Flexural strength of glass-ceramic for structural applications

被引:20
|
作者
Collini, Luca [1 ]
Carfagni, Gianni Royer [1 ]
机构
[1] Univ Parma, Dept Ind Engn, I-43100 Parma, Italy
关键词
Glass ceramic; Glass; Bending test; Weibull statistics; Static fatigue; SLOW CRACK-GROWTH; BRITTLE MATERIALS;
D O I
10.1016/j.jeurceramsoc.2013.10.032
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to characterise the design strength of an innovative type of glass-ceramic with a view to structural applications, 4-point-bending and Ring-on-Ring biaxial bending tests have been performed. Strength is comparable with that of tempered glass but remarkably, the material breaks into large pieces like annealed glass. Interpreted through Weibull-type probability distributions, the data show much lower dispersion with respect to glass. Additional tests performed at different load rates have allowed an evaluation of the effects of static fatigue. Using a phenomenological model of equivalent-crack growth, a method is presented to calculate the decay of strength with loading time. As expected, this material is proven to be less sensitive than glass to this type of degradation. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2675 / 2685
页数:11
相关论文
共 50 条
  • [11] Structural and strength degradation of canasite glass-ceramic at Hertzian contacts
    Chan, JY
    Mecholsky, JJ
    Anusavice, KJ
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 387 - 387
  • [12] Influence of Structural Factors on the Mechanical Strength of Glass-Ceramic Proppants
    Pavliukevich, Yu. G.
    Laryionov, P. S.
    Kavrus, I. V.
    GLASS AND CERAMICS, 2023, 80 (1-2) : 17 - 21
  • [13] The influence of veneering porcelain on the biaxial flexural strength of pressed glass-ceramic core material
    Isgró, G
    Van Der Zel, JM
    De Gee, AJ
    Feilzer, AJ
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B258 - B258
  • [14] FLEXURAL STRENGTH AND FRACTURE-TOUGHNESS OF DICOR GLASS-CERAMIC AFTER EMBEDMENT MODIFICATION
    DENRY, IL
    ROSENSTIEL, SF
    JOURNAL OF DENTAL RESEARCH, 1993, 72 (03) : 572 - 576
  • [15] OBSERVATIONS ON THE STRENGTH OF A COMMERCIAL GLASS-CERAMIC
    LEWIS, D
    AMERICAN CERAMIC SOCIETY BULLETIN, 1982, 61 (11): : 1208 - 1214
  • [16] BIOACTIVE GLASS-CERAMIC SCAFFOLDS WITH HIGH-STRENGTH FOR ORTHOPEDIC APPLICATIONS
    Aguilar-Reyes, E. A.
    Leon-Patino, C. A.
    Villicana-Molina, E.
    Lefebvre, L. -P.
    BIOMATERIALS SCIENCE: PROCESSING, PROPERTIES AND APPLICATIONS IV, 2014, 251 : 1 - 10
  • [17] Flexural Strength of Ceramic and Glass Rods
    Quinn, George D.
    Sparenberg, Brian T.
    Koshy, Philip
    Ives, Lewis K.
    Jahanmir, Said
    Arola, Dwayne D.
    JOURNAL OF TESTING AND EVALUATION, 2009, 37 (03) : 222 - 244
  • [18] Analysis of Topography, Flexural Strength, and Microstructure of a Lithium Disilicate Glass-Ceramic After Surface Finishing
    Furini, Giordana Picolo
    Pecho, Oscar E.
    Alvarez-Lloret, Pedro
    Benetti, Paula
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2024, 37 (04) : 439 - 446
  • [19] Bonding strength of glass-ceramic trabecular-like coatings to ceramic substrates for prosthetic applications
    Chen, Qiang
    Baino, Francesco
    Pugno, Nicola M.
    Vitale-Brovarone, Chiara
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2013, 33 (03): : 1530 - 1538
  • [20] Transparent ceramic and glass-ceramic materials for armor applications
    Benitez, Tobias
    Gomez, Sergio Y.
    Novaes de Oliveira, Antonio Pedro
    Travitzky, Nahum
    Hotza, Dachamir
    CERAMICS INTERNATIONAL, 2017, 43 (16) : 13031 - 13046