Effect of different resin luting cements on the marginal fit of lithium disilicate pressed crowns

被引:25
|
作者
Mounajjed, Radek [1 ]
Salinas, Thomas J. [2 ]
Ingr, Tomas [3 ]
Azar, Basel [1 ]
机构
[1] Palacky Univ, Inst Dent & Oral Sci, Palackeho 12, Olomouc 77900, Czech Republic
[2] Mayo Clin, Dent, Rochester, MN USA
[3] Palacky Univ, Dept Expt Phys, Olomouc, Czech Republic
来源
JOURNAL OF PROSTHETIC DENTISTRY | 2018年 / 119卷 / 06期
关键词
ALL-CERAMIC CROWNS; IN-VITRO EVALUATION; AESTHETIC RESTORATIONS; FILM THICKNESS; INTERNAL FIT; COMPOSITE; TEMPERATURE; CONVERSION; COPINGS; SYSTEMS;
D O I
10.1016/j.prosdent.2017.08.001
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. The vertical marginal discrepancy of restorations can increase upon cementation, and poor marginal fit can lead to cement dissolution, marginal discoloration, microleakage, and secondary caries. The amount of increase is related to the type of luting cement used, but how lithium disilicate pressed crowns are affected by different resin cements is unclear. Purpose. The purpose of this in vitro study was to compare the effect of using different resin luting cements on the vertical marginal discrepancy of lithium disilicate pressed crowns. Material and methods. A total of 18 intact extracted mandibular third molars were disinfected in a solution of 10% formalin for 7 days and were then prepared to receive a ceramic crown. Impressions were made with polyvinyl siloxane and lithium disilicate pressed crowns made and cemented with 1 of 3 resin luting cements. The marginal discrepancy was measured at 4 points on the finishing line of each tooth, with optical microscopy at x200 magnification before and after cementation. Statistical analysis was done with the Kruskal-Wallis test to compare the median marginal increase among the 3 groups (alpha=05). Results. The least amount of marginal increase after cementation was with Harvard PremiumFlow cement, with an average marginal increase of 42 +/- 11 mu m. RelyX Ultimate cement increased the margins by an average 45 +/- 29 mu m. The highest marginal increase was found in the Enamel Plus HRi preheated composite resin group (116 +/- 47 mu m). Conclusions. The marginal increase of pressed crowns cemented with preheated composite resin (Enamel Plus HRi) exceeded the clinically acceptable range of marginal discrepancy.
引用
收藏
页码:975 / 980
页数:6
相关论文
共 50 条
  • [21] Effect of crystallization and finish line curvature on the marginal integrity of lithium disilicate crowns
    Lee, Ki-Un
    Ko, Kyung-Ho
    Huh, Yoon-Hyuk
    Park, Chan-Jin
    Cho, Lee-Ra
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2025,
  • [22] Evaluation of the Marginal Fit of Virgilite Based Lithium Disilicate Ceramic Crowns: An In-Vitro Comparative Study
    Sultan, Sherif El Sayed
    Alsabilah, Khaled Ahmad Saud
    Alharbi, Bader Mahali
    Alnaser, Addulrhman Fahad
    JOURNAL OF PHARMACY AND BIOALLIED SCIENCES, 2024, 16 : S2479 - S2481
  • [23] Comparison of marginal fit between CAD-CAM and hot-press lithium disilicate crowns
    Dolev, Eran
    Bitterman, Yoli
    Meirowitz, Avi
    JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (01): : 124 - 128
  • [24] A comparison of the marginal gaps of lithium disilicate crowns fabricated by two different intraoral scanners
    Kwong, B.
    Dudley, J.
    AUSTRALIAN DENTAL JOURNAL, 2020, 65 (02) : 150 - 157
  • [25] A Comparative Three- and Bi-dimensional Research of the Marginal Fit of Pressed Lithium Disilicate Inlays
    Baciu, Sorana
    Berece, Cristian
    Florea, Adrian
    Burde, Alexandru Victor
    Negrutiu, Meda Lavinia
    Szuhanek, Camelia
    Sinescu, Cosmin
    Duma, Virgil Florin
    Manole, Marius
    REVISTA DE CHIMIE, 2017, 68 (06): : 1316 - 1319
  • [26] The marginal gaps of lithium disilicate crowns constructed by different scanner and milling unit combinations
    Su, Sinclair
    Dudley, James
    AUSTRALIAN DENTAL JOURNAL, 2022, 67 (02) : 125 - 131
  • [27] Correlation between Microleakage and Absolute Marginal Discrepancy in Zirconia Crowns Cemented with Four Resin Luting Cements: An In Vitro Study
    Cristian, Abad-Coronel
    Jeanette, Li
    Francisco, Martnez-Rus
    Guillermo, Pradies
    INTERNATIONAL JOURNAL OF DENTISTRY, 2016, 2016
  • [28] The Effect of Different Wax Pattern Fabrication Techniques on the Marginal Fit of Customized Lithium Disilicate Implant Abutments
    Taha, Doaa
    Nour, Moustafa
    Zohdy, Maged
    El-Etreby, Amr
    Hamdy, Amina
    Salah, Tarek
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (09): : 1018 - 1023
  • [29] Effect of different retraction and impression techniques on the marginal fit of crowns
    Woestmann, Bernd
    Rehmann, Peter
    Trost, Dieter
    Balkenhol, Markus
    JOURNAL OF DENTISTRY, 2008, 36 (07) : 508 - 512
  • [30] Effect of brand and shade of resin cements on the final color of lithium disilicate ceramic
    Dede, Dogu Omur
    Ceylan, Gozlem
    Yilmaz, Burak
    JOURNAL OF PROSTHETIC DENTISTRY, 2017, 117 (04): : 539 - 544