Poly(phenylenesulfide)-based coatings for carbon steel heat exchanger tubes in geothermal environments

被引:22
|
作者
Sugama, T [1 ]
Elling, D
Gawlik, K
机构
[1] Brookhaven Natl Lab, Energy Resources Div, Energy Sci & Technol Dept, Upton, NY 11973 USA
[2] Natl Renewable Energy Lab, Golden, CO 80401 USA
关键词
D O I
10.1023/A:1020806012202
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To inhibit corrosion and fouling by calcium silicate and silica scales of the carbon steel heat exchanger tubes in geothermal power plants operating at brine temperature of 160degreesC, their internal surfaces were lined with high-temperature performance poly( phenylenesulfide) (PPS)-based coating systems. The systems included the PPS containing polytetrafluoroethylene (PTFE) as an anti-oxidant additive, silicon carbide (SiC) as a thermally conductive filler, and aluminum oxide-rich calcium aluminate (ACA) as an abrasive wear resistant filler. Then, the lined tubes underwent an eleven-month-long field exposure at the site of power plant. The results from the post-test analyses of the exposed liners revealed that these PPS coating systems had an excellent thermal stability, and satisfyingly withstood this brine temperature, and also greatly resisted the permeation of brine, demonstrating that they adequately protect the tubes against corrosion in a wet, harsh geothermal environment. Furthermore, modifying the surfaces of the PPS top layer with PTFE, retarded the hydrothermal oxidation of the liner, thereby reducing significantly the rate of scale deposition and creating surfaces unsusceptible to reactions with scales. Thus, all the scales deposited on the liner's surfaces were readily scoured off by hydroblasting at a very low pressure. By contrast, although the stainless steel tubes had a great protection against corrosion, the formation of passive oxide layers at their outermost surface sites was detrimental in that they became more susceptible to scale deposition and developed strong adherence to the scales. As a result, the high-pressure hydroblasting was required to remove this scale adhering to the tubes' surfaces. (C) 2002 Kluwer Academic Publishers.
引用
收藏
页码:4871 / 4880
页数:10
相关论文
共 50 条
  • [41] Effects of using expander and internal heat exchanger on carbon dioxide direct-expansion geothermal heat pump
    Ghazizade-Ahsaee, Hossein
    Ameri, Mehran
    APPLIED THERMAL ENGINEERING, 2018, 136 : 389 - 407
  • [42] Failure Analysis of Authentic Stainless Steel Tubes in a Vertical Fixed Shell–Tube Heat Exchanger
    Wang S.
    Xu S.
    Huang S.
    Journal of Failure Analysis and Prevention, 2018, 18 (2) : 405 - 412
  • [43] PRODUCTION OF HIGH-QUALITY WELDED STAINLESS-STEEL HEAT-EXCHANGER TUBES
    DOUGHTY, SE
    MATERIALS PERFORMANCE, 1977, 16 (01) : 19 - 22
  • [44] Operational life estimation of carbon steel heat exchanger with cooling water based on extreme value analysis
    Nakahara, Masao
    Shoji, Tetsuo
    Zairyo to Kankyo/ Corrosion Engineering, 1994, 43 (11):
  • [45] Polyphenylenesulphide-sealed Ni–Al coatings for protecting steel from corrosion and oxidation in geothermal environments
    T. Sugama
    Journal of Materials Science, 1998, 33 : 3791 - 3803
  • [46] EXPERIMENTAL STUDY ON EXCITATION OF HEAT EXCHANGER TUBES BASED ON TURBULENCE POWER SPECTRUM
    Wang, Yuqi
    Tian, Ce
    Guo, Kai
    Zhu, Guorui
    Tan, Wei
    PROCEEDINGS OF THE ASME 2020 PRESSURE VESSELS & PIPING CONFERENCE (PVP2020), VOL 4, 2020,
  • [47] Effects of metal mass on the performance of adsorption heat pumps utilizing zeolite 4A coatings synthesized on heat exchanger tubes
    Tatlier, M
    Erdem-Senatalar, A
    INTERNATIONAL JOURNAL OF REFRIGERATION-REVUE INTERNATIONALE DU FROID, 2000, 23 (04): : 260 - 268
  • [48] Condition-Based Inspection Grouping Policy for Boiler Heat Exchanger Tubes
    Huy Truong Ba
    Cholette, Michael E.
    Ma, Lin
    Kent, Geoff
    15TH WCEAM PROCEEDINGS, 2022, : 400 - 410
  • [49] Geothermal heat exchanger energy prediction based on time series and monitoring sensors optimization
    Baruque, Bruno
    Porras, Santiago
    Jove, Esteban
    Luis Calvo-Rolle, Jose
    ENERGY, 2019, 171 : 49 - 60
  • [50] IN-SERVICE INSPECTION OF CARBON-STEEL HEAT-EXCHANGER TUBE
    MATSUMOTO, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1096 - 1096