Investigation of the Effect of Zirconium Amount on Grain Size and Wear Performance in TZM Alloys Produced by Mechanical Alloying Method

被引:1
|
作者
Sirali, Haktan [1 ]
Simsek, Dogan [2 ]
Ozyurek, Dursun [3 ]
机构
[1] Karabuk Univ, Inst Sci, Karabuk, Turkey
[2] Natl Def Univ, Army NCO Vocat HE Sch, Balikesir, Turkey
[3] Karabuk Univ, Technol Fac, Karabuk, Turkey
关键词
TZM alloy; Zirconium; Grain size; Wear; BEHAVIOR;
D O I
10.1007/s12666-021-02510-4
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this study, the relation between grain size, hardness and wear performance of Titanium-Zirconium-Molybdenum (TZM) alloys with different amounts (0.06, 0.07, 0.08 and 0.09 wt%) of Zr added by the mechanical alloying method was investigated. As a result of the studies, it was observed that the number of pores in the structure increased with the increase in the amount of Zr, while there was a decrease in the grain size. In the hardness and density results, it was observed that while the hardness values increased with increasing Zr amount, there was a decrease in the density values. As a result of the wear tests, the lowest weight loss at 10-30 N loads was obtained in the TZM alloy with the highest Zr added (0.09% Zr). The lowest friction coefficient in the friction coefficient results was obtained in TZM alloy with 0.09% Zr added.
引用
收藏
页码:805 / 812
页数:8
相关论文
共 50 条
  • [31] Effect of the size of powder on the Microstructures and Grain Refining Performance of AlTiC alloys
    Jing, Cao
    Wang, Yongfeng
    Wei, Chunxue
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 887 - +
  • [32] Microstructure, Mechanical Properties, and Antibacterial Performance of Novel Fe-Mn-Zn Nanocrystalline Alloys Produced by Mechanical Alloying
    Dag, Ilker Emin
    Kilic, Funda
    Panigrahi, Mrutyunjay
    Avar, Baris
    ADVANCED ENGINEERING MATERIALS, 2025,
  • [33] Influence of CaO on the Nanohardness Behaviour of AZ63 Magnesium Alloys Produced by Mechanical Alloying Method
    Boztas, M.
    Ozarslan, S.
    Sahin, O.
    ACTA PHYSICA POLONICA A, 2016, 130 (01) : 357 - 361
  • [34] Alloying effect on grain-size dependent deformation twinning in nanocrystalline Cu-Zn alloys
    Ma, X. L.
    Xu, W. Z.
    Zhou, H.
    Moering, J. A.
    Narayan, J.
    Zhu, Y. T.
    PHILOSOPHICAL MAGAZINE, 2015, 95 (03) : 301 - 310
  • [35] Investigation of Wear Performance of Different Amount SiC Reinforcements A356 Matrix Composite Materials Produced by Semi-Solid Process Method
    Simsek, Ijlal
    Simsek, Dogan
    Ozyurek, Dursun
    JOURNAL OF POLYTECHNIC-POLITEKNIK DERGISI, 2020, 23 (04): : 1237 - 1243
  • [36] Effect of grain size composition on mechanical performance requirement for particles in aggregate blend based on photoelastic method
    Wang, Sudi
    Miao, Yinghao
    Wang, Linbing
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 363
  • [37] Investigation of the wear and corrosion behaviors of Ti5Al2.5Fe and Ti6Al4V alloys produced by mechanical alloying method in simulated body fluid environment
    Simsek, Ijlal
    Ozyurek, Dursun
    MATERIALS SCIENCE AND ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2019, 94 : 357 - 363
  • [38] Grain size effect on mechanical performance of nanostructured superelastic NiTi alloy
    Xiao, Yao
    Zeng, Pan
    Lei, Liping
    MATERIALS RESEARCH EXPRESS, 2017, 4 (03):
  • [39] Exchange of experience the effect of synthesis time on the wear behavior of Al–8%Ti alloy produced by mechanical alloying
    D. Özyürek
    S. Tekeli
    T. Tuncay
    R. Yilmaz
    Powder Metallurgy and Metal Ceramics, 2012, 51 : 491 - 495
  • [40] Effect of particle size of starting oxide powders on the performance of doped-lanthanum oxyapatite produced by mechanical alloying followed by microwave sintering
    Oliveira, F. A. C.
    Marcelo, T.
    Alves, C.
    Santos, M.
    Mascarenhas, J.
    Trindade, B.
    ADVANCED POWDER TECHNOLOGY, 2014, 25 (05) : 1455 - 1461