Reshock behavior of silicon carbide

被引:8
|
作者
Dandekar, DP [1 ]
Reinhart, WD
Chhabildas, LC
机构
[1] AMSRL WM TD, Army Res Lab, Aberdeen Proving Ground, MD 21005 USA
[2] Sandia Natl Labs, Albuquerque, NM 87185 USA
来源
JOURNAL DE PHYSIQUE IV | 2003年 / 110卷
关键词
D O I
10.1051/jp4:20030796
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
The shear strength of a ceramic is an important material property which is indicative of its behaviour under impact loading condition. The brittle nature of ceramics suggest that impact loading of a ceramic attained due to subsonic impact could change the initial shear strength of the ceramic. If so, the subsequent behaviour of the ceramic may not be dependent on the the initial strength. Thus, it is necessary to determine the shear strength of a cermaic under single and multiple impacts. The present work determines the change in the shear strength of silicon carbide under a single shock, shock-reshock, and shock-release wave propagation, respectively. The material used in this work is marketed by CERCOM Inc. as SiC-B. The results of this work indicate that shear strength of SiC-B increases under shock-reshock.
引用
收藏
页码:827 / 831
页数:5
相关论文
共 50 条
  • [41] Hot-corrosion behavior of silicon nitride-bonded silicon carbide
    Woo, SK
    Han, IS
    Ri, GG
    Park, SC
    Cho, K
    Jang, BK
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2001, 109 (01) : 23 - 28
  • [42] Silicon carbide platelet/silicon carbide composites
    Mitchell Jr., Tyrone
    De Jonghe, Lutgard C.
    MoberlyChan, Warren J.
    Ritchie, Robert O.
    Journal of the American Ceramic Society, 1995, 78 (01): : 97 - 103
  • [43] EFFECT OF SILICON-CARBIDE WHISKER AND TITANIUM CARBIDE PARTICULATE ADDITIONS ON THE FRICTION AND WEAR BEHAVIOR OF SILICON-NITRIDE
    BLANCHARD, CR
    PAGE, RA
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (11) : 3442 - 3452
  • [44] Thermal Fatigue Behavior of Silicon-Carbide-Doped Silver Microflake Sinter Joints for Die Attachment in Silicon/Silicon Carbide Power Devices
    Hao Zhang
    Chuantong Chen
    Shijo Nagao
    Katsuaki Suganuma
    Journal of Electronic Materials, 2017, 46 : 1055 - 1060
  • [45] Thermal Fatigue Behavior of Silicon-Carbide-Doped Silver Microflake Sinter Joints for Die Attachment in Silicon/Silicon Carbide Power Devices
    Zhang, Hao
    Chen, Chuantong
    Nagao, Shijo
    Suganuma, Katsuaki
    JOURNAL OF ELECTRONIC MATERIALS, 2017, 46 (02) : 1055 - 1060
  • [46] Optimization of fracture behavior of alumina/silicon carbide nano ceramic
    Kordani, Naser
    Vanini, Ali Sadough
    Asadi, Ali
    Jabbari, Amin
    NEURAL COMPUTING & APPLICATIONS, 2013, 23 (7-8): : 2379 - 2385
  • [47] Fracture Behavior of Silicon Carbide Measured by Different Test Methods
    Jiang, Liang
    Chen, Yuhong
    Han, Fei
    Hua, Siming
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 140 - 143
  • [48] Tensile and compressive mechanical behavior of twinned silicon carbide nanowires
    Wang, Z. G.
    Li, J. B.
    Gao, F.
    Weber, W. J.
    ACTA MATERIALIA, 2010, 58 (06) : 1963 - 1971
  • [49] Creep behavior of a zirconium diboride-silicon carbide composite
    Bird, Marc W.
    Aune, Robert P.
    Yu, Feng
    Becher, Paul F.
    White, Kenneth W.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (13-14) : 2407 - 2420
  • [50] Effect of rheological behavior on properties of cast and sintered silicon carbide
    Liu, DM
    Fu, CT
    CERAMICS INTERNATIONAL, 1996, 22 (02) : 101 - 106