Patterning PDMS using a combination of wet and dry etching

被引:78
|
作者
Balakrisnan, B. [1 ]
Patil, S. [1 ]
Smela, E. [1 ]
机构
[1] Univ Maryland, Dept Mech Engn, College Pk, MD 20742 USA
基金
美国国家科学基金会;
关键词
MICROFLUIDIC DEVICES; SOFT LITHOGRAPHY; POLYDIMETHYLSILOXANE; SURFACES; POLYMER;
D O I
10.1088/0960-1317/19/4/047002
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
PDMS films of 10 mu m thickness can be patterned within 30 min by combining dry etching to achieve substantially vertical sidewalls with wet etching to achieve high etch rates and to protect the underlying substrate from attack. Dry etching alone would have taken 5 h, and wet etching alone would produce severe undercutting. In addition, using either technique alone produces undesirable surface morphologies. The mask used during etching is critical to a successful patterning outcome. E-beam evaporated Al was found to work well, adhering strongly to oxygen-plasma-treated PDMS and holding up well during both dry and wet etching. To prevent wrinkling of the PDMS, a fast deposition rate should be used.
引用
收藏
页数:7
相关论文
共 50 条
  • [31] Modification on surface roughness by combining dry and wet etching
    Lee, CC
    Hsu, WY
    SMART SENSORS, ACTUATORS, AND MEMS, PTS 1 AND 2, 2003, 5116 : 627 - 635
  • [32] TRANSPORT AND REACTION DURING ETCHING IN WET AND DRY SYSTEMS
    ALKIRE, RC
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1988, 135 (03) : C122 - C122
  • [33] Electron Beam Assisted Patterning and Dry Etching of Nafion Membranes
    Omosebi, A.
    Besser, R. S.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2011, 158 (10) : D603 - D610
  • [34] Patterning innovative conducting interpenetrating polymer network by dry etching
    Khaldi, Alexandre
    Maziz, Ali
    Plesse, Cedric
    Soyer, Caroline
    Tevssie, Dominique
    Vidal, Frederic
    Cattan, Eric
    2014 IEEE/ASME INTERNATIONAL CONFERENCE ON ADVANCED INTELLIGENT MECHATRONICS (AIM), 2014, : 1424 - 1429
  • [35] Patterning of inorganic polymer glass waveguiding films by dry etching
    Madden, S. J.
    Zhang, M.
    Luther-Davies, B.
    Charters, R.
    PHOTONICS: DESIGN, TECHNOLOGY, AND PACKAGING III, 2008, 6801
  • [36] AlSb/InAs HEMTs on InP substrate using wet and dry etching for mesa isolation
    Olivier, Aurelien
    Gehin, Thomas
    Desplanque, Ludovic
    Wallart, Xavier
    Roelens, Yannick
    Dambrine, Gilles
    Cappy, Alain
    Bollaert, Sylvain
    Lefebvre, Eric
    Malmkvist, Mikael
    Grahn, Jan
    2008 IEEE 20TH INTERNATIONAL CONFERENCE ON INDIUM PHOSPHIDE AND RELATED MATERIALS (IPRM), 2008, : 316 - +
  • [37] Patterning of ZnS-SiO2 by laser irradiation and wet etching
    Miura, H
    Toyoshima, N
    Hayashi, Y
    Sangu, S
    Iwata, N
    Takahashi, J
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2006, 45 (2B): : 1410 - 1413
  • [38] Electrode Fabrication of MWCNT-PDMS Strain Sensors by Wet-etching
    Jung, La-Hee
    Hwang, Hui-Yun
    COMPOSITES RESEARCH, 2021, 34 (06): : 387 - 393
  • [39] Fabrication of an 3D aspherical microlens for OLED with PDMS modified using a dry etching process
    Chen, Y. C.
    Pan, C. T.
    Wu, H. C.
    Lin, P. H.
    Hsu, F. T.
    Li, W. C.
    Pan, C. T.
    INNOVATION, COMMUNICATION AND ENGINEERING, 2014, : 541 - 544
  • [40] Patterning of LiNbO3 by means of ion irradiation using the electronic energy deposition and wet etching
    Gischkat, Th.
    Hartung, H.
    Schrempel, F.
    Kley, E. B.
    Tuennermann, A.
    Wesch, W.
    MICROELECTRONIC ENGINEERING, 2009, 86 (4-6) : 910 - 912