Carbon-carbon composite bearing materials in hip arthroplasty: analysis of wear and biological response to wear debris

被引:31
|
作者
Howling, GI
Ingham, E
Sakoda, H
Stewart, TD
Fisher, J
Antonarulrajah, A
Appleyard, S
Rand, B
机构
[1] Univ Leeds, Old Med Sch, Div Microbiol, Leeds LS2 9NL, W Yorkshire, England
[2] Univ Leeds, Sch Mech Engn, Leeds LS2 9JT, W Yorkshire, England
[3] Univ Leeds, Dept Mat, Leeds LS2 9JT, W Yorkshire, England
基金
英国工程与自然科学研究理事会;
关键词
D O I
10.1023/B:JMSM.0000010102.26218.d1
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Ultra-high molecular weight polyethylene wear particles have been implicated as the major cause of osteolysis, implant loosening and late aseptic failure in total hip arthroplasties in vivo. This study initially screened 22 carbon-carbon composite materials as alternatives for UHMWPE in joint bearings. New bearing materials should satisfy certain criteria-they should have good wear properties that at least match UHMWPE. and produce wear particles with low levels of cytotoxic and osteolytic activity. Initial screening was based on wear resistance determined in short-term tribological pin-on-plate tests. Three materials (HMU-PP(s), HMU-RC-P(s), and SMS-RC-P(s)) which had superior wear resistance were selected for long-term testing. All materials had very low wear factors and SMS-RC-P(s), which had a wear factor of 0.08+/-0.56x10(-7) mm(3)/Nm, was selected for the subsequent biological testing and particle size analysis. SMS-RC-P(s) showed good biocompatibility in bulk material form and also the wear particles had low cytotoxicity for L929 fibroblasts in culture compared to metal wear particles. Wear debris size analysis by transmission electron microscopy showed that the particles were very small, with the vast majority being under 100 nm in size, similar to metal wear particles. The potential osteolytic effect of SMS-RC-P(s) wear particles was investigated by culturing particles with human peripheral blood mononuclear cells and measuring TNFalpha production. SMS-RC-P(s) did not significantly stimulate TNFalpha production at a particle volume to cell number ratio of 80:1, indicating that the debris had a low osteolytic potential. The results of this study suggest that carbon-carbon composites, particularly those composed of PAN-based fibers may be important biomaterials in the development of next generation bearing surfaces for use in total joint replacements that have very low wear rates and reduced osteolytic and cytotoxic potential. (C) 2004 Kluwer Academic Publishers.
引用
收藏
页码:91 / 98
页数:8
相关论文
共 50 条
  • [31] ULTRASONIC EVALUATION OF CARBON-CARBON COMPOSITE MATERIALS
    BAKER, RA
    MATERIALS EVALUATION, 1970, 28 (09) : A36 - &
  • [32] The thermal properties of carbon-carbon composite materials
    Volkov, DP
    Zarichnyak, YP
    HIGH TEMPERATURE, 1995, 33 (06) : 938 - 943
  • [33] Wear debris from total hip arthroplasty presenting as an intrapelvic mass
    Mak, KH
    Wong, TK
    Poddar, NC
    JOURNAL OF ARTHROPLASTY, 2001, 16 (05): : 674 - 676
  • [34] Periprosthetic osteolysis in total hip arthroplasty: The role of particulate wear debris
    Maloney, WJ
    Smith, RL
    INSTRUCTIONAL COURSE LECTURES, VOL 45, 1996, 1996, 45 : 171 - 182
  • [35] BIOLOGICAL RESPONSE TO WEAR DEBRIS IN TOTAL JOINT REPLACEMENT
    WILLERT, H
    BIOMATERIALS, 1980, 1 (03) : 170 - 170
  • [36] A Review on Wear and Friction Performance of Carbon-Carbon Composites at High Temperature
    Kumar, Parshant
    Srivastava, Vijay Kumar
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2016, 13 (04) : 702 - 710
  • [37] Influence of environment and temperature on ''dusting'' wear transitions of carbon-carbon composites
    Yen, BK
    Ishihara, T
    Yamamoto, I
    JOURNAL OF MATERIALS SCIENCE, 1997, 32 (03) : 681 - 686
  • [38] Friction and wear behaviors of carbon-carbon composites used in finger seal
    Lu F.
    Chen G.
    Su H.
    Yi M.
    Peng K.
    Harbin Gongye Daxue Xuebao/Journal of Harbin Institute of Technology, 2017, 49 (01): : 184 - 188
  • [39] Influence of oxidation inhibitor on carbon-carbon composites: 6. Studies on friction and wear properties of carbon-carbon composites
    Park, SJ
    Seo, MK
    Lee, JR
    POLYMER-KOREA, 2001, 25 (01) : 133 - 141
  • [40] Evaluation of the Size-Dependent Cytotoxicity of DLC (Diamondlike Carbon) Wear Debris in Arthroplasty Applications
    Liao, T. T.
    Deng, Q. Y.
    Li, S. S.
    Li, X.
    Ji, L.
    Wang, Q.
    Leng, Y. X.
    Huang, N.
    ACS BIOMATERIALS SCIENCE & ENGINEERING, 2017, 3 (04): : 530 - 539