The influences of ECAP on the dry sliding wear behaviour of AA7075 aluminium alloy

被引:54
|
作者
Avcu, Egemen [1 ]
机构
[1] Kocaeli Univ, Ford Otosan Ihsaniye Automot Vocat Sch, Dept Machine & Met Technol, TR-41680 Kocaeli, Turkey
关键词
Aluminium alloys; Dry sliding wear; Equal channel angular processing; Microstructure; Oxide particles; Surface topography; Three-body abrasion; PITTING CORROSION-RESISTANCE; MECHANICAL-PROPERTIES; TRIBOLOGICAL PROPERTIES; ZR ALLOY; CHANNEL; MICROSTRUCTURE; EVOLUTION;
D O I
10.1016/j.triboint.2017.02.023
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The coefficient of friction and specific wear rate of the AA7075 alloy increased with ECAP despite of the enhanced hardness. The visualization of the complete wear track highlighted the peaks and valleys formed during the dry sliding and the depth of the wear tracks and volume loss increased with ECAP. The dominant wear mechanisms varied depending on the ECAP. Material pileup with smearing and adhesion mechanisms were predominant for the homogenized specimen whereas the oxidation of wear tracks and progressive breakdown of oxide layer led to the three-body abrasion caused by formed oxide particles. The variation of dominant wear mechanisms surpassed the enhanced mechanical properties obtained with ECAP and diminished the wear resistance of ECAP processed AA7075 alloy.
引用
收藏
页码:173 / 184
页数:12
相关论文
共 50 条
  • [11] Microstructure and high temperature deformation of an ultra-fine grained ECAP AA7075 aluminium alloy
    Malek, Premysl
    Turba, Krystof
    Cieslar, Miroslav
    Harcuba, Petr
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2013, 104 (01) : 3 - 10
  • [12] Experimental Investigation of Dry and Cryogenic Friction Stir Welding of AA7075 Aluminium Alloy
    Navukkarasan, A. Praveen Raj
    Sundaram, K. Shanmuga
    Sastry, C. Chandrasekhara
    Manickam, M. A. Muthu
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2021, 2021
  • [13] Fatigue Behaviour and Mechanical Properties of ECAP'ed and Thixoformed AA7075
    Kaya, Hasan
    Ucar, Mehmet
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2014, 33 (03) : 277 - 285
  • [14] Deformation homogeneity of extruded AA7075 alloy during subsequent Ecap
    Ghazani, Mehdi Shaban
    EMERGING MATERIALS RESEARCH, 2020, 9 (02) : 446 - 450
  • [15] Effect of Friction Stir Welding on the Mechanical and Microstructural Behaviour of AA7075 Aluminium Alloy
    Mahesha, C. R.
    Suprabha, R.
    Kumar, Nellore Manoj
    Kosanam, Koushik
    Anandaram, Harishchander
    Naidu, S. C. V. Ramana Murty
    Chakravarthi, M. Kalyan
    Govindarajan, Venkatesan
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2022, 2022
  • [16] Improving sliding and abrasive wear behaviour of cast A356 and wrought AA7075 aluminium alloys by plasma electrolytic oxidation
    Sabatini, G.
    Ceschini, L.
    Martini, C.
    Williams, J. A.
    Hutchings, I. M.
    MATERIALS & DESIGN, 2010, 31 (02) : 816 - 828
  • [17] Wear behaviour analysis of thermo-mechanically processed AA7075 and AA7075/SiC/Graphite composite
    Murugabalaji, V.
    Rout, Matruprasad
    Sahoo, Biranchi Narayan
    MATERIALS CHEMISTRY AND PHYSICS, 2024, 327
  • [18] Influence of fly ash particles on dry sliding wear behaviour of AA6061 aluminium alloy
    Selvam, J. David Raja
    Smart, D. S. Robinson
    Dinaharan, I.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2016, 54 (03): : 175 - 183
  • [19] Ductility of aluminium alloy AA7075 at high strain rates
    El-Magd, E
    Brodmann, M
    JOURNAL DE PHYSIQUE IV, 2000, 10 (P9): : 335 - 340
  • [20] Investigation of internal cracks in aluminium alloy AA7075 forging
    Gupta, RK
    Ramkumar, P
    Ghosh, BR
    ENGINEERING FAILURE ANALYSIS, 2006, 13 (01) : 1 - 8