摘要
Ti3AlC2 has good oxidation resistance at high temperatures owing to the formation of protective Al2O3 layer. However, as it is directly exposed to air at 500 degreesC and especially 600 degreesC, the scales formed on Ti3AlC2 exhibits poor protectivity because of the oxidation-induced microcracks, which limits the potential application of this technologically important material. In this work, the oxidation resistance of Ti3AlC2 at 500 degreesC and 600 degreesC was significantly improved by pre-oxidation at 1000-1300 degreesC for a short time of 2 h in air. The oxidation of the pre-oxidized Ti3AlC2 at 600 degreesC generally obeyed a parabolic rate law instead of the speed-up linear relation in the case without pre-oxidation. As revealed by X-ray diffraction, Raman spectroscopy results and SEM observations, the remarkable improvement of oxidation resistance after pre-oxidation was attributed to the protective layers formed on Ti3AlC2 during pre-oxidation, which inhibited the formation of anatase TiO2 that resulted in the oxidation-induced microcracks. Moreover, this work confirmed that the mechanism proposed previously for the anomalous oxidation of Ti3AlC2 in air at 500-600 degreesC was correct.
引用
收藏
页码:205 / 211
页数:7
相关论文
共 50 条
  • [31] Reaction Behavior of Ti3AlC2 with Fe at High Temperature
    Chen Xinhua
    Zhai Hongxiang
    Song Pengfei
    Huang Zhenying
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 499 - 502
  • [32] High-temperature oxidation behavior of un-dense Ti3AlC2 material at 1000 °C in air
    Ai, Taotao
    CERAMICS INTERNATIONAL, 2012, 38 (03) : 2537 - 2541
  • [33] Anisotropic arc erosion resistance of Ag/Ti3AlC2 composites induced by the alignment of Ti3AlC2
    Wang, Dan Dan
    Tian, Wu Bian
    Ding, Jian Xiang
    Ma, Ai Bin
    Zhu, Yong Fa
    Zhang, Pei Gen
    He, Wei
    Sun, Zheng Ming
    CORROSION SCIENCE, 2020, 171
  • [34] Oxidation resistance of Ti3AlC2 and Ti3Al0.8Sn0.2C2 MAX phases: A comparison
    Drouelle, Elodie
    Brunet, Veronique
    Cormier, Jonathan
    Villechaise, Patrick
    Sallot, Pierre
    Naimi, Foad
    Bernard, Frederic
    Dubois, Sylvain
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2020, 103 (02) : 1270 - 1280
  • [35] Cyclic oxidation of Ti3AlC2 at 1000-1300 °C in air
    Qian, X. K.
    He, X. D.
    Li, Y. B.
    Sun, Y.
    Li, H.
    Xu, D. L.
    CORROSION SCIENCE, 2011, 53 (01) : 290 - 295
  • [36] Oxidation behavior of Ti3AlC2 at 1000-1400°C in air
    Wang, XH
    Zhou, YC
    CORROSION SCIENCE, 2003, 45 (05) : 891 - 907
  • [37] Suppressing the anomalous rapid oxidation of Ti3AlC2 by incorporating TiB2
    Li, Chao
    Qian, Yuhai
    Ma, Chunlei
    Wang, Shumin
    Li, Meishuan
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2019, 35 (03) : 432 - 439
  • [38] Suppressing the anomalous rapid oxidation of Ti3AlC2 by incorporating TiB2
    Chao Li
    Yuhai Qian
    Chunlei Ma
    Shumin Wang
    Meishuan Li
    JournalofMaterialsScience&Technology, 2019, 35 (03) : 432 - 439
  • [39] High Temperature Stability of Bulk Ti3AlC2 Materials in Air
    Lee, D. H.
    Lee, D. B.
    THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 410 - 415
  • [40] Bending creep and stress relaxation of Ti3AlC2 at high temperature
    Bao, YW
    Zhou, YC
    HIGH-PERFORMANCE CERAMICS III, PTS 1 AND 2, 2005, 280-283 : 1373 - 1377