Effects of internal stresses on the mechanical properties of deposition thin films

被引:41
|
作者
Chuang, C. T. [1 ]
Chao, C. K. [2 ]
Chang, R. C. [1 ]
Chu, K. Y. [2 ]
机构
[1] St Johns Univ, Dept Mech & Comp Aided Engn, Taipei 25135, Taiwan
[2] Natl Taiwan Univ Sci & Technol, Dept Mech Engn, Taipei 106, Taiwan
关键词
thin films; internal stresses; mechanical properties; nanoindentation;
D O I
10.1016/j.jmatprotec.2007.11.258
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Thin films become an important technology because of its outstanding performance in wide engineering applications. The basic of thin film technology is to characterize its mechanical proper-ties, which are strongly dependent on the internal stresses induced by deposition processes. Therefore, an investigation of mechanical properties of thin films affected by internal stresses is presented. In this work, titanium thin films are deposited on silicon wafer substrate by evaporation deposition. internal stresses of thin films are measured by a surface profiler and the elastic modulus and hardness of the thin films are tested by a nanoindenter with a standard Berkovich probe tip. Corelation between the internal stresses and mechanical properties are also discussed. (C) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:770 / 774
页数:5
相关论文
共 50 条
  • [31] Effects of mechanical stresses, thickness and atmosphere on aging of polyimide thin films at high temperature
    Khazaka, R.
    Locatelli, M. L.
    Diaham, S.
    Bidan, P.
    POLYMER DEGRADATION AND STABILITY, 2013, 98 (01) : 361 - 367
  • [32] EFFECT OF DEPOSITION CONDITIONS ON MECHANICAL PROPERTIES OF MAGNETRON SPUTTERED SiC THIN FILMS
    Ctvrtlik, Radim
    Kulikovsky, Valeriy
    Bohac, Petr
    Blahova, Olga
    CHEMICKE LISTY, 2012, 106 : S395 - S398
  • [33] Mechanical and physicochernical properties of AlN thin films obtained by pulsed laser deposition
    Cibert, C
    Tétard, F
    Djemia, P
    Champeaux, C
    Catherinot, A
    Tétard, D
    SUPERLATTICES AND MICROSTRUCTURES, 2004, 36 (4-6) : 409 - 416
  • [34] INTERNAL-STRESSES IN THIN GE, ZNS, AND ZNSE FILMS
    GUSEV, AG
    NESMELOV, EA
    NIKITIN, AS
    GAINUTDINOV, IS
    SOVIET JOURNAL OF OPTICAL TECHNOLOGY, 1982, 49 (08): : 508 - 510
  • [35] Internal oxidation and mechanical properties of Pt-IrO2 thin films
    Chromik, RR
    Bannuru, T
    Vinci, RP
    THIN FILMS-STRESSES AND MECHANICAL PROPERTIES X, 2004, 795 : 485 - 490
  • [36] Evaluation of internal stresses in TiN thin films by synchrotron radiation
    Hanabusa, T
    Kusaka, K
    Matsue, T
    Nishida, M
    Sakata, O
    Sato, T
    VACUUM, 2004, 74 (3-4) : 571 - 575
  • [37] Dependence of the pyroelectric response on internal stresses in ferroelectric thin films
    Ban, ZG
    Alpay, SP
    APPLIED PHYSICS LETTERS, 2003, 82 (20) : 3499 - 3501
  • [38] The Effects of Ti Additions and Deposition Parameters on the Structural and Mechanical Properties of Stainless Steel-Nitride Thin Films
    Alresheedi, Faisal I.
    Krzanowski, James E.
    COATINGS, 2019, 9 (05):
  • [39] Strain ratio effects in mechanical properties of supported thin films
    Godard, P.
    Faurie, D.
    Renault, P. O.
    JOURNAL OF APPLIED PHYSICS, 2020, 127 (10)
  • [40] The effects of radiation on the mechanical properties of polysilicon and polydiamond thin films
    Newton, RL
    Davidson, JL
    MECHANICAL PROPERTIES OF STRUCTURAL FILMS, 2001, 1413 : 318 - 327