Chemical interactions between pre-oxidized Zircaloy-4 and 304 stainless steel-B4C melt at 1300°C

被引:14
|
作者
Zheng, Lichun [1 ]
Hosoi, Kazuya [1 ]
Ueda, Shigeru [1 ]
Gao, Xu [1 ]
Kitamura, Shin-ya [1 ]
Kobayashi, Yoshinao [2 ]
Sudo, Ayako [3 ]
机构
[1] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Katahira 2-1-1, Sendai, Miyagi 9808577, Japan
[2] Tokyo Inst Technol, Inst Innovat Res, Lab Adv Nucl Energy, Meguro Ku, Ookayama 2-12-1, Tokyo 1528550, Japan
[3] Japan Atom Energy Agcy, Shirakata 2-4, Tokai, Ibaraki 3191195, Japan
基金
日本科学技术振兴机构;
关键词
304 stainless steel; B4C; Zircaloy-4; ZrO2 oxide scale; Chemical interactions; Mechanism; Kinetics; REACTION BEHAVIOR; FE-ZR; B4C; OXIDATION; STEAM; TEMPERATURES; DEGRADATION; ACCIDENT; KINETICS;
D O I
10.1016/j.jnucmat.2018.05.057
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
During severe nuclear accidents, control rods rapidly liquefy at temperatures above 1250 degrees C due to eutectic reaction, forming a 304 stainless steel (304SS)-B4C melt. The melt will relocate and attack surrounding fuel rod claddings made of Zircaloy-4 (Zry-4). To understand to what extent ZrO2 oxide scale formed on Zry-4 will protect Zry-4 claddings against 304SS-B4C melt attack, we studied the chemical interactions between pre-oxidized Zry-4 and 304SS-B4C melt at 1300 degrees C. Bare Zry-4 was completely dissolved in 304SS-B4C melt within 60 min. The presence of ZrO2 oxide scale on Zry-4 significantly delayed the interactions, especially when ZrO2 oxide scale was dense. Typically, the reaction zone consists of ZrB2,Zr-6(Fe, Ni, Cr) 23 and Fe-Ni-Cr metallic phase at room temperature. Due to the presence of alpha-Zr and beta-Zr in Zry-4 metal matrix, ZrO2 oxide scale becomes thermodynamically unstable. Dissolution of dense ZrO2 oxide scale can be described in three stages with different dissolution rates. Dissolution of ZrO2 oxide scale provides Zr source for the growth of reaction zone. Generally, the thickness of reaction zone linearly increases with time. Compared with the reaction couples of pre-oxidized Zry-4 and solid 316 stainless steel, both ZrO2 dissolution rate and reaction zone growth rate are much slower in the reaction couples of pre-oxidized Zry-4 and 304SS-B4C melt. The corresponding reasons were discussed. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:361 / 370
页数:10
相关论文
共 50 条
  • [21] An investigation on diffusion bonding of Zircaloy-4 and 304L stainless steel with Ti and Ag multiple interlayers
    Pan, Houhong
    Liu, Baoshuan
    Guo, Yangyang
    Liu, Yan
    Quan, Gaofeng
    MATERIALS LETTERS, 2019, 240 : 185 - 188
  • [22] Experimental and Theoretical Analysis of Zircaloy-4 and AISI 304 Stainless Steel Material Pair in Water Sliding Conditions
    Khare, Neelima
    Limaye, Praveen Kumar
    Singh, Kulwant
    Jadhav, Dhananjay Tatyasaheb
    Bute, Arundhati
    Kalel, Navnath
    ADVANCES IN TRIBOLOGY, 2018, 2018
  • [23] Joining of stainless steel 304L with Zircaloy-4 by diffusion bonding technique using Ni and Ti interlayers
    Srikanth, V.
    Laik, A.
    Dey, G. K.
    MATERIALS & DESIGN, 2017, 126 : 141 - 154
  • [24] Interaction between mechanical loading in creep and reactivity of Zircaloy-4 at 450°C
    El Tahhan, R
    Moulin, G
    Viennot, M
    Favergeon, J
    Berger, P
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 783 - 790
  • [25] A thermogravimetric comparative study of the high temperature steam oxidation of bare and pre-oxidized Zircaloy-4, M5Framatome and Optimized ZIRLO™
    Duriez, C.
    Richez, H.
    Eymery, C.
    Desquines, J.
    Guilbert, S.
    JOURNAL OF NUCLEAR MATERIALS, 2024, 597
  • [26] Chemical interaction between granular B4C and 304L-type stainless steel materials used in BWRs in Japan
    Shibata, Hiroki
    Sakamoto, Kan
    Ouchi, Atsushi
    Kurata, Masaki
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 2015, 52 (10) : 1313 - 1317
  • [27] MODELING OF THE INTERACTIONS BETWEEN B4C AND STAINLESS-STEEL AT HIGH-TEMPERATURES
    VESHCHUNOV, MS
    HOFMANN, P
    JOURNAL OF NUCLEAR MATERIALS, 1995, 226 (1-2) : 72 - 91
  • [28] Investigation of the HCl (g) attack on pre-oxidized pure Fe, Cr, Ni and commercial 304 steel at 400 °C
    Asteman, H.
    Spiegel, M.
    CORROSION SCIENCE, 2007, 49 (09) : 3626 - 3637
  • [29] POISSON RATIO IN ZIRCALOY-4 BETWEEN 24-DEGREES-C AND 316-DEGREES-C
    SCHWENK, EB
    WHEELER, KR
    SHEARER, GD
    WEBSTER, RT
    JOURNAL OF NUCLEAR MATERIALS, 1978, 73 (01) : 129 - 131
  • [30] Modelling of B4C interactions with Zircaloy at high temperatures
    Veshchunov, M.S., 1600, (210): : 1 - 2