - 2574
  • [29] Experimental study of particle deposition on semiconductor wafers
    Pui, D.Y.H.
    Ye, Y.
    Liu, B.Y.H.
    Aerosol Science and Technology, 1990, 12 (04): : 795 - 804
  • [30] Scribing of Semiconductor Wafers with the Aid of Lasers.
    Laemmel, B.
    Zscherpe, G.
    Fricke, P.
    1600, (34):