Controlled synthesis and photoluminescence behaviors of Lu2O2SO4:Eu3+ and Lu2O2S:Eu3+ phosphors

被引:6
|
作者
Liu, Mingyang [1 ,2 ]
Wang, Li [1 ]
Lian, Jingbao [2 ]
机构
[1] Liaoning Petrochem Univ, Coll Sci, Fushun 113001, Peoples R China
[2] Liaoning Petrochem Univ, Sch Mech Engn, Fushun 113001, Peoples R China
关键词
A "general" amorphous precursor; Lutetium oxysulfate; oxysulfide; Co-precipitation and solid-state method; Photoluminescence; Red phosphor; COPRECIPITATION SYNTHESIS; LUMINESCENCE; CONVERSION; LN; NANOPARTICLES; EU3+; OXYSULFATE/OXYSULFIDE; YB3+; LU; GD;
D O I
10.1016/j.poly.2021.115527
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
A "general" amorphous precursor that can synthesize Eu3+ doped Lu2O2SO4 and Lu2O2S phosphors was prepared from commercially available Lu2O3 (AR), HNO3 (99.95% purity), (NH4)(2)SO4 (AR) and NH3.H2O (99.95% purity) as raw materials via a facile co-precipitation method. Based on this, block-like Lu2O2SO4:Eu3+ phosphors were synthesized by calcination in air, and mixed structures of near-spherical and rod-like Lu2O2S:Eu3+ phosphors were synthesized by calcination in a confined sulfuration atmosphere created using a solid-state method. Studies have shown that the molar ratio of SO42-:Lu3+ and the aqueous ammonia titration volume is very important in the co-precipitation process, the optimal ratio was selected as 25:1, and the optimal 1.5 M NH3.H2O solution volume was selected as 22 mL in this study. In the subsequent calcination process, the effect of calcination temperature on the target product was studied. The optimal calcination conditions are a calcination temperature of 800 degrees C for 2 h in air and 500 degrees C for 2 h in a closed sulfuration atmosphere, respectively, for the oxysulfate and oxysulfide phosphors. The photoluminescence (PL) behavior of the two phosphors was systematically investigated. The oxysulfate and oxysulfide phosphors show the characteristic red-light emission of the Eu3+ ion at about 620 and 628 nm, respectively, which originates from the D-5(0)-F-7(J) (J = 0,1,2,4) transition of the Eu3+ ion. The luminescence quenching types of both phosphors were dominated by exchange interactions and the optimum Eu3+ molar concentrations were found to be 3.0% for Lu2O2SO4:Eu3+ and 6.0% for Lu2O2S:Eu3+. The oxysulfide phosphor had a PL intensity-2.15 times stronger than the oxysulfate phosphor. The CIE color coordinates of the Lu2O2SO4:Eu3+ and Lu2O2S:Eu3+ phosphors are (0.6551, 0.3444) and (0.5842, 0.413), which belong to the categories of reddish-orange and orange colors, respectively. A shorter fluorescence lifetime (-12.650 mu s) and CCT (1738 K) was observed for the oxysulfide phosphor relative to those of the oxysulfate phosphor (-377.956 mu s and 2787 K).
引用
收藏
页数:11
相关论文
共 50 条
  • [11] Photoluminescence of Lu2O3:Eu3+ phosphors obtained by glycine-nitrate combustion synthesis
    Qiwei Chen
    Ying Shi
    Jiyang Chen
    Jianlin Shi
    Journal of Materials Research, 2005, 20 : 1409 - 1414
  • [12] Photoluminescence of Lu2O3:Eu3+ phosphors obtained by glycine-nitrate combustion synthesis
    Chen, QW
    Shi, Y
    Chen, JY
    Shi, JL
    JOURNAL OF MATERIALS RESEARCH, 2005, 20 (06) : 1409 - 1414
  • [13] SYNTHESIS AND PHOTOLUMINESCENCE PROPERTIES OF ELLIPSOIDAL La2O2SO4:Eu3+ PHOSPHORS
    Li, Xing
    Gao, Lutong
    Lian, Jingbao
    MATERIALI IN TEHNOLOGIJE, 2022, 56 (06): : 669 - 676
  • [14] 3D-hierarchical Lu2O2S:Eu3+ micro/nano-structures: controlled synthesis and luminescence properties
    Zhao, Qi
    Zheng, Yuhua
    Guo, Ning
    Jia, Yongchao
    Qiao, Hui
    Lv, Wenzhen
    You, Hongpeng
    CRYSTENGCOMM, 2012, 14 (20): : 6659 - 6664
  • [15] Preparation and optical properties of nanocrystalline Lu2O3:Eu3+ phosphors
    Daldosso, Matteo
    Sokolnicki, Jerzy
    Kepinski, Leszek
    Legendziewicz, Janina
    Speghini, Adolfo
    Bettinelli, Marco
    JOURNAL OF LUMINESCENCE, 2007, 122 : 858 - 861
  • [16] Co-precipitation synthesis of Y2O2SO4:Eu3+ nanophosphor and comparison of photoluminescence properties with Y2O2:Eu3+ and Y2O2S:Eu3+ nanophosphors
    Lian, Jingbao
    Qin, Hua
    Liang, Ping
    Liu, Feng
    SOLID STATE SCIENCES, 2015, 48 : 147 - 154
  • [17] Synthesis and photoluminescence properties of MgAl2O4:Eu3+ phosphors
    Yoon, S. J.
    Hakeem, D. A.
    Park, K.
    CERAMICS INTERNATIONAL, 2016, 42 (01) : 1261 - 1266
  • [18] Synthesis and photoluminescence of nano-Y2O3:Eu3+ phosphors
    He, CA
    Guan, YF
    Yao, LZ
    Cai, WL
    Li, XG
    Yao, Z
    MATERIALS RESEARCH BULLETIN, 2003, 38 (06) : 973 - 979
  • [19] Lu2O2S:Tb3+, Eu3+ nanorods: luminescence, energy transfer, and multicolour tuneable emission
    Zhang, Bowen
    Zou, Haifeng
    Guan, Hongxia
    Dai, Yunzhi
    Song, Yanhua
    Zhou, Xiuqing
    Sheng, Ye
    CRYSTENGCOMM, 2016, 18 (39): : 7620 - 7628
  • [20] Synthesis, characterization and formation mechanism of pompon-like Lu2O2SO4: Eu3+ phosphors via a facile homogeneous precipitation method followed by calcination
    Liu, Mingyang
    Lian, Jingbao
    Wu, Nianchu
    Zhang, Xue
    He, Jiao
    SOLID STATE SCIENCES, 2021, 112