High-temperature oxidation behavior of un-dense Ti3AlC2 material at 1000 °C in air

被引:21
|
作者
Ai, Taotao [1 ]
机构
[1] Shaanxi Univ Technol, Sch Mat Sci & Engn, Hanzhong 723003, Peoples R China
关键词
Hot pressing; Ti3AlC2; Oxidation behavior; High-temperature; SPACE-CHARGE SEGREGATION; TITANIUM-DIOXIDE; GRAIN-BOUNDARIES; TI3SIC2; AL;
D O I
10.1016/j.ceramint.2011.10.091
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Un-dense Ti3AlC2 material containing 3 wt% TiC was prepared by hot-pressing process using elemental powders of 2TiC/Ti/Al. Its oxidation behavior at 1000 degrees C in static air was investigated. SEM analysis indicates that the as fabricated sample is un-dense and the Ti3AlC2 grains with plate-like shape exhibit two types of fracture surfaces of layered and flat features. The oxidation behavior of the product exposed at 1000 degrees C for 30 h obeys a near-cubic law. The scale consists of rutile TiO2 and alpha-Al2O3 phases, and presents three layers, including an outer un-dense TiO2 layer adhering to a little Al2O3, a thick intermediate TiO2 + Al2O3 mixed layer and a thin inner Al2O3 layer with some pores. The thickness of the oxide layer was higher than 300 mu m. In addition, the deleterious effects of TiC and innate-pores on the oxidation resistance of the product were also investigated. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:2537 / 2541
页数:5
相关论文
共 50 条
  • [1] High-temperature oxidation behavior of Ti3AlC2 in air
    徐学文
    李养贤
    朱教群
    梅炳初
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S2) : 869 - 873
  • [2] High-temperature oxidation behavior of Ti3AlC2 in air
    Xu Xue-wen
    Li Yang-xian
    Zhu Jia-qun
    Mei Bing-chu
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S869 - S873
  • [3] Oxidation behavior of Ti3AlC2 at 1000-1400°C in air
    Wang, XH
    Zhou, YC
    CORROSION SCIENCE, 2003, 45 (05) : 891 - 907
  • [4] Microstructure and High-temperature Oxidation Behavior of Ti3AlC2/W Composites
    Cui, Bai
    Zapata-Solvas, Eugenio
    Reece, Michael J.
    Wang, Chang-An
    Lee, William E.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (02) : 584 - 591
  • [5] Oxidation Behavior of a Ti3AlC2/TiB2 Composite at 1000°-1400°C in Air
    Li, Meishuan
    Li, Chao
    Li, Jingjing
    Zhou, Yanchun
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2010, 93 (02) : 554 - 560
  • [6] Cyclic oxidation of Ti3AlC2 at 1000-1300 °C in air
    Qian, X. K.
    He, X. D.
    Li, Y. B.
    Sun, Y.
    Li, H.
    Xu, D. L.
    CORROSION SCIENCE, 2011, 53 (01) : 290 - 295
  • [7] High-temperature oxidation of Ti3AlC2 between 1173 and 1473 K in air
    Lee, D. B.
    Park, S. W.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 434 (1-2): : 147 - 154
  • [8] High-Temperature Oxidation Behavior of Ti2AlC in Air
    X.H. Wang
    Y.C. Zhou
    Oxidation of Metals, 2003, 59 : 303 - 320
  • [9] High-temperature oxidation behavior of Ti2AlC in air
    Wang, XH
    Zhou, YC
    OXIDATION OF METALS, 2003, 59 (3-4): : 303 - 320
  • [10] Oxidation behavior of Ti3AlC2 powders in flowing air
    Wang, XH
    Zhou, YC
    JOURNAL OF MATERIALS CHEMISTRY, 2002, 12 (09) : 2781 - 2785