Controlled synthesis and photoluminescence behaviors of Lu2O2SO4:Eu3+ and Lu2O2S:Eu3+ phosphors

被引:6
|
作者
Liu, Mingyang [1 ,2 ]
Wang, Li [1 ]
Lian, Jingbao [2 ]
机构
[1] Liaoning Petrochem Univ, Coll Sci, Fushun 113001, Peoples R China
[2] Liaoning Petrochem Univ, Sch Mech Engn, Fushun 113001, Peoples R China
关键词
A "general" amorphous precursor; Lutetium oxysulfate; oxysulfide; Co-precipitation and solid-state method; Photoluminescence; Red phosphor; COPRECIPITATION SYNTHESIS; LUMINESCENCE; CONVERSION; LN; NANOPARTICLES; EU3+; OXYSULFATE/OXYSULFIDE; YB3+; LU; GD;
D O I
10.1016/j.poly.2021.115527
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
A "general" amorphous precursor that can synthesize Eu3+ doped Lu2O2SO4 and Lu2O2S phosphors was prepared from commercially available Lu2O3 (AR), HNO3 (99.95% purity), (NH4)(2)SO4 (AR) and NH3.H2O (99.95% purity) as raw materials via a facile co-precipitation method. Based on this, block-like Lu2O2SO4:Eu3+ phosphors were synthesized by calcination in air, and mixed structures of near-spherical and rod-like Lu2O2S:Eu3+ phosphors were synthesized by calcination in a confined sulfuration atmosphere created using a solid-state method. Studies have shown that the molar ratio of SO42-:Lu3+ and the aqueous ammonia titration volume is very important in the co-precipitation process, the optimal ratio was selected as 25:1, and the optimal 1.5 M NH3.H2O solution volume was selected as 22 mL in this study. In the subsequent calcination process, the effect of calcination temperature on the target product was studied. The optimal calcination conditions are a calcination temperature of 800 degrees C for 2 h in air and 500 degrees C for 2 h in a closed sulfuration atmosphere, respectively, for the oxysulfate and oxysulfide phosphors. The photoluminescence (PL) behavior of the two phosphors was systematically investigated. The oxysulfate and oxysulfide phosphors show the characteristic red-light emission of the Eu3+ ion at about 620 and 628 nm, respectively, which originates from the D-5(0)-F-7(J) (J = 0,1,2,4) transition of the Eu3+ ion. The luminescence quenching types of both phosphors were dominated by exchange interactions and the optimum Eu3+ molar concentrations were found to be 3.0% for Lu2O2SO4:Eu3+ and 6.0% for Lu2O2S:Eu3+. The oxysulfide phosphor had a PL intensity-2.15 times stronger than the oxysulfate phosphor. The CIE color coordinates of the Lu2O2SO4:Eu3+ and Lu2O2S:Eu3+ phosphors are (0.6551, 0.3444) and (0.5842, 0.413), which belong to the categories of reddish-orange and orange colors, respectively. A shorter fluorescence lifetime (-12.650 mu s) and CCT (1738 K) was observed for the oxysulfide phosphor relative to those of the oxysulfate phosphor (-377.956 mu s and 2787 K).
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Multiplication of electronic excitations in nanophosphors Lu2O3:Eu3+ and Lu2O3:Tb3+
    Makhov, Vladimir N.
    Lushchik, Cheslav
    Lushchik, Aleksandr
    Kirm, Marco
    Wang, Zhi-Fang
    Zhang, Wei-Ping
    Yin, Min
    Zhao, Jing-Tai
    JOURNAL OF LUMINESCENCE, 2009, 129 (12) : 1711 - 1714
  • [32] Selective Synthesis of Morphology and Species Controlled La2O3:Eu3+ and La2O2CO3:Eu3+ Phosphors by Hydrothermal Method
    Mao, Guojuan
    Zhang, Hongwu
    Li, Haiyan
    Jin, Jing
    Niu, Shuyun
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2012, 159 (03) : J48 - J53
  • [33] Lu2O3:Eu3+ ULTRADISPERSED POWDERS AND TRANSLUCENT CERAMICS
    Yavetskiy, R. P.
    Vovk, E. A.
    Kosmyna, M. B.
    Sergienko, Z. P.
    Tolmachev, A. V.
    Puzikov, V. M.
    Nazarenko, B. P.
    Shekhovtsov, A. N.
    CERAMIC MATERIALS AND COMPONENTS FOR ENERGY AND ENVIRONMENTAL APPLICATIONS, 2010, 210 : 597 - 603
  • [34] Preparation and characterization of a new phosphor Lu2O3: Eu3+
    Chen, QW
    Shi, Y
    Shi, JL
    HIGH-PERFORMANCE CERAMICS III, PTS 1 AND 2, 2005, 280-283 : 525 - 528
  • [35] Crystal-field analysis of Eu3+ in Lu2O3
    Karbowiak, M
    Zych, E
    Hölsä, J
    JOURNAL OF PHYSICS-CONDENSED MATTER, 2003, 15 (13) : 2169 - 2181
  • [36] Preparation of Lu2O3:Eu3+ nanopowders for optical ceramics
    Yavetskiy, R. P.
    FUNCTIONAL MATERIALS, 2008, 15 (04): : 569 - 573
  • [37] Relationship between Eu3+ substitution sites and photoluminescence properties of SrIn2O4:Eu3+ spinel phosphors
    Kang, Yipu
    Thuy, Bui
    Shimokawa, Yohei
    Hayakawa, Tomokatsu
    Sakaida, Satoshi
    Miao, Lei
    Tanemura, Sakae
    Honda, Sawao
    Iwamoto, Yuji
    JOURNAL OF LUMINESCENCE, 2016, 169 : 78 - 85
  • [38] Photoluminescence and gamma-ray irradiation of SrAl2O4:Eu2+ and Y2O3:Eu3+ phosphors
    Zhu, Chaofeng
    Yang, Yunxia
    Chen, Guorong
    Baccaro, S.
    Cecilia, A.
    Falconieri, M.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2007, 68 (09) : 1721 - 1724
  • [39] X-ray luminescence of core-shell structured SiO2/Lu2O3:Eu3+ and SiO2/Lu2Si2O7:Eu3+ particles
    Yermolayeva, Yu V.
    Korshikova, T. I.
    Tolmachev, A. V.
    Yavetskiy, R. P.
    RADIATION MEASUREMENTS, 2011, 46 (05) : 551 - 554
  • [40] Synthesis of Y2O3:Eu3+ phosphors by surface diffusion and their photoluminescence properties
    Zhang Ming
    Li Xin-hai
    Wang Zhi-xing
    Hu Qi-yang
    Guo Hua-jun
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (01) : 115 - 118