Chemical interactions between pre-oxidized Zircaloy-4 and 304 stainless steel-B4C melt at 1300°C

被引:14
|
作者
Zheng, Lichun [1 ]
Hosoi, Kazuya [1 ]
Ueda, Shigeru [1 ]
Gao, Xu [1 ]
Kitamura, Shin-ya [1 ]
Kobayashi, Yoshinao [2 ]
Sudo, Ayako [3 ]
机构
[1] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Katahira 2-1-1, Sendai, Miyagi 9808577, Japan
[2] Tokyo Inst Technol, Inst Innovat Res, Lab Adv Nucl Energy, Meguro Ku, Ookayama 2-12-1, Tokyo 1528550, Japan
[3] Japan Atom Energy Agcy, Shirakata 2-4, Tokai, Ibaraki 3191195, Japan
基金
日本科学技术振兴机构;
关键词
304 stainless steel; B4C; Zircaloy-4; ZrO2 oxide scale; Chemical interactions; Mechanism; Kinetics; REACTION BEHAVIOR; FE-ZR; B4C; OXIDATION; STEAM; TEMPERATURES; DEGRADATION; ACCIDENT; KINETICS;
D O I
10.1016/j.jnucmat.2018.05.057
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During severe nuclear accidents, control rods rapidly liquefy at temperatures above 1250 degrees C due to eutectic reaction, forming a 304 stainless steel (304SS)-B4C melt. The melt will relocate and attack surrounding fuel rod claddings made of Zircaloy-4 (Zry-4). To understand to what extent ZrO2 oxide scale formed on Zry-4 will protect Zry-4 claddings against 304SS-B4C melt attack, we studied the chemical interactions between pre-oxidized Zry-4 and 304SS-B4C melt at 1300 degrees C. Bare Zry-4 was completely dissolved in 304SS-B4C melt within 60 min. The presence of ZrO2 oxide scale on Zry-4 significantly delayed the interactions, especially when ZrO2 oxide scale was dense. Typically, the reaction zone consists of ZrB2,Zr-6(Fe, Ni, Cr) 23 and Fe-Ni-Cr metallic phase at room temperature. Due to the presence of alpha-Zr and beta-Zr in Zry-4 metal matrix, ZrO2 oxide scale becomes thermodynamically unstable. Dissolution of dense ZrO2 oxide scale can be described in three stages with different dissolution rates. Dissolution of ZrO2 oxide scale provides Zr source for the growth of reaction zone. Generally, the thickness of reaction zone linearly increases with time. Compared with the reaction couples of pre-oxidized Zry-4 and solid 316 stainless steel, both ZrO2 dissolution rate and reaction zone growth rate are much slower in the reaction couples of pre-oxidized Zry-4 and 304SS-B4C melt. The corresponding reasons were discussed. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:361 / 370
页数:10
相关论文
共 50 条
  • [31] THE OXIDATION BEHAVIOR OF ZIRCALOY-4 IN STEAM BETWEEN 600-DEGREES-C AND 1600-DEGREES-C
    LEISTIKOW, S
    SCHANZ, G
    WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1985, 36 (03): : 105 - 116
  • [32] Microstructure evolution and oxidation behavior of bi-layer CrAl-Mo coated Zircaloy-4 in steam at 1200 °C and 1300 °C
    Zhu, Chaowen
    Li, Pengcheng
    Chen, Chen
    Tian, Junhua
    Zeng, Song
    Meng, Yan
    Shen, Huahai
    Han, Xiaochun
    Zhang, Haibin
    CORROSION SCIENCE, 2022, 208
  • [33] Interfacial interactions between 304L stainless steel and Zy-4 alloy during isothermal holdings at 1050 °C
    Lebaili, Abdelatif
    Lebaili, Soltane
    Hodaj, Figiri
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 805 : 565 - 577
  • [34] Study on the difference between B4C powder and B4C pellet regarding the eutectic reaction with stainless steel
    Hong, Zhenhan
    Ahmed, Zeeshan
    Pellegrini, Marco
    Yamano, Hidemasa
    Erkan, Nejdet
    Sharma, Avadhesh Kumar
    Okamoto, Koji
    PROGRESS IN NUCLEAR ENERGY, 2024, 171
  • [35] MODELING OF B4C INTERACTIONS WITH ZIRCALOY AT HIGH-TEMPERATURES
    VESHCHUNOV, MS
    HOFMANN, P
    JOURNAL OF NUCLEAR MATERIALS, 1994, 210 (1-2) : 11 - 20
  • [36] CHEMICAL INTERACTIONS BETWEEN AL2O3, WHICH IS USED IN BURNABLE POISON RODS, AND ZIRCALOY-4 UP TO 1500-DEGREES-C
    HOFMANN, P
    MARKIEWICZ, M
    SPINO, J
    JOURNAL OF NUCLEAR MATERIALS, 1989, 166 (03) : 287 - 299
  • [37] Effect of Pre-charging Hydrogen on Corrosion Resistance of Zircaloy-4 in LiOH Aqueous Solution at 360 °C
    Xu Shitong
    Yao Meiyi
    Mao Yajing
    Liang Xue
    Peng Jianchao
    Zhou Bangxin
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (02) : 670 - 678
  • [38] UO2/ZIRCALOY-4 CHEMICAL INTERACTIONS FROM 1000-DEGREES-C TO 1700-DEGREES-C UNDER ISOTHERMAL AND TRANSIENT TEMPERATURE CONDITIONS
    HOFMANN, P
    KERWINPECK, D
    JOURNAL OF NUCLEAR MATERIALS, 1984, 124 : 80 - 105
  • [39] Investigation of corrosion-erosion behavior of stainless steel considering SS-B4C melt
    Sumita, Takehiro
    Kobayashi, Yoshinao
    JOURNAL OF NUCLEAR MATERIALS, 2019, 515 : 71 - 79
  • [40] High temperature reaction of multiple eutectic-component system: The case of solid metallic Zr and molten stainless steel-B4C
    Sumita, Takehiro
    Kobata, Masaaki
    Takano, Masahide
    Ikeda-Ohno, Atsushi
    MATERIALIA, 2021, 20