Acid dissolution of ultrathin glass-ceramic and its correlation with flexural strength

被引:4
|
作者
Garfias, Carolina S. [1 ]
de Goes, Mario Fernando [1 ]
机构
[1] Univ Campinas UNICAMP, Piracicaba Dent Sch, Dept Restorat Dent, Dent Mat Div, Ave Limeira 901, BR-13414903 Piracicaba, SP, Brazil
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2022年 / 128卷 / 05期
关键词
BOND STRENGTH;
D O I
10.1016/j.prosdent.2022.08.035
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. When glass-ceramics are treated with hydrofluoric acid (HF), not only the area of application is affected but also other surfaces. Information regarding the correlation of the dissolution caused by HF and the flexural strength of the ceramic is lacking. Purpose. The purpose of this in vitro study was to investigate the effect of HF etching protocols on the flexural strength of 2 glass-ceramics, the correlation of their flexural strength with the internal and lateral dissolution, and the differences in Weibull characteristics concerning the etching protocols. Material and methods. Specimens (4x12x0.3mm) of leucite-reinforced glass-ceramic-LEU (IPS Empress) and of lithium disilicate-reinforced glass-ceramic-LD (IPS e.max) were prepared. The specimens were divided into 5 groups (n=12) according to etching protocol: control-untreated; hydrofluoric acid (HF) 5% for 20 seconds (HF5%20s); HF5%60s; HF10%20s; and HF10%60s. Flexural strength was evaluated through 3-point bend testing. The fractured specimens were submitted to a morphological and metrical analysis of each pattern (LEU I-IV, LD I-III) on the lateral surface (LS) and of the dissolution areas (mu m(2)) on the internal surface (IS) using a scanning electron microscopy (SEM) and a software program (FIJI). Flexural strength (MPa) values were analyzed by 1-way ANOVA, Bonferroni test, and Weibull and the correlation between flexural strength and dissolution by Pearson correlation coefficient (alpha=.05). Results. ANOVA revealed that the HF etching protocol was significant (P<.001) for LEU ceramic. When HF10%60s was applied, LEU showed Weibull characteristic strength (sigma theta) values lower than those of the other protocols. LD showed no difference in sigma theta and reliability (m) among the groups. The internal dissolution areas concerning LEU had a significant high negative correlation with the flexural strength (r=-0.6; P<.001). LEU-IV on the LS was the only pattern to show a significant decrease in flexural strength (r=-0.3, P<.05). Conclusions. Special care should be taken when applying hydrofluoric acid on glass-ceramic restorations. Protocols with higher hydrofluoric acid concentrations and longer application times were more related to greater internal areas of dissolution which reduced the flexural strength of leucite ceramics.
引用
收藏
页码:1084.e1 / 1084.e8
页数:8
相关论文
共 50 条
  • [1] Flexural strength of glass-ceramic for structural applications
    Collini, Luca
    Carfagni, Gianni Royer
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (11) : 2675 - 2685
  • [2] FLEXURAL STRENGTH OF AN INFUSED CERAMIC, GLASS-CERAMIC, AND FELDSPATHIC PORCELAIN
    GIORDANO, RA
    PELLETIER, L
    CAMPBELL, S
    POBER, R
    JOURNAL OF PROSTHETIC DENTISTRY, 1995, 73 (05): : 411 - 418
  • [3] EFFECT OF ACID ETCHING ON THE FLEXURAL STRENGTH OF A FELDSPATHIC PORCELAIN AND A CASTABLE GLASS-CERAMIC
    YEN, TW
    BLACKMAN, RB
    BAEZ, RJ
    JOURNAL OF PROSTHETIC DENTISTRY, 1993, 70 (03): : 224 - 233
  • [4] STRENGTH OF A GLASS-CERAMIC
    KAY, JF
    DOREMUS, RH
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (04): : 350 - 350
  • [5] Evaluation of machinability and flexural strength of a novel dental machinable glass-ceramic
    Qin, Feng
    Zheng, Shucan
    Luo, Zufeng
    Li, Yong
    Guo, Ling
    Zhao, Yunfeng
    Fu, Qiang
    JOURNAL OF DENTISTRY, 2009, 37 (10) : 776 - 780
  • [6] The effect of casting conditions on the biaxial flexural strength of glass-ceramic materials
    Johnson, A
    Shareef, MY
    Walsh, JM
    Hatton, PV
    van Noort, R
    Hill, RG
    DENTAL MATERIALS, 1998, 14 (06) : 412 - 416
  • [7] Effect of fluorine content on the crystallization and flexural strength of fluorosilicic mica glass-ceramic
    Cao, XG
    Tian, JM
    Qin, YJ
    Zhang, BQ
    Wang, C
    HIGH-PERFORMANCE CERAMICS 2001, PROCEEDINGS, 2002, 224-2 : 445 - 448
  • [8] Flexural Strength of Preheated Resin Composites and Bonding Properties to Glass-Ceramic and Dentin
    Kramer, Matthias Richard
    Edelhoff, Daniel
    Stawarczyk, Bogna
    MATERIALS, 2016, 9 (02)
  • [9] Biaxial flexural strength of various CAD-CAM glass-ceramic materials
    Alakkad, Layali
    Kostagianni, Aikaterini
    Finkelman, Matthew
    Maawadh, Ahmed
    Ali, Ala
    Papathanasiou, Aikaterini
    AMERICAN JOURNAL OF DENTISTRY, 2021, 34 (02): : 91 - 96
  • [10] The influence of veneering porcelain on the biaxial flexural strength of pressed glass-ceramic core material
    Isgró, G
    Van Der Zel, JM
    De Gee, AJ
    Feilzer, AJ
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B258 - B258