Strengthening of Vickers indented 3Y-TZP by hydrothermal ageing

被引:15
|
作者
Marro, F. G. [1 ,2 ]
Anglada, M. [1 ,2 ]
机构
[1] Univ Politecn Cataluna, Ctr Res Nanoengn, CRnE, E-08028 Barcelona, Spain
[2] Univ Politecn Cataluna, Dept Mat Sci & Met Engn, E-08028 Barcelona, Spain
关键词
ZrO(2); Fracture; Mechanical properties; Strength; Toughness and toughening; LOW-TEMPERATURE DEGRADATION; FRACTURE-TOUGHNESS; INDENTATION TECHNIQUES; FEMORAL-HEAD; ZIRCONIA; CRACK;
D O I
10.1016/j.jeurceramsoc.2011.08.019
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of hydrothermal ageing on indentation cracks has been determined in 3Y-TZP by measuring the flexure strength of indented specimens before and after ageing. A substantial increase in strength was observed after ageing, in contrast to the well known decrease in strength in smooth specimens with only natural flaws. The increase in strength with ageing also occurs if the indentation residual stresses are previously removed by annealing. Observations around the crack tip show the formation of a highly microcracked zone during vapour exposure. Fractographic and micro-Raman analysis observations show that the profile of the cracks is marked on the fracture surface by this zone which is intergranular with a crumbled appearance and in which transformation has taken place. The increase in strength is discussed in terms of crack tip blunting induced by the multiaxial stresses that develop in front of the crack under bending. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:317 / 324
页数:8
相关论文
共 50 条
  • [41] Effect of a small amount of Al2O3 addition on the hydrothermal degradation of 3Y-TZP
    Zhikai Wu
    Ning Li
    Yuhua Wen
    Journal of Materials Science, 2013, 48 : 1256 - 1261
  • [42] The combined effect of alumina and silica co-doping on the ageing resistance of 3Y-TZP bioceramics
    Samodurova, Anastasia
    Kocjan, Andraz
    Swain, Michael V.
    Kosmac, Tomaz
    ACTA BIOMATERIALIA, 2015, 11 : 477 - 487
  • [43] Ion-plating of TiN on superplastically deformed 3Y-TZP ceramic and 3Y-TZP/Al2O3 composite
    Kamiya, S
    Motohashi, Y
    Harjo, S
    Wan, C
    Urao, R
    SURFACE & COATINGS TECHNOLOGY, 2003, 169 : 464 - 467
  • [44] Effect of a small amount of Al2O3 addition on the hydrothermal degradation of 3Y-TZP
    Wu, Zhikai
    Li, Ning
    Wen, Yuhua
    JOURNAL OF MATERIALS SCIENCE, 2013, 48 (03) : 1256 - 1261
  • [45] Effect of grain size on mechanical properties of submicrometer 3Y-TZP:: Fracture strength and hydrothermal degradation
    Eichler, Jens
    Roedel, Juergen
    Eisele, Ulrich
    Hoffman, Mark
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (09) : 2830 - 2836
  • [46] Transition metals increase hydrothermal stability of yttria-tetragonal zirconia polycrystals (3Y-TZP)
    Zhu, Wenliang
    Fujiwara, Aiko
    Nishiike, Naomichi
    Marin, Elia
    Sugano, Nobuhiko
    Pezzotti, Giuseppe
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (10) : 3573 - 3577
  • [47] Characterisation of Ce0.8Gd0.2O1.9/3Y-TZP composite electrolytes—Effects of 3Y-TZP particle treatment
    R. J. Ball
    R. Stevens
    Journal of Materials Science, 2002, 37 : 4137 - 4144
  • [48] Characterisation of Ce0.8Gd0.2O1.9/3Y-TZP composite electrolytes—effects of weight % 3Y-TZP particles
    R. J. Ball
    R. Stevens
    Journal of Materials Science, 2003, 38 : 1413 - 1423
  • [49] Characterisation of Ce0.8Gd0.2O1.9/3Y-TZP composite electrolytes -: effects of weight % 3Y-TZP particles
    Ball, RJ
    Stevens, R
    JOURNAL OF MATERIALS SCIENCE, 2003, 38 (07) : 1413 - 1423
  • [50] Role of 3Y-TZP grain boundaries in glazing and layering
    Shahmiri, R.
    Standard, O. C.
    Hart, J. N.
    Gharagozlu, N.
    Bahmanrokh, G.
    Yin, Y.
    Mofarah, S. S.
    Adabifiroozjaei, E.
    Webster, R.
    Sorrell, C. C.
    DENTAL MATERIALS, 2024, 40 (12) : 2148 - 2156