Flexural strength of glass-ceramic for structural applications

被引:20
|
作者
Collini, Luca [1 ]
Carfagni, Gianni Royer [1 ]
机构
[1] Univ Parma, Dept Ind Engn, I-43100 Parma, Italy
关键词
Glass ceramic; Glass; Bending test; Weibull statistics; Static fatigue; SLOW CRACK-GROWTH; BRITTLE MATERIALS;
D O I
10.1016/j.jeurceramsoc.2013.10.032
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to characterise the design strength of an innovative type of glass-ceramic with a view to structural applications, 4-point-bending and Ring-on-Ring biaxial bending tests have been performed. Strength is comparable with that of tempered glass but remarkably, the material breaks into large pieces like annealed glass. Interpreted through Weibull-type probability distributions, the data show much lower dispersion with respect to glass. Additional tests performed at different load rates have allowed an evaluation of the effects of static fatigue. Using a phenomenological model of equivalent-crack growth, a method is presented to calculate the decay of strength with loading time. As expected, this material is proven to be less sensitive than glass to this type of degradation. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2675 / 2685
页数:11
相关论文
共 50 条
  • [1] FLEXURAL STRENGTH OF AN INFUSED CERAMIC, GLASS-CERAMIC, AND FELDSPATHIC PORCELAIN
    GIORDANO, RA
    PELLETIER, L
    CAMPBELL, S
    POBER, R
    JOURNAL OF PROSTHETIC DENTISTRY, 1995, 73 (05): : 411 - 418
  • [2] STRENGTH OF A GLASS-CERAMIC
    KAY, JF
    DOREMUS, RH
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (04): : 350 - 350
  • [3] Evaluation of machinability and flexural strength of a novel dental machinable glass-ceramic
    Qin, Feng
    Zheng, Shucan
    Luo, Zufeng
    Li, Yong
    Guo, Ling
    Zhao, Yunfeng
    Fu, Qiang
    JOURNAL OF DENTISTRY, 2009, 37 (10) : 776 - 780
  • [4] The effect of casting conditions on the biaxial flexural strength of glass-ceramic materials
    Johnson, A
    Shareef, MY
    Walsh, JM
    Hatton, PV
    van Noort, R
    Hill, RG
    DENTAL MATERIALS, 1998, 14 (06) : 412 - 416
  • [5] Acid dissolution of ultrathin glass-ceramic and its correlation with flexural strength
    Garfias, Carolina S.
    de Goes, Mario Fernando
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (05): : 1084.e1 - 1084.e8
  • [6] EFFECT OF ACID ETCHING ON THE FLEXURAL STRENGTH OF A FELDSPATHIC PORCELAIN AND A CASTABLE GLASS-CERAMIC
    YEN, TW
    BLACKMAN, RB
    BAEZ, RJ
    JOURNAL OF PROSTHETIC DENTISTRY, 1993, 70 (03): : 224 - 233
  • [7] Effect of fluorine content on the crystallization and flexural strength of fluorosilicic mica glass-ceramic
    Cao, XG
    Tian, JM
    Qin, YJ
    Zhang, BQ
    Wang, C
    HIGH-PERFORMANCE CERAMICS 2001, PROCEEDINGS, 2002, 224-2 : 445 - 448
  • [8] Flexural Strength of Preheated Resin Composites and Bonding Properties to Glass-Ceramic and Dentin
    Kramer, Matthias Richard
    Edelhoff, Daniel
    Stawarczyk, Bogna
    MATERIALS, 2016, 9 (02)
  • [9] Biaxial flexural strength of various CAD-CAM glass-ceramic materials
    Alakkad, Layali
    Kostagianni, Aikaterini
    Finkelman, Matthew
    Maawadh, Ahmed
    Ali, Ala
    Papathanasiou, Aikaterini
    AMERICAN JOURNAL OF DENTISTRY, 2021, 34 (02): : 91 - 96
  • [10] Influence of Structural Factors on the Mechanical Strength of Glass-Ceramic Proppants
    Yu. G. Pavliukevich
    P. S. Laryionov
    I. V. Kavrus
    Glass and Ceramics, 2023, 80 : 17 - 21